Tensile , thermal, and barrier properties of polylactide PLA-based
nanocomposite films that were prepared by solvent casting method with
polyethylene glycol (PEG), and alumina were studied. PLA/PEG blend showed
decrease in tensile strength and Young modulus but increased in elongation in
PLA/PEG and increased in crystalline of PLA but decrease in glass transition
temperature with the increasing of PEG concentration . A nano blend composites of
PLA/PEG/alumina (50/50/4) when compared to PLA/PEG blend indicated that
tensile strength , Young modulus and glass transition temperature (Tg) increased
with adding alumina nano particles, concentration and barrier properties
improvement due to its nucleating and reinforcing function mineral when add nano
alumina to PLA/PEG blend . These results indicated that the incorporation of Al2O3
enhanced the Oxygen barrier properties of the PLA.
The chemical additives used to enhance the properties of drilling mud cause damage to humans and the environment. Therefore, it is necessary to search for alternative additives to add them to the drilling mud. Thus, this study investigates the effects of pomegranate peel and grape seed powders as natural waste when added to un-weighted water-based mud. The test includes measurements of the rheological properties and filtration, as well as the alkanity and density of the drilling mud. The results showed a decrease in PH values with an increase in the concentrations of pomegranate peel or grapeseed, and a decrease in mud density with an increase in powders of pomegranate peel and grape seed concentrations that resulted f
... Show More(Cu1-x,Agx)2ZnSnSe4 alloys have been fabricated with different Ag content(x=0, 0.1, and 0.2) successfully from their elements. Thin films of these alloys have been deposited on coring glass substrate at room temperature by thermal evaporation technique under vacuum of 10-5Torr with thickness of 800nm and deposition rate of 0.53 nm/sec. Later, films have been annealed in vacuum at (373, and 473)K, for one hour. The crystal structure of fabricated alloys and as deposited thin films had been examined by XRD analysis, which confirms the formation of tetragonal phase in [112] direction, and no secondary phases are founded. The shifting of main polycrystalline peak (112) to lower Bragg’s angle as compared to Cu2ZnSnSe4 angle refers to incorpora
... Show MoreIn this research, we studied the structural properties of SnO2 films nanostructure which prepared by chemical spray pyrolysis method at room temperature on the rules of glass heated (400oC) with rate of spraying (2.5 ml/ min). The effect of annealing temperaturs (450,500,550,600 and 650oC) for two hours on those properties has been indicated. The results of x-ray diffraction showed that all of the prepared films were polycrystalline with tetragonal type and orientation was (110) for all models before and after annealing, and the annealing led to an increase in the grain size. The full width at half maximum (FWHM) values of the (110) peaks of the films decreased from 1.492o to 1.064o with increasing annealing temperature .The surface morp
... Show MoreRecent research has examined the improvement of physical and dielectric properties of BaTiO3 ceramic material by small addition of excess TiO2 or BaCO3. The prepared samples sintered at different temperatures and varying soaking time. The results show that increasing the sintering temperature within 1350°C and soaking time of 10 hrs give better electrical and physical properties, which indicate the reaction is complete at higher temperature and period.
Copper oxide thin films were synthesized by using spray pyrolysis deposition technique, in the temperature around 400°C in atmosphere from alcoholic solutions. Copper (II) chloride as precursor and glass as a substrate. The textural and structural properties of the films were characterized by atomic force microscopy (AFM), X-ray diffraction (XRD). The average particle size determined from the AFM images ranged from 30 to 90 nm and the roughness average was equal to 9.3 nm. The XRD patterns revealed the formation of a polycrystalline hexagonal CuO. The absorption and transmission spectrum, band gap, film thickness was investigated. The films were tested as an |
In the present work, the ternary compound MgxZn7-x O7Wurtzoid with variable Zn and Mg contents was analyzed using density functional theory with B3LYP 6-311G**basis set. The electronic and vibrational properties of MgxZn7-xO7 wurtzoids, were investigated, including energy gaps, bond lengths, spectral properties, such like infrared spectra and Raman. IR and Raman spectra were compared with experimental longitudinal optical modes frequency results. The theoretical results agree well with experiments and previous data. It has been found that the energy gap is increasing with the increased Mg concentration, and that the longitudinal optical position exposes a UV shift movement with an increase in the concentration.
The properties of structural and optical of pure and doped nano titanium dioxide (TiO2) films, prepared using chemical spray pyrolysis (CPS) technique, with different nanosize nickel oxide (NiO) concentrations in the range (3-9)wt% have been studied. X-Ray diffraction (XRD) technique where using to analysis the structure properties of the prepared thin films. The results revealed that the structure properties of TiO2 have polycrystalline structure with anatase phase. The parameters, energy gap, extinction coefficient, refractive index, real and imaginary parts were studied using absorbance and transmittance measurements from a computerized ultraviolet visible spectrophotometer (Shimadzu UV-1601 PC) in the wavelength
... Show MoreCu X Zn1-XO films with different x content have been prepared by
pulse laser deposition technique at room temperatures (RT) and
different annealing temperatures (373 and 473) K. The effect of x
content of Cu (0, 0.2, 0.4, 0.6, 0.8) wt.% on morphology and
electrical properties of CuXZn1-XO thin films have been studied.
AFM measurements showed that the average grain size values for
CuXZn1-xO thin films at RT and different annealing temperatures
(373, 473) K decreases, while the average Roughness values increase
with increasing x content. The D.C conductivity for all films
increases as the x content increase and decreases with increasing the
annealing temperatures. Hall measurements showed that there are
two