This paper displays the effect of uncoated and coated chopped carbon fibers with alumina Al2O3 or Tri calcium phosphate (TCP) on the impact strength of acrylic poly methyl methacrylate (PMMA) denture base resin. To improve bonding between carbon fibers and coating materials powders, the surface of carbon fibers has been treated with Para amino benzoic acid (C9H10N2O3) and poly vinyl alcohol (PVA) was also used. The morphology of the coating layers has been examined by field emission scanning electron microscope (FE-SEM). From the results, PMMA reinforced with uncoated chopped carbon fiber has high impact strength value but still have bad aesthetic. Samples prepared by coated carbon fiber with Al2O3 or TCP have high impact strength values when compared to control group with good aesthetic. Impact strength was increased in samples when PVA increased and fibers amount decreased.
Positron annihilation lifetime (PAL) technique has been employed to
study the microstructural changes of polyurethane (PU), EUXIT 101
and epoxy risen (EP), EUXIT 60 by Gamma-ray irradiation with the
dose range (95.76 - 957.6) kGy. The size of the free volume hole and
their fraction in PU and EP were determined from ortho-positronium
lifetime component and its intensity in the measured lifetime spectra.
The results show that the irradiation causes significant changes in the
free volume hole size (Vh) and the fractional free volume (Fh), and
thereby the microstructure of PU and EP. The results indicate that
the γ-dose increases the crystallinity in the amorphous regions of PU
and increas
Background: Color stability of glass ionomers (GIs) could be affected by many factors such as pH and consumption of liquid medications like antibiotics. Most common antibiotics used during childhood are amoxicillin suspension (AM.S) and azithromycin suspension (AZ.S) which have acidic and basic pH respectively. Aim: to evaluate and compare the effect of AM.S and AZ.S on color stability of nano resin-modified GI. Methods: Thirty disc of nano resin-modified glass ionomer (2mm height x 4mm diameter) were divided into three groups (n=10 for each) and independently exposed to AM.S, AZ.S, and artificial saliva (A.S.). Color stability was evaluated in triplicate by VITA Easyshade® before and after three immersion protocols, repeated over a thr
... Show MoreBackground: Color stability of glass ionomers (GIs) could be affected by many factors such as pH and consumption of liquid medications like antibiotics. Most common antibiotics used during childhood are amoxicillin suspension (AM.S) and azithromycin suspension (AZ.S) which have acidic and basic pH respectively. Aim: to evaluate and compare the effect of AM.S and AZ.S on color stability of nano resin-modified GI. Methods: Thirty disc of nano resin-modified glass ionomer (2mm height x 4mm diameter) were divided into three groups (n=10 for each) and independently exposed to AM.S, AZ.S, and artificial saliva (A.S.). Color stability was evaluated in triplicate by VITA Easyshade® before and after three immersion protocols, repeated over
... Show MoreThis study was design to investigate the dimensional stability of heat-activated acrylic resin with different methods of flask cooling (15 minutes rapid cooling, one hour bench cooling, four hours delayed deflasking, and 24 hours delayed deflasking) at different time intervals (immediately, two days, seven days, 30 days) after deflasking. Heat-activated acrylic resin was used to prepare acrylic samples. Then, measurement of the distances where achieved between the centers of selected marks in the acrylic samples. They were measured at different time intervals for different methods of flask cooling. The results showed that the group samples of the four hours and 24 hours of delayed deflasking was insignificantly different from the control an
... Show MoreThis study aims to find the effect of water-cement ratio on the compressive strength of concrete by using ultrasonic pulse velocity test (UPVT). Over 230 standard cube specimens were used in this study, with dimensions of 150mm, and concrete cubes were cured in water at 20 °C. Also, the specimens used in the study were made of concrete with varied water-cement ratio contents from 0.48 to 0.59. The specimens were taken from Diyarbakir-Turkey concrete centers and tested at the structure and material science lab, civil engineering, faculty of engineering from Dicle University. The UPV measurement and compressive strength tests were carried out at the concrete age of 28 days. Their UPV and compressive strength ranged
... Show MoreBackground: The bond strength of endodontic sealers with dentin is a very important property for maintaining the integrity and seal of the root canal filling. The aim of this study was to evaluate and compare the effect of various irrigants (QMix, 17% EDTA and 2.5% NaOCl) on the push-out bond strength of AH plus and Bioceramic sealers. Materials and methods: Forty eight freshly extracted maxillary first molars human teeth with striaght palatal root were used in the study. The collected samples were randomly divided into three groups of equal sample size (n=16), according to the final irrigation regimen as follows: Group (1): QMix 2 in 1, Group (2): 17% ethylenediaminetetraacetic acid, Group (3): 2.5% sodium hypochloride. All samples were
... Show MoreBackground: The aim of this study was to evaluate the push-out bond strength of four different obturation materials to intraradicular dentin and to determine the failure mode. Materials and method: forty straight palatal roots of the maxillary first molars teeth were used in this study, the roots were instrumented using crown down technique and rotary EndoSequence system, the roots were randomly divided into four groups according to the materials used for obturation (n=10).Group (1): AH Plus sealer and gutta-percha. Group (2): Activ GP glass ionomer sealer and Activ GP gutta-percha (Activ GP system). Group (3): Bioceramic sealer and Bioceramic gutta-percha. Group (4): GuttaFlow2 sealer and gutta-percha. For all groups single cone obturatio
... Show MoreDate palm fiber is one of the common wastes available in the M. E. countries essentially Iraq. The aim of search to investigate the performance and effects of fiber date palm on the mechanical properties of high strength concrete, this fiber was used in three ratio 2, 4 and 6 % by vol. of concrete at ages of (7, 28, 90) days. Results demonstrated improvement in the compressive strength increased 19.2 %, 23.6%, 24.9 % for 2%, 4%, 6% of fiber respectively at age 28 days. Flexural strength increases 47.6%, 66.2%, 93.8% form (2,4,6) % of fiber respectively at age 28 days. Density increase about 0.41%, 0, 61 % 0.69 % for (2,4,6) % of fiber respectively at age 28. Absorption water decrease
Water absorbent polymers (WAP) are new component in producing building materials. They provide internal curing which reduces autogenous cracking, eliminates autogenous shrinkage, mortar strength increased, enhance early age strength to withstand strain, improve the durability, introduce higher early age compressive strength, have higher performance and reduce the effect of insufficient external curing. This research used different percent of polymer balls to choose the percent that provides good development in compressive strength with time for both water and air curing. The water absorption polymer balls in this research have the ability to absorb water and after usage in concrete they spill out the water (internal curing) and shri