In this work, the copper metal was treated using Nd:YAG laser with energy 1Joul to enhance corrosion resistance and improve surface properties. The copper metal has many applications in industry as well as water, oil and gas pipes. The same conditions, (laser power density, scan speed, distance between paths, medium gas-air) were applied in the laser surface treatment, After laser treatment, the samples microstructures were investigated using optical microscope (OM) to examine micro structural changes due to laser irradiation. Specimen surfaces were investigated using atomic force microscopy (AFM), X-ray diffraction (XRD), macro hardness, and corrosion test before and after laser treatment to examine the surface properties changes as a result of laser irradiation, and X-ray fluorescence (XRF). Results showed that laser irradiation enhances the corrosion resistance of the metal copper. Corrosion rates as low as 0.550 mpy for laser treated samples were obtained in comparison to 0.699 mpy obtained for the untreated samples. The corrosion protection afforded by laser treatment is attributed mainly to the grain refinement of the top surface layer. This layer is found to consist of nano-scale grains. Higher hardness and lower average roughness due to laser surface treatment.
Magnesium Phthalocyanine (MgPc) was deposited on a glass substrate by pulsed laser deposition (PLD) using Q-Switching Nd:YAG laser with wavelength 1064 nm, repetition rate 6 Hz, at room temperature (300K) and different annealing temperatures (373, 473, and 573)K under vacuum condition of 10-3 torr. All films were annealed for one hour to attain crystallinity. X-ray diffraction (XRD) of MgPc powder indicated that MgPc crystallizes in polycrystalline with a monoclinic structure. While comparing the MgPc films, it was observed that the intensity of the characteristic peak increases with temperature, and the crystallization exhibited a monoclinic structure typical of the β-form. The Miller indices, hkl, values for each diffraction peak
... Show MoreThe incorporation of safety characteristics into the traditional pavement structural design or in the functional evaluation of pavement condition has not been established yet. The design has focused on the structural capacity of the roadway so that the pavement can withstand specific level of repetitive loading over the design life. On the other hand, the surface texture condition was neither included in the AASHTO design procedure nor in the present serviceability index measurements.
The pavement surface course should provide adequate levels of friction and ride quality and maintain low levels of noise and roughness. Many transportation departments perform routine skid resistant testing, the type of equipment us
... Show MoreThe project has been described the design and construction of a reliable optical testing platform used for evaluate the reflectivity of metal surfaces treated with special paintings required for laser beam attenuation. The platform comprises an Nd-YAG laser system which has been designed and fabricated with specifications to be compatible with their corresponding in laser range finder transmitters used for various applications. The reflectivity of various attenuating paintings, at different detection angles, has been observed. Moreover, the variation of the reflected energy with painting type and metal type to be painted has been studied experimentally. Results illustrated the existence of a definite angle, at which the reflectivity was max
... Show MoreIn this work, studying the effect of ethylenediamine as a corrosion inhibitor was investigated for carbon steel in aerated HCl solution in range of 0.1-1N under dynamic conditions, i.e., rotational velocity of 400–1200 rpm in the temperature range 35 – 65 ºC. Weight loss method was employed in absence and presence of the inhibitor as an adsorption type in concentration range 1000 – 5000 ppm using rotating cylinder specimens. The experimental results showed that corrosion rate in absence and presence of inhibitor is increased with increasing temperature, rotational velocity and concentration of acid. It is decreased with increasing inhibitor concentration for the whole range of temperature, rotational velocity and concentrati
... Show MoreAbstract
Magnetic abrasive finishing (MAF) process is one of non-traditional or advanced finishing methods which is suitable for different materials and produces high quality level of surface finish where it uses magnetic force as a machining pressure. A set of experimental tests was planned according to Taguchi orthogonal array (OA) L27 (36) with three levels and six input parameters. Experimental estimation and optimization of input parameters for MAF process for stainless steel type 316 plate work piece, six input parameters including amplitude of tooth pole, and number of cycle between teeth, current, cutting speed, working gap, and finishing time, were performed by design of experiment
... Show MoreIn the current research, we investigated the absorption spectrum for R590 and C480 dyes in ethanol solvent for different dye solution concentrations of 10-4, 10-5 and 10-6M. These dyes have been prepared and studied before and after gamma irradiation (first, second ionization) using cesium-137 source with absorbed doses of 18.36 Gy (time exposure of 10 days) and 73.44 Gy (with time exposure of 40 days). We noticed that the absorption intensity was decreased with decreasing concentration, before gamma irradiation while the absorption spectrum peak shifted towards the short wavelength (blue shift). It was also found that the intensity of absorption spectrum increased and shifted the absorption spectrum peak towards the long wavelength (red
... Show MoreThe corrosion of low carbon steel boiler tubes in demi water had been investigated. The purpose of this investigation was to determine the change produced in corrosion behavior of the carbon steel as a result of the specific presence of chloride and copper ions in the water under different temperatures. For low carbon steel experiments, the temperature was taken in three levels (125, 175, and 215°C) under about 27 bar pressure and 1500 rpm in autoclave. Using weight loss technique, the corrosion rate ranges from (85 to 789 gmd) for low carbon steel boiler tubes.