This paper was aimed to evaluate the polyurethane (PU) and polyurethane/polyvinyl chloride (90 wt. % / 10 wt. %) as organic coating of carbon steel substrate against marine environment (3.5 wt.% NaCl aqueous solution) as a severe corrosion environment . The electrochemical impedance spectroscopy (EIS) and fitting impedance data by ZsimpWin 3.22 software were used to estimate the physical barrier of the samples for different exposure times. Different equivalent electrical circuits were proposed for the physical barrier at different immersion times to get appropriate fitting .Both PU and PU/PVC coatings showed excellent corrosion protection ability for steel .The PU/PVC coating showed better protection and stability than PU coating against aggressive salt solution. The relation between dielectric properties (impedance spectrum) of coating film with their behavior as physical barrier protection gave useful information about electrochemical process and predicts the barrier protective behavior in natural environment.
Abstract The aim of this research is to show the grade of implementation of ISO 26000 (Social Responsibility Standard), specifically which related in clause sex (consumer issues), this study was achieved in Market Research and Consumer Protection Center (MRCPC) / University of Baghdad. The seven consumer issues of ISO 26000 was analyzed to show the extent of its implementation in MRCPC depending of using a check list as a principle instrument to collect research data and information. Results analysis was achieved by percentages and mean average. The research was leaded some of results and the most importance one was that the grade of implementation of the center in related to consumer issues given in the standard was medium
The using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreThe using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreThe using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreIn this work, functionally graded materials were synthesized by centrifugal technique at different
volume fractions 0.5, 1, 1.5, and 2% Vf with a rotation speed of 1200 rpm and a constant rotation time, T
= 6 min . The mechanical properties were characterized to study the graded and non-graded nanocomposites
and the pure epoxy material. The mechanical tests showed that graded and non-graded added alumina
(Al2O3) nanoparticles enhanced the effect more than pure epoxy. The maximum difference in impact strength
occurred at (FGM), which was loaded from the rich side of the nano-alumina where the maximum value was
at 1% Vf by 133.33% of the sample epoxy side. The flexural strength and Young modulus of the fu
Numerous tests are recently conducted to assess vibration's role in accelerating the heat transfer rate in various heat exchangers. In this work, the enhancement of heat transfer by the effect of transfer vibration and inclination angles on the surface of a double pipe heat exchanger experimentally has been investigated. A data acquisition system is applied to record the data of temperatures, flow rates, and frequencies over the tests. A compound technique was adopted, including the application of a set of inclination angles of (0°, 10°, 20°, and 30°) under the effect of frequency of vibration ranging from sub-resonance to over-resonance frequencies. The results showed that the overall heat transfer coefficient enhan
... Show MoreMercuric chloride (HgCl2) pollution and poisoning has been a worldwide health concern for decades, especially after the industrial revolutions. The aim of this study was to investigate the role of resveratrol in reversing the deleterious effects of HgCl2 exposure to resume the normal functions of hepatocyte. To achieve the study, mature Sprague Dawley rats were assigned to five groups. Negative control group (C) kept without any treatment; vehicle-treated group (D) received dimethyl sulfoxide (DMSO); resveratrol-treated group (R), received 100 mg/kg of resveratrol; HgCl2-intoxicated group (HD), received i.p. injection of HgCl2 at a dose of 1 mg/kg for 30 consecutive days along to oral gavage of DMSO; and finally H
... Show More