Biosorption is an effective method to remove toxic metals from wastewaters. In this
study biosorption of lead and chromium ions from solution was studied using
Citrobacter freundii and Citrobacter kosari isolated from industrial wastewater. The
experimental results showed that optimum grwoth temperature for both bacteria is 30oC
and the optimum pH is 7 &6 for C. freundii and C. kosari respectively. While the
optimum incubation period to remove Pb and Cr for C. freundii and C. kosari is 4 days
and 3days respectively. Also the biosorption of Pb and Cr in mixed culture of bacteria
and mixed culture of Pb and Cr was investigated. Result indicate that uptake of Cr and
Pb for C.freundii, C. kosari and in mixes culture of both bacteria is 58%, 53% and 82%
respectively for chromium in solution containing 1000ppm of Cr and 59%, 63% and
78% respectively for lead in solution containing 1000ppm of lead. But the uptake
decreases in solution containing both heavy metals lead and chromium.
A colloidal indium oxide (In2O3) nanoparticles (NPs) were synthesized pulsed laser ablation (PLA) of indium plate placed on the bottom of the quartz vessel containing (3ml) of pure ethanol. The influence laser energy on the properties of the formed nano-particles were characterized by using atomic force microscopy (AFM), X-ray diffraction (XRD), Ultraviolet Visible (UV-Vis) technique, and electrical properties measurements. The XRD revealed the crystallization structure of In2O3 nanoparticles and all the films having preferential orientation along (222) plane and intensity increases with increasing laser energy, The UV–Visible spect
... Show MoreIn this study, the investigation of Local natural Iraqi rocks kaolin with the addition of different proportions of bauxite and its effect on the physical and mechanical properties of the produced refractories was conducted. Kaolin/bauxite mixture was milled and classified into various size fractions, the kaolin (less than 105 μm) and the bauxite (less than 70μm). The specimens were mixed from kaolin and bauxite in ranges B1 (95+5)%, B2 (90+10)%, B3(85+15)%, and B4 (80+20)% respectively. The green specimens were shaped by the semi-dry method using a hydraulic press and a molding pressure of 7 MPa with the addition of (9-12) %wt. of PVA ratio. After molding and drying, the specimens were fired at (1100, 1200 and 13
... Show MorePolypyrrole/silver (PPy/Ag) nanocomposites was synthesized via a chemical oxidative method. The AFM analysis is performed to study the surface roughness, morphology and size distribution of the PPy particles and PPy-ag nanocomposites. The results indicated that as the concentration of Ag in the nanocomposite increases, the roughness also increases. The size of nanoparticles was also evaluated and found in the range of 15 nm to 125 nm. The PPy/Ag nanocomposites exhibited an effectiveness against Gram-negative Escherichia coli showing an inhibition zone of 4mm and displayed poor efficacy against Gram-positive Staphylococcus aureus. Based on given adequate antibacterial characteristics of PPy/Ag nanocomposites, it can be identified as
... Show MoreThe combination of carbon nanotubes (CNT) and conducting polymers offers an attractive route for the production of novel compounds that can be used in a variety of applications such as sensors, actuators, and molecular scale electronic devices. In this work, functionalized multiwall carbon nanotubes (f-MWCNTs) were added in different load ratios (3 wt%, 5 wt% and 10 wt%) to thiophen (PTh) polymer to procedure PTh/CNTs nanocomposite and deposited on porous silicon substrate by electropolarization. Photoconductive detectors were fabricated using PTh/f-MWCNTs matrix to work in the near region and middle IR regions. These detectors were illuminated by semiconductor laser diode wavelength of 808(nm) and Nd-YAG laser of wavelength 1064 (n
... Show MoreBiosynthesis of nanoparticles has received considerable attention due to the growing need to develop environmentally benign nanoparticle synthesis processes that do not use toxic chemicals. Therefore, biosynthetic methods employing both biological agents such as bacteria and fungus or plant extracts have emerged as a simple and a viable alternative to chemical synthetic and physical method .It is well known that many microbes produce an organic material either intracellular or extracellular which is playing important role in the remediation of toxic metals through reduction of metal ions and acting as interesting Nano factories. As a result, in the present study Ag NPs were syn
... Show MoreThere has been an increase in demand for nanocomposite, which has resulted in large-scale manufacturers employing high-energy processes and harmful solvents. Because of this, the need for environmentally benign "green" synthesis processes has grown. Other methods for making nanocomposite include using plants and plant products, bacteria, fungi, yeast, and algae. Green synthesis has minimal toxicity and is safe for human health and the environment compared to other processes, making it the ideal option for creating nanocomposite materials. This work reveals an environmentally friendly synthesis method for magnetic nanocomposites. In particular, they were using an aqueous extract of Artemisia to obtain ZnO/Fe3O4
... Show MoreContext and its influence in direction of reference by Abi Hussein Al Basri
BaTiO3 thin films have been deposited on Si (111) and glass substrates by using pulsed laser deposition technique. The films were characterized by using X-ray diffraction, atomic force microscope and optical transmission spectra. The films growth on Si after annealing at 873K showed a polycrystalline nature, and exhibited tetragonal structure, while on glass substrate no growth was noticed at that temperature. UV-VIS transmittance measurements showed that the films are highly transparent in the visible wavelength region and near-infrared region for sample annealing on glass substrate. The optical gap of the film were calculated from the curve of absorption coefficient (αhν) 2 vs. hν and was found tobe 3.6 eV at substrate temperature 5
... Show MoreThis paper present a simple and sensitive method for the determination of DL-Histidine using FIA-Chemiluminometric measurement resulted from oxidation of luminol molecule by hydrogen peroxide in alkaline medium in the presence of DL-Histidine. Using 70?l. sample linear plot with a coefficient of determination 95.79% for (5-60) mmol.L-1 while for a quadratic relation C.O.D = 96.44% for (5-80) mmol.L-1 and found that guadratic plot in more representative. Limit of detection was 31.93 ?g DL-Histidine (S/N = 3), repeatability of measurement was less that 5% (n=6). Positive and negative ion interferances was removed by using minicolume containing ion exchange resin located after injection valve position.