PMMA/TiO2 homogeneous thin films were deposited by using plasma jet system under normal atmospheric pressure and room temperature. PMMA/TiO2 nanocomposite thin film synthesized by plasma polymerization. Titanium oxide was mixed with Methyl Methacrylate Monomer (MMA) with specific weight ratios (1, 3 and 5 grams of TiO2 per 100 ml of MMA). Optical properties of PMMA/TiO2 nanocomposite thin films were characterized by UV-Visible absorption spectra using a double beam UV-Vis-NIR Spectrophotometer. The thin films surface morphological analysis is carried out by employing SEM. The structure analysis are achieved by X-ray diffraction. UV-Visible absorption spectra shows that the increasing the concentration of titanium oxide added to the polymer leads to shift the peak position (λmax) toward the infrared region of the electromagnetic spectrum. Also the peak width increases when the concentration of TiO2 increases. It can be controlled optical energy band gap of PMMA/TiO2 nanocomposite thin films by changing concentration of TiO2. SEM indicate a uniform distribution of titanium oxide particles in PMMA matrix. The x-ray diffraction pattern indicated that the thin films have amorphous structure.
Traditional healthcare for chronic wounds and Cold Atmospheric Plasma (CAP) treatments relies on passive dressings and large-volume stationary equipment operating with open-loop systems, which severely limits their use and confines it to specialized clinical environments. To address the lack of active thermal safety mechanisms in mobile devices, this research proposes a wearable smart plasma patch equipped with a closed-loop adaptive electronic control system to ensure safe patient care and treatment at home. The smart patch integrates real-time analog biosensors to continuously monitor skin temperature and relative humidity. An algorithm running on a microcontroller dynamically adjusts the high-voltage plasma parameters using Pulse
... Show MoreA new scheme of plasma-mediated thermal coupling has been implemented which yields the temporal distributions of the thermal flux which reaches the metal surface, from which the spatial and temporal temperature profiles can be calculated. The model has shown that the temperature of evaporating surface is determined by the balance between the absorbed power and the rate of energy loss due to evaporation. When the laser power intensity range is 107 to108 W/cm2 the temperature of vapor could increase beyond the critical temperature of plasma ignition, i.e. plasma will be ignited above the metal surface. The plasma density has been analyzed at different values of vapor temperature and pressure using Boltzmann’s code for calculation of elec
... Show MoreBackground: The preparation of Platelet-rich plasma (PRP) is minimally invasive way, simple, low cost to obtain natural autologous growth factors and is now being widely used in different fields of medicine for its ability to increase the regeneration potential of tissue. The aim of this study was to investigate the effect of local application of autologous PRP gel on acceleration rate of osseointegration period by clinical assessment accomplished by determining the changes in implant stability during 3 months healing period using resonance frequency analysis (RFA). Materials and methods: A total of 28 dental implants were inserted in edentulous maxillae or mandibles of 13 patients using a split mouth design, i.e. each patient was received
... Show MoreIn this work, radius of shock wave of plasma plume (R) and speed of plasma (U) have been calculated theoretically using Matlab program.
In this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest degradation percent. In additio
... Show MoreIn this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest degradation percent. In additio
... Show MoreIn this research, we studied the effect of concentration carriers on the efficiency of the N749-TiO2 heterogeneous solar cell based on quantum electron transfer theory using a donor-acceptor scenario. The photoelectric properties of the N749-TiO2 interfaces in dye sensitized solar cells DSSCs are calculated using the J-V curves. For the 〖(CH_3)〗_3 COH solvent, the N749-TiO2 heterogeneous solar cell shows that the concentration carrier together with the strength coupling are the main factors affecting the current density, fill factor and efficiency. The current density and current increase as the concentration increases and the strength coupling increases as the N749-TiO2 heterogeneous in solar cell. However, the efficiency is more sens
... Show MoreTitanium dioxide nanotube arrays (TiO2 NTAs) were successfully decorated with nanoclusters of cobalt by an electrochemical deposition method. This Co-TiO2 NTAs nanostructure exhibited high compatibility with aluminum chloride\ chloroacetamide (an ionic liquid) and calcium chloride dihydrate\ acetamide (a deep eutectic solvent), leading to significant improvements in the electrochemical properties of the system. Significantly, this led to a discernible augmentation in both potential and current values, concomitant with a decrease in internal resistance. The presence of cobalt facilitated a faster transfer of electric charge, enhancing the overall efficiency of the system. Moreover, the incorporation of cobalt exhibited a ben
... Show MoreIn this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest deg
... Show More