Fe, Co and Sb nanopowders were fruitfully prepared by electrical wire explosion method in Double distilled and de-ionized water (DDDW) media. The formation of iron, cobalt and antimony (FeCoSb) alloy nanopowder was monitored by X-ray diffraction. The x-ray diffraction pattern indicates that there are iron, cobalt and antimony peaks. Optical properties of this alloy nanoparticles were characterized by UV-Visible absorption spectra. The absorption peak position is shifted to the lower wavelengths when the current increases. That means the mean size of the nanoparticles controlled by changing the magnitude of the current. The surface morphological analysis is carried out by employing Scanning Electron Microscope (SEM). Particles with varies size were observed also from the images the some particles have uneven shapes with agglomerate and the other have spherical shape. The exploding FeCoSb alloy wire plasma parameters is study by optical emission spectroscopy. The emission spectra of the plasma have been recorded and analyzed. The plasma electron temperature (Te), was determined by Boltzmann plot, and the electron density (ne), by Stark broadening for wire with diameter 0.3 mm and current of 75A in distilled water.
There is currently a pressing need to create an electro-analytical approach capable of detecting and monitoring genosensors in a highly sensitive, specific, and selective way. In this work, Functionalized Multiwall Carbon Nanotubes, Graphene, Polypyrrole, and gold nanoparticles nanocomposite (f-MWCNTs-GR-PPy-AuNP) were effectively deposited on the surface of the ITO electrode using a drop-casting process to modify it. The structural, morphological, and optical analysis of the modified ITO electrodes was carried out at room temperature using X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM) images, atomic force microscopy (AFM) and Fourier transform infrared (FTIR) spectra. Cyclic voltammetry (CV) and electrochemi
... Show MoreThis research aims to examine the relationship between hydrothermal alteration and mineralization (ore mineralogy) in the study area and geological structures in the deformation mechanism. The hydrothermal alteration was determined based on petrographic analysis, and ore mineralogy which was determined based on the ore microscopic analysis. The deformation mechanism is determined by paleo stress analysis using win-tensor, and the direction of principal stress on joints/veins and faults is calculated by the right-dihedron method. Hydrothermal alteration includes silicification, argillic, propylitic, and phyllic alterations; and ore mineralogy consists of stibnite, cinnabar, pyrite, chalcopyrite, sphalerite, covellite, hematite, and a
... Show MoreIn this work, an important sugar alkynyl ether has been synthesized in two subsequent steps starting from commercially available D-galactose (3). This kind of compounds is highly significant in the synthesis of biologically active molecules such as 1,2,3-triazole and isoxazoles. In the first step, galactose (3) was reacted with acetone in the presence of anhydrous copper (II) sulfate to produce 1,2:3,4-di-O-isopropylidene-α-D-galactose (4) in good yield. The latter was reacted with excess of 3-bromoprop-1-yne in DMF in the presence of NaOH pellets to afford the target molecule 5 in a very good yield. The temperature of this step is crucial in determining the reaction yi
... Show MoreAu nanoparticle-functionalized (TiO2)1−x(ZnO:MgO)x nanocomposite thin films (0≤x≤0.3) were effectively produced by chemical spray pyrolysis and annealed at 600 °C. The effects of ZnO incorporation and Au nanoparticle modification on the films' structural, optical, and antibacterial properties were studied using X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), UV–Vis spectroscopy, and field-emission scanning electron microscopy (FESEM). XRD analysis confirms the formation of polycrystalline anatase TiO2 and shows a composition-dependent structural develop- ment with increasing ZnO concentration. The optical experiments revealed increased transmittance and a progressive wid- ening of the optical band gap f
... Show MoreIn this study, thin flms containing titanium dioxide (TiO₂), iron (III) oxide (Fe2O3) and cerium oxide (CeO2), with varying Fe2O3:CeO2 concentrations ranging from 0 to 30 wt% and 10 wt% gold nanoparticles (AuNPs), were prepared on glass using chemical spray pyrolysis. The structural, morphological, and sensing properties of the prepared thin flms were examined. XRD analysis revealed that a phase transformation occurred based on the dopant concentration: flms with x = 0 or 0.1 formed a polycrystalline anatase structure, whereas those with intermediate concentrations (x = 0.15 or 0.20) were amorphous. At higher doping concentrations (x = 0.25, 0.30), the structure developed a hematite Fe2O3, CeO2 and Au phase. Morphologicall
... Show MoreAu nanoparticle-functionalized (TiO2)1−x(ZnO:MgO)x nanocomposite thin films (0≤x≤0.3) were effectively produced by chemical spray pyrolysis and annealed at 600 °C. The effects of ZnO incorporation and Au nanoparticle modification on the films' structural, optical, and antibacterial properties were studied using X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), UV–Vis spectroscopy, and field-emission scanning electron microscopy (FESEM). XRD analysis confirms the formation of polycrystalline anatase TiO2 and shows a composition-dependent structural development with increasing ZnO concentration. The optical experiments revealed increased transmittance and a progressive widening of the optical band gap from 3
... Show MoreCopper oxide thin films were deposited on glass substrate using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature. The thickness of the thin films was around 0.43?m.Copper oxide thin films were annealed in air at (200, 300 and 400°C for 45min.The film structure properties were characterized by x-ray diffraction (XRD). XRD patterns indicated the presence of polycrystalline CuO. The average grain size is calculated from the X-rays pattern, it is found that the grain size increased with increasing annealing temperature. Optical transmitter microscope (OTM) and atomic force microscope (AFM) was also used. Direct band gap values of 2.2 eV for an annealed sample and (2, 1.5, 1.4) eV at 200, 300,400oC respect
... Show More