The present work aimed to study the SiO2μPs, and NPs effect on the biodegradability of St/PVA blends. The samples were prepared by casting method as PVA, St/PVA blends with different concentrations (30, 40, 50, and 60 %). FTIR test was carried out for the samples preparation. The results proved some changes which might be related to changing in crystallinity of St/PVA matrix as well as physical incorporation of SiO2 μPs, and NPs addition. The enzymatic test and water uptake results proved that increase in weight loss with increases of starch ratio. The lowest weight loss was PVA; the highest weight loss is 60% St/PVA whereas the lowest weight loss is 30%St/PVA for blends involved. SiO2μPs (753.7 nm), and NPs (263.1 nm) were added at different concentrations (1.5, 2, and 2.5 %). 1.5% SiO2 μPs, and NPs were the lowest weight loss then it was increased by SiO2μPs, and NPs addition. The samples were investigated with optical microscope. It was concluded that the samples involved could be used as packaging materials for medical application and its degradation could be controlled by SiO2μPs, and NPs addition.
By- products of corn starch industry were used to prepare media for propagation the lactic acid bacteria as a natural auxotroph. The by- products used were the corn steep water (S) and gluten extract (G) after a proper treatment to get them ready for media preparation. The results showed that it was possible to replace the peptone and meat extract by gluten extract in MRS medium. The growth was approximately similar to that obtained in standard MRS media. Corn steep water (S) was used as well and the growth enhanced by including Tween – 80 at 1% level. The later media named MZ, which was superior for growing standard and local strains and starters. The MZ medium modified by adding acetate and glacial acetic acid similarly to
... Show MoreThe polymeric hydrogels composed of poly vinyl alcohol (m.wt 72000) and glutaraldehyde(5%,8% and 10%) , have been thermally prepared for the purpose of studying their swelling and drug release behavior . The swelling ratio was measured for all the hydrogel samples at 37°C, in three different media pH (1.2, 4.7 and 6.8) as a function of time. The results show that the maximum swelling ratios were arranged as follows :pH =6.8 > pH =4.7 > pH =1.2 hydrogels cross linked PVA showed a typical pH responsive behavior such as high pH has maximum swelling while low pH shows minimum swelling.
The electrical characteristics of polyvinyl alcohol PVA doped with different concentrations (0, 1, 2, 3 and 4wt%) of sodium iodide NaI powder were studied. The films are prepared using solution casting technique, in order to investigate the effect of sodium iodide NaI additions on the electrical properties of PVA host. The D.C conductivity measured by measuring the D.C electrical resistance using the Keithly Electrometer type 616C, and for different temperatures ranging from 30 – 70oC.
The dielectric properties measured by measuring the capacitor and the loss
... Show MoreThe polymeric hydrogels composed of poly vinyl alcohol (m.wt 72000) and glutaraldehyde(5%,8% and 10%) , have been thermally prepared for the purpose of studying their swelling and drug release behavior . The swelling ratio was measured for all the hydrogel samples at 37°C, in three different media pH (1.2, 4.7 and 6.8) as a function of time. The results show that the maximum swelling ratios were arranged as follows :pH =6.8 > pH =4.7 > pH =1.2 hydrogels cross linked PVA showed a typical pH responsive behavior such as high pH has maximum swelling while low pH shows minimum swelling.
The aim of this research is to employ starch as a stabilizing and reducing agent in the production of CdS nanoparticles with less environmental risk, easy scaling, stability, economical feasibility, and suitability for large-scale production. Nanoparticles of CdS have been successfully produced by employing starch as a reducing agent in a simple green synthesis technique and then doped with Sn in certain proportions (1%, 2%, 3%, 4%, and 5%).According to the XRD data, the samples were crystallized in a hexagonal pattern, because the average crystal size of pure CdS is 5.6nm and fluctuates in response to the changes in doping concentration 1, 2, 3, 4, 5 %wt Sn, to become 4.8, 3.9, 11.5, 13.1, 9.3 nm respectively. An increase in crystal
... Show MoreAs modern radiotherapy technology advances, radiation dose and dose distribution have improved significantly. As part of a natural evolution, there has recently been renewed interest in therapy, particularly in the use of heavy charged particles, because these types of radiation serve theoretical advantages in all biological and physical aspects. The interactions of alpha particle with matter were studied and the stopping powers of alpha particle with Breast Tissue were calculated by using Beth-Bloch equation, Zeigler's formula and SRIM software, also the Range and Liner Energy Transfer (LET) and Breast Thickness As well as Dose and Dose equivalent for this particle were calculated by using Mat lab language for (0.01-200) MeV alpha ene
... Show MoreNuclear medicine is important for both diagnosis and treatment. The most common treatment for diseases is radiation therapy used against cancer. The radiation intensity of the treatment is often less than its ability to cause damage, so radiation must be carefully controlled. The interactions of alpha particle with matter were studied and the stopping powers of alpha particle with ovary tissue were calculated using Beth-Bloch equation, Zeigler’s formula and SRIM Software also the range and Liner Energy Transfer (LET) and ovary thickness as well as dose and dose equivalent for this particle were calculated by using Matlab language for (0.01-200) MeV alpha energy.
The interlaminar fracture toughness of polymer blends reinforced by glass fiber has
been investigated. Epoxy (EP), unsaturated polyester(UPE), polystyrene (PS),
polyurethane (PU) and their blends with different ratios (10%PS/90%EP),
(20%PS/80%EP), (20%PU/80%EP) and (20%PU/80%UPE) were chosen as a matrices A
sheet of composites were prepared using hand lay -up method, these sheet were cut as the
double cantilever beam (DCB) specimen to determine interlaminar fracture toughness of
these composites .Its found that, blending of EP,UPE with 20% of PU will improve the
interlaminar fracture toughness ,but the adding of 10% PS, 20%PS to EP will decrease
the interlaminar toughness of these composites.
The mass attenuation coefficient for beta particles through pure Polyvinyl chloride (PVC) and flax fibers- reinforced PVC composite were investigated as a function of the absorber thickness and the absorber to source distance. The beta particles mass attenuation coefficients were obtained using a NaI(Tl) energy selective scintillation counter with 90Sr/ 90Y beta source having an energy range from (0.546-2.275) MeV. Pure PVC polymer samples were prepared by compacting the PVC powder in a mould at high pressure (10bar) and temperature about 140°C for 30 minutes. A hot press system was used for this process. The experimentally obtained values of mass attenuation coefficients for 90Sr and 90Y were found to be 7.72 cm2.g-1and 0.842 cm2.g-1 r