Optical and structural properties of synthesized ZnO nanorods through chemical bath deposition on various substrates

Chemical bath deposition was used to synthesize ZnO nanorods (NRs) on glass and fluorine_doped tin oxide (FTO) substrates. X-ray diffraction was performed to examine the crystallinity of ZnO nanorod. Results showed that ZnO NRs had a wurtzite crystal structure. Field emission scanning electron microscopy images showed that glass sample had rod-like structure distribution with (50 nm) diameter and average length of approximately (700 nm), whereas the FTO-coated glass sample had 25 nm diameter and average length of approximately 950 nm. The direct optical transition band gaps of the glass and FTO_coated glass samples were( 4 and 4.43 eV), respectively. The structural and optical properties of the synthesized ZnO products were described. The grown ZnO NRs have good optical properties. The proposed method is simple, inexpensive, soft, and environmentally friendly compared with other methods, making it appropriate for the large-scale manufacturing of devices and other app1ications.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Thu May 11 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Effect Annealing Temperatures On The Structural Proerties of ZnO Thin Films Prepared By Chemical Bath Deposition

In this research, we study the changing structural properties of ZnO with changing annealing temp., in the range  (473-773)K prepared by chemical bath deposition method at temp. (353)K, where deposited on glasses substrates at thickness (500±25)nm, the investigation of (XRD) indicates that the (ZnO) films are polycrystalline type of Hexagonal.

            The results of the measuring of each sample from grain size, microstrain, dislocation density, integral breadth, shape factor and texture coefficient, show that annealing process leads to increase the grain size (26.74-57.96)nm, and decrease microstrain (0.130-0.01478), dislocation density (1.398-0.297)*1015

... Show More
View Publication Preview PDF
Publication Date
Wed Aug 01 2018
Journal Name
Materials Research Bulletin
Chemical bath deposition of single crystal SnS nanobelts on glass substrates

SnS nanobelt thin films were deposited on glass substrates in acidic solution by chemical bath deposition (CBD) method. The belt-like morphologies of as-deposited SnS thin films were characterized by scanning electron microscope (SEM) and transmission electron microscopy (TEM). X-ray diffraction (XRD) and Raman measurements were carried out to confirm the crystal structures and phase purities of SnS nanobelt thin films. The morphologies and phase purities of SnS thin films were influenced greatly by the tin and sulfur precursors. The bandgaps of SnS nanobelts were determined to be 1.39–1.41 eV by UV–vis absorption and photoluminescence (PL) spectra. Current-voltage ((I-V)) and current-time ((I-T)) characteristics were studied to demon

... Show More
Scopus (26)
Crossref (25)
Scopus Clarivate Crossref
View Publication
Publication Date
Sun Mar 07 2010
Journal Name
Baghdad Science Journal
The Effect of Thickness on Some Optical Properties of Sb2S3 Thin Films Prepared by Chemical Bath Deposition

Sb2S3 thin films have been prepared by chemical bath deposition on a glas sub Absorbance and transmittance spectra were recorded in the wavelength range (30-900) nm. The effects of thickness on absorption coefficient, reflectance, refractive index, extinction coefficient, real and imaginary parts of dielectric constant were estimated. It was found that the reflectivity, absorption coefficient , extinction coefficient, real part of dielectric constant and refractive index, all these parameters decrease as the thickness increased, while the imaginary part of the dielectric constant increase as the thickness incre

... Show More
Crossref (4)
Crossref
View Publication Preview PDF
Publication Date
Fri Dec 29 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Structure and Optical Properties of BhSe3 Thin Films Prepared by Chemical Bath Deposition Method

Thin films of  BhSe3  have being deposited on glass substrates of

about 80 - 172 ± 14 nm thickness from an aqueous solution bath at temperature 293 K for period 0.5 to 6.0 hours  using alchemical bath deposition method .

The  films  are  characterized   by  X-ray  diffraction,     X-ray

florescent techniques and optical transmittance spectra measurements in the rang 350 - 400 nm at 293 K. And shows that as deposited  films are amorphous and a  transition to polycrystalline state has taken place after  annealing  them  at  373  K,  for  30  minutes,  But  they  will  be dan1aged

... Show More
View Publication Preview PDF
Publication Date
Thu Dec 23 2021
Journal Name
Iraqi Journal Of Science
Structural, Optical and Morphological Characterization of Cdse/Cds Core / Shell Quantum Dots Synthesized via Chemical Bath

     CdSe/CdS Core/shell nanostructures were prepared through the chemical synthesis method. XRD ,FESEM and TEM investigations confirmed the formation of core/shell structure for the sample. The AFM measurement was employed to reveal the morphology of the prepared thin films. Optical characterizations of the quantum dots were done by UV-visible and photoluminescence spectra. It was found that the quantum dots prepared has  good optical properties. Due to the presence of shell coating on core CdSe, the energy gap of the core/shell nanomaterial were increased from 2.2 to 2.3eV. The resulted QDs  are a promising candidate for photovoltaic and biosensor applications.

