In the present work, the fabrication techniques of type of Nd +3-glass laser active
media : namely, Neodymium- Tellurite glass, where the glass system(TeO2(1-x) - BaOZnO-
Nd2O3x) for values of (X=1,1.5,2,2.5,3,3.5 wt%) was used.
Measurements have been taken for the signal of fluorescence spectrum of Nd+3- glass
samples. The fluorescence spectrum, for one of the samples, has been taken, after the
sequences of polishing for the out surface.
The results give signal of fluorescence spectrum for the samples. Intensity of the peak of
the signal increases with Nd +3 concentration. The fluorescence at (l=1.06 mm) for one
of the samples has been detected and the fluorescence line width was (100 cm-1). The
cross section of stimulated emission for this type of laser active media (sp(lp=1.06
mm)=3.59*10-20 cm2), and the results compared with the published data.
The aim of this work is to study the influence of the type of fiber glass –mat on fatigue behavior of composite material which is manufactured from polyester and E-glass (woven roving, chopped strand mat (CSM)) as a laminate with a constant fiber volume fraction (VF) of 33%. The results showed that the laminates reinforced with E-glass (woven roving) [0/90, ±45.0/90] and [0/90, CSM, 0/90] have lower fatigue strength than the laminates reinforced with E-glass [0/90]3,[CSM]3 and [CSM, 0/90, CSM] although they had different tensile strength; the best laminate was [0/90]3 .
Vitrifications process one of the important methods to immobilize nuclear waste. In this research nuclear waste (Strontium Oxides) with molecular weight (5%) was immobilized by vitrification methods in two types of borosilicate glass (c-type) which are glass and glass-ceramics. To investigate the physical, chemical and mechanical properties of glass and glass-ceramic after immobilize nuclear waste these samples irradiated by gamma ray radiation. Co-60 was used as gamma a irradiation with dose rate 0.38 kGy/hr for different period of time. It’s found that gamma radiation affected the glass and glass-ceramic properties. From phase analysis by the x-ray diffraction for glass-ceramic samples proved that at doses 343kGy change the cry
... Show MoreLandfill and incineration are the most common and widely used methods to dispose of solid wastes; both of these techniques are considered the main sources of pollution in the world due to the harmful toxic emissions that are considered an environmental problem. Because of the large areas used by landfills, they are not always considered an economical method. With the increase in the production of solid materials, solid wastes increase the pressure on incinerators and landfills, making the environmental pollution hazard more serious. Instead, these waste materials can be used in some other applications. One of the most important of these applications is asphalt pavements, which are the most used types of pavements in the
... Show MoreThe most important environmental constraints at the present time
is the accumulation of glass waste (transparent glass bottles). A lot of
experiments and research have been made on waste and recycling
glass to get use it as much as possible. This research using recycling
of locally waste colorless glass to turn them into raw materials as
alternative of certain percentages of cement to save the environment
from glass waste and reduce some of the disadvantages of cement
with conserving the mechanical and physical properties of concrete
made. A set of required samples were prepared for mechanical test
with different weight percentage of waste glass (2%, 4%, 5%, 6%,
8%, 10%, 15%, 20% and 25%). American standard
This research is devoted to study the effect of different in weight percentage of Sio2 particles and glass fibers (5, 10, 15, 20) wt. % on the wear rate epoxy resin. The results show that the value of hardness increase with the increase for the weight percentage of reinforcing particles and fibers, while the wear rate decrease with the increase the load level of the reinforcing particles and fibers . The largest value of the hardness, and the lowest value of the wear rate for epoxy reinforced with 20% of SiO2, the wear rate increase in general with increasing the applied load.
The using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreThe using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreBackground: This study aimed to compare the surface microhardness (MH) and mineral content of white spot lesions(WSLs) after using bioactive glass (BAG)casein phosphopep-tides-amorphous calcium phosphate(CPP-ACP),and nanohydroxyapatite(Nano-HAP) under pHcycling. Material and method:18 sound maxillary first premolar were used for the study.10 were selected for the vickers microhardness test, For Energy-dispersive X-ray spectroscopy analysis (EDX), the remaining 8 premolar teeth were used, 40 sections of enamel blocks (Four from each tooth) were produced from the middle part of the buccal and palatal surfaces of teeth for MH test while 48 sections of enamel blocks (Six from each tooth) were produced for EDX analysis. Enamel slabs were
... Show MoreThe using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreEnamel White Spot Lesions (EWSLs) are a common dental condition characterized by being opaque or chalky white in appearance. In this review, an overview of the etiology, prevention, and treatment techniques for EWSLs is presented. Enamel demineralization caused by bacteria in dental plaque which releases acids upon the consumption of fermentable carbohydrates causing mineral loss is thought to be the main cause of those lesions, which could be predisposed through orthodontic treatment, poor diet, inadequate oral hygiene and certain medical conditions. So, sustaining an adequate carbohydrate consumption, proper fluoride exposure and good oral hygiene are some of the practices which aid in these lesions’ prevention. Although the suc
... Show More