Fabrication of porous clay refractory insulating specimens from Iraqi kaolin with different percentage of Expanded Polystyrene (EPS) waste crumbs additions were investigated. After mixing and forming by hand molding, the specimens was dried and fired at 1300 oC. The structural, physical, mechanical and thermal properties of the refractory insulating products were measured. Maximum addition of EPS (1.25 wt%) lead to reduce the linear shrinkage to less than 1.7% and increased apparent porosity up to 50 %. As well as, the density, Modulus of rupture and thermal conductivity were reduced to 1.39 g/cm3, 4.1 MPa and 0.21 W/m.K, respectively. The final outcome, addition of EPS showed good results in the formation of pores without distorting the dimensions of specimens and without any cracks. In addition, it is possible to use these thermal insulators at temperatures up to 1300 oC.
In this study, the adsorption of Zn (NO3)2 is carried out by using surfaces of malvaparviflora. The validity of the adsorption is evaluated by using atomic absorption Spectrophotometry through determination the amount of adsorbed Zn (NO3)2. Various parameters such as PH, adsorbent weight and contact time are studied in terms of their effect on the reaction progress. Furthermore, Lagergren’s equation is used to determine adsorption kinetics. It is observed that high removal of Zn (NO3)2 is obtained at PH=2. High removal of Zn (NO3)2 is at the time equivalent of 60 min and reaches equilibrium,where 0.25gm is the best weight of adsorbant . For kinetics the reaction onto malvaparviflora follows pseudo first order Lagergren’s equation.
A total of four types of instant dry yeast
Reaction of,2- [( 4- amio phenyl ) diazenyl] 1,3,4- thiadiazole -5- thiol (S1) with p- chlorobenzeldehyde,3,4 – dimethoxy benzaldehyde and pyrrol-2- carbonxaldehyde gave -5- [{4-(4-chlorobenzylidene amino) phenyl} diezenyl]-1,3,4- thiadiazole-2- thiol (S2),5-[{ 4-[(3,4- dimethoxybenzyldene )amino phenyl ] diazenyl)-1,3,4- thiadiazole-2-thiol,(S3) and -5- [4-(1,H – pyrrol -2- yl- methylene)amino phenyl] diazenyl)-1,3,4- thiadiazole-2- thiol (S4) respectively as schiff's bases compounds. On the same route-2-[(4-amino-1- naphthyl ) diazenyl] -1,3,4- thiadiazole -5- thiol (S5) reacts with –p- chloro benzaldehyde and –m- nitrobenzaldehyde to give the follwing schiff's bases -5-[{ 4-(4- chloro benzylidene ) amino -1- naphthyl} diazenyl]
... Show MoreSchiff bases were prepared prepared Baaan NMR to some elements of which have contributed to the results of different methods in diagnosis prove structural formulas of compounds prepared
A new series polymers was synthesized from reaction starting material Bisacodyl A or [(2-Pyridinylmethylene) di-4, 1-phenylene di acetate] with hydrogen bromide, then the products were polymerized by addition polymerization from used adipoyl and glutaroyl chloride. The structure of these compounds was characterized by FT-IR, melting points, TLC, X-Ray, DSC and 1H-NMR for starting material. These compounds were also screened for their antibacterial activists?
Catalase (EC 1.11.1.6) is a well known enzyme which exists in almost all living creatures exposing to oxygen (such as plants, bacteria, and animals). It is a very necessary enzyme to protect the cell from oxidative detriment by reactive oxygen species (ROS). The aim of this study is the partial purification and characterization of Catalase enzyme from Banana peels. In this study, fresh banana peels are treated with 70 % ethanol ,further separated with chloroform ,water and ethyl acetate respectively .The supernatant of the enzymatic sample which is treated with chloroform is loaded into gel filtration column with Sephadex G-100 (1.0 x 90 cm) equilibrated with pH7 buffer media (phosphate buffer 0.1 M). Kinetic studies of the purified en
... Show MoreIn this study, crop residues from rice husks were used to enhance the properties of the prepared
wood-plastic composites (W.P.C) are made from epoxy (EP) and unsaturated polyester (UPE) at
a ratio of (50:50) and reinforced with scales in different proportions, both types are fine
(300μm≤) and coarse (300μm>). These blends were undergoing (wear, impact, hardness,
differential scanning calorimetry (DSC), and thermal conductivity) tests and the results showed
the best weight fraction. is the fine particle weight fraction at 25% and coarse at 15%, depending
on the studied tribological characteristics. The results showed by thermal properties of glass
transition temperatures (Tg). For each of the (EP,