Various Hall Effects have been successfully observed in samples of n-type indium antimonide with values for conductivity, energy gap, Hall mobility and Hall coefficient all agreeing with theory. A particular interest in developing a method for obtaining accurate values of carrier concentrations in semiconductor samples has been fulfilled with an experimental result of (1.6×1016 cm-3 ±10.7%) giving a percentage difference of (6.7%) to a quoted value of (1.5×1016cm-3) at (77K) using an (80mW C.W. CO2) laser beam at (10.6μm) to illuminate a similar sample of n-type indium antimonide, an "Optical" Hall effect has been observed. Although some doubt has been raised as to the validity of effect i.e. "thermal" rather than "Optical", values of (45.8×10-8 seconds) for recombination times of electron, and (3.2×1016cm-3) for the dynamic carrier concentration were calculated by this method. A similar attempt at illuminating the sample with an R.S. catalogue ultra bright L.E.D proved inconsistent with theory and consequent result have been left inconclusive.
The preparation of the title compound, C26H25N, was achieved by the condensation of an ethanolic mixture of benzaldehyde, cyclohexanone and ammonium acetate in a 2:1:1 molar ratio. There are two crystallographically independent molecules in the asymmetric unit. The two cyclohexyl rings adopt an
Ebastine (EBS) is a poorly water-soluble antihistaminic drug; it belongs to the class II group according to the biopharmaceutical classification system (BCS). The aim of the present work was to enhance the solubility, dissolution rate and micromeritic properties of the drug, by formulating it as spherical crystal agglomerates by Quasi Emulsion Solvent Diffusion (QESD) method.
Spherical crystal agglomerates (SCAs) were prepared in presence of three solvents dichloromethane (DCM), water and chloroform as a good solvent, poor solvent and bridging solvent respectively. Agglomeration of EBS involved the use of some hydrophilic polymers like polyethylene glycol 4000 (PEG 4000), polyvinyl pyrrolidine K30 (PVP K30), D-?-tocopheryl
... Show MorePhotonic crystal fiber interferometers are used in many sensing applications. In this work, an in-reflection photonic crystal fiber (PCF) based on Mach-Zehnder (micro-holes collapsing) (MZ) interferometer, which exhibits high sensitivity to different volatile organic compounds (VOCs), without the needing of any permeable material. The interferometer is robust, compact, and consists of a stub photonic crystal fiber of large-mode area, photonic crystal fiber spliced to standard single mode fiber (SMF) (corning-28), this splicing occurs with optimized splice loss 0.19 dB In the splice regions the voids of the holey fiber are completely collapsed, which allows the excitation and recombination of core and cladding modes. The device reflection
... Show MoreThe limited availability of the two-circle diffractometer to collect intensity measurements down to the monoclinic system has been extended in a novel procedure to collect intensities for the triclinic system. The procedure involves the derivation of matrix elements from graphical representation of the reciprocal lattice. Offset of the origins of the upper layers from that of the zero-layer - characteristic of triclinic system - is determined and the 3 x 3 matrix elements are evaluated accordingly. Details of crystal alignment by X-rays for the triclinic system utilizing the intensities of equivalent reflections is described
To learn how the manner of preparation influences film development, this study examined film expansion under a variety of deposition settings. To learn about the membrane’s properties and to ascertain the optimal pretreatment conditions, which are represented by ambient temperature and pressure, Laser pressure of 2.5[Formula: see text]m bar, the laser energy density of 500[Formula: see text]mJ, distortion ratio ([Formula: see text]) as a function of laser pulse count, all achieved with the double-frequency Nd: YAG laser operating in quality-factor mode at 1064[Formula: see text]nm. MgxZn[Formula: see text] films of thickness [Formula: see text][Formula: see text]nm were deposited on glass substrates at pulse
... Show MoreIn this work, InSe thin films were deposited on glass substrates by thermal evaporation technique with a deposit rate of (2.5∓0.2) nm/sec. The thickness of the films was around (300∓10) nm, and the thin films were annealed at (100, 200 and 300)°C. The structural, morphology, and optical properties of Indium selenide thin films were studied using X-ray diffraction, Scanning Electron Microscope and UV–Visible spectrometry respectively. X-ray diffraction analyses showed that the as deposited thin films have amorphous structures. At annealing temperature of 100°C and 200°C, the films show enhanced crystalline nature, but at 300°C the film shows a polycrystalline structure with Rhombohedral phase with crystallites size of 17.459 nm. Th
... Show More