Scopus (3)
Crossref (3)
Scopus Crossref
View Publication Preview PDF
Publication Date
Tue Apr 05 2022
Journal Name
Nano Hybrids And Composites
Structural and Optical Properties of ZnO Nanostructures Synthesized by Hydrothermal Method at Different Conditions

Zinc oxide (ZnO) nanoparticles were synthesized using a modified hydrothermal approach at different reaction temperatures and growth times. Moreover, a thorough morphological, structural and optical investigation was demonstrated using scanning electron microscopy (SEM), x-ray diffraction (XRD), ultra-violate visible light spectroscopy (UV-Vis.), and photoluminescence (PL) techniques. Notably, SEM analysis revealed the occurrence of nanorods-shaped surface morphology with a wide range of length and diameter. Meanwhile, a hexagonal crystal structure of the ZnO nanoparticles was perceived using XRD analysis and crystallite size ranging from 14.7 to 23.8 nm at 7 and 8 ℎ𝑟𝑠., respectively. The prepared ZnO samples showed good abso

... Show More
Publication Date
Tue Apr 05 2022
Journal Name
Nano Hybrids And Composites
Structural and Optical Properties of ZnO Nanostructures Synthesized by Hydrothermal Method at Different Conditions

ZnO nanostructures were synthesized by hydrothermal method at different temperatures and growth times. The effect of increasing the temperature on structural and optical properties of ZnO were analyzed and discussed. The prepared ZnO nanostructures were characterized by X-ray diffraction (XRD), UV–Vis. absorption spectroscopy (UV–Vis.), Photoluminescence (PL), and scanning electron microscopy (SEM). In this work, hexagonal crystal structure prepared ZnO nanostructures was observed using X-ray diffraction (XRD) and the average crystallite size equal 14.7 and 23.8 nm for samples synthesized at growth time 7 and 8 hours respectively. A nanotubes-shaped surface morphology was found using scanning electron microscopy (SEM). The optic

... Show More
Crossref (2)
Clarivate Crossref
View Publication
Publication Date
Tue Feb 12 2019
Journal Name
Iraqi Journal Of Physics
Structural and optical properties of ZnO doped Mg thin films deposited by pulse laser deposition (PLD)

This paper reports the effect of Mg doping on structural and optical properties of ZnO prepared by pulse laser deposition (PLD). The films deposited on glass substrate using Nd:YAG laser (1064 nm) as the light source. The structure and optical properties were characterized by X-ray diffraction (XRD) and transmittance measurements. The films grown have a polycrystalline wurtzite structure and high transmission in the UV-Vis (300-900) nm. The optical energy gap of ZnO:Mg thin films could be controlled between (3.2eV and 3.9eV). The refractive index of ZnO:Mg thin films decreases with Mg doping. The extinction coefficient and the complex dielectric constant were also investigate.

Crossref (2)
Crossref
View Publication Preview PDF
Publication Date
Fri Jan 11 2019
Journal Name
Iraqi Journal Of Physics
Effect of thickness on the optical properties of ZnO thin films prepared by pulsed laser deposition technique (PLD)

Zinc Oxide (ZnO) thin films of different thickness were prepared
on ultrasonically cleaned corning glass substrate, by pulsed laser
deposition technique (PLD) at room temperature. Since most
application of ZnO thin film are certainly related to its optical
properties, so the optical properties of ZnO thin film in the
wavelength range (300-1100) nm were studied, it was observed that
all ZnO films have high transmittance (˃ 80 %) in the wavelength
region (400-1100) nm and it increase as the film thickness increase,
using the optical transmittance to calculate optical energy gap (Eg
opt)
show that (Eg
opt) of a direct allowed transition and its value nearly
constant (~ 3.2 eV) for all film thickness (150

... Show More
Crossref (3)
Crossref
View Publication Preview PDF
Publication Date
Wed Sep 12 2018
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Thickness Influence on Structural and Optical Properties of ZnO Thin Films Prepared by Thermal Evaporation

  A thermal evaporation technique was used to prepare ZnO thin films. The samples were prepared with good quality onto a glass substrate and using Zn metal. The thickness varied from (100 to 300) ±10 nm. The structure and optical properties of the ZnO thin films were studied. The results of XRD spectra confirm that the thin films grown by this technique have hexagonal wurtzite, and also aproved that ZnO films have a polycrystalline structure. UV-Vis measurement, optical transmittance spectra, showed high transmission about 90% within visible and infrared range. The energy gap is found to be between 3.26 and 3.14e.V for 100 to 300 nm thickness respectivly. Atomic Force Microscope AFM (topographic image ) shows the grain size incre

... Show More
Crossref (1)
Crossref
View Publication Preview PDF