CR-39 is a solid state nuclear track detector (SSNTD) that has been used in many research areas. In spite of the assumption that the CR-39 detectors are insensitive to beta and gamma rays, irradiation with these rays can have significant effects on the detector properties. In this study, beta and gamma rays mass attenuation coefficients μ/ρ (cm2 g-1) for the CR-39 detector have been measured using NaI(Tl) scintillation spectrometer along with a standard geometrical arrangement in the energy region of (0.546-2.274) MeV beta rays and standard gamma sources having energy 0.356, 0.5697, 0.6617 and 1.063 MeV. The total atomic cross-section (σtot), total electronic cross-section (σT E) and the effective atomic number (Zeff) of gamma rays at energy of 1keV- 105 MeV have been also calculated using the Winxcom and MathCAD programs. The data base and the calculated results were compared with the measured experimental values. It has been found that the mass attenuation coefficients vary with the type of interaction of radiation, photoelectric interaction gives dominant contribution to the total mass attenuation coefficients for CR-39 detectors. Further, the Zeff changes with change of energy.
A gamma T_ pure sub-module also the intersection property for gamma T_pure sub-modules have been studied in this action. Different descriptions and discuss some ownership, as Γ-module Z owns the TΓ_pure intersection property if and only if (J2 ΓK ∩ J^2 ΓF)=J^2 Γ(K ∩ F) for each Γ-ideal J and for all TΓ_pure K, and F in Z Q/P is TΓ_pure sub-module in Z/P, if P in Q.
Autorías: Amwag Mohammed Ali Qasim, Ghassan Adeeb Abdulhasan. Localización: Revista iberoamericana de psicología del ejercicio y el deporte. Nº. 6, 2021. Artículo de Revista en Dialnet.
paper
Abstract
Corrosion-fatigue occurs by the combined actions of cyclic loading and corrosive environment. The effect of shot peening on cumulative corrosion-fatigue life of 1100-H12 Al alloy was investigated. Before fatigue testing, specimens were submerged in 3.5%NaCl solution for 71 days. Constant fatigue tests were performed with and without corrosive environment. Cumulative corrosion-fatigue tests were also carried out in order to determine the fatigue life before and after shot peening. The constant fatigue life was significantly reduced due to corrosive environment and the endurance fatigue limit was reduced by 13% compared with dry fatigue. In case of shot peening the cumul
... Show MoreObjective : Multiple sclerosis (MS) is a common neurological disease deeply linked with the immune-inflammatory disorders whereas the term (multiple) mostly refers to the multi-focal zones of Inflammation caused by lymphocytes and macrophages infiltration besides oligodendrocytes death. Accordingly , the dysfunctional immune system able to damage myelin ( a pivotal component of the central nervous system ) which responsible for communication among neurons. The aim of the present study is to innovate a biochemical relationship between MS and thyroid hormones (THs) by highlighting immunological responses and also to examine the action of Interferon beta (IFNβ) drug on thyroid hormone (THs) and thyroid stimulation hormone (TSH). Materials and
... Show MoreBackground: Beta thalassemia is a typically autosomal recessive form of severe anemia which is caused by an imbalance of two types of protein (alpha and beta) subunits of hemoglobin. Oxidative stress imbalance is the equilibrium between pro-oxidant\antioxidant statuses in cellular system, which results in damaging the cells. Antioxidant is a chemical that delays the start or slows the rate of lipid oxidation reaction and it play a very important role in the body defense system against reactive oxygen species. The aims of this study were to recorded the oro-facial manifestations in beta thalassemic patients and assess the oxidative stress marker malondialdehyde in serum and salivs and their role in the pathogenesis of beta thalassemia and ev
... Show MoreThe creation and characterisation of biodegradable blend films based on chitosan and polyvinyl alcohol for application in a range of packaging is described. The compatibility between the chitosan and PVA polymers was good. Composite films had a compact and homogeneous structure, according to the morphology analysis. The mechanical test result of PVA/CH at concentrations 5% showed, that The higher values of TS recorded in sample (p1, with 40 MPa) while the lower values appeared in sample (p9, with 22.09 MPa), the TS decreased gradually as the amount of PVA increased in blend film. While the blend film of pure Chitosan exhibits a poor mechanical strength which makes it a poor candidate for packaging but Blending CH with PVA together improved
... Show MoreConstruction projects have become a changing dramatically in recent decades and that the goal of the beneficiaries of the implementation of structural project is to complete the work with less time and within the cost of the specific and the best possible quality may sometimes happen that highlights the importance of time on the rest of the items at the implementation of projects for various reasons, including the need to use the project as soon as possible possible change rapidly to customer's requests, but the high cost of the project represents the biggest obstacle for entrepreneurs with its effects on the quality and the time workers, and is a measure of those elements in monetary terms is the key to integration between them, so the
... Show More