Exploding wire Technique is a way for production metal and its compound nanoparticle that is capable of production of bulk amount at low cost semiconductor. In this work a copper iodine nanoparticles were fabricate by exploding copper wires with different currents in iodine solution. The produced samples were examined by XRD, FTIR, SEM and TEM to characterize their properties. The XRD proved the Nano-size for producer. The crystalline size increases with increasing current. FTIR measurements show a peaks located at 638.92 for Cu-I stretch bond indicate on formation of copper iodide compound and the peaks intensities increase with increasing current. The SEM and TEM measurements show that the thin films have nanostructures.
The current study was conductedas a pot experiment to determine the effect of soil texture on biological nitrogen fixation (BNF) of six most efficient local isolates, specified, of Bradyrhizobium. Cowpea (Vignaunguiculata L.), as a legume host crop, was used as a host crop and 15N dilution analysis was used for accurate determination of the amount of N biologically fixed under experimental parameters specified. Soils used are clay loam, sandy clay loam and sandy loam. Biological Nitrogen Fixation (BNF), in different soil textural classes, was as in the following order: medium texture soil > heavy texture soil > light textured soil. Statistical analysis showed that there is a significant variation in BNF % among six Iraqi isolates in the th
... Show MoreFe, Co and Sb nanopowders were fruitfully prepared by electrical wire explosion method in Double distilled and de-ionized water (DDDW) media. The formation of iron, cobalt and antimony (FeCoSb) alloy nanopowder was monitored by X-ray diffraction. The x-ray diffraction pattern indicates that there are iron, cobalt and antimony peaks. Optical properties of this alloy nanoparticles were characterized by UV-Visible absorption spectra. The absorption peak position is shifted to the lower wavelengths when the current increases. That means the mean size of the nanoparticles controlled by changing the magnitude of the current. The surface morphological analysis is carried out by employing Scanning Electron Microscope (SEM). Particles with varies
... Show MoreIn this study, the results of x-ray diffraction methods were used to determine the Crystallite size and Lattice strain of Cu2O nanoparticles then to compare the results obtained by using variance analysis method, Scherrer method and Williamson-Hall method. The results of these methods of the same powder which is cuprous oxide, using equations during the determination the crystallite size and lattice strain, It was found that the results obtained the values of the crystallite size (28.302nm) and the lattice strain (0.03541) of the variance analysis method respectively and for the Williamson-Hall method were the results of the crystallite size (21.678nm) and lattice strain (0.00317) respectively, and Scherrer method which gives the value of c
... Show MoreProteases have various applications in the food, pharmaceutical, medicine, pathogenicity of some pathogenic bacteria, and detergent sectors as well as meeting the needs of approximately 60% of the global enzyme industry, whereas they catalyze the breakdown of protein molecules into peptides and amino acids. Production and purification of protease enzyme by the isolate Escherichia coli AJ55 was scrutinized in the present study. Cultivation optimum conditions, were various complex medium, carbon source, nitrogen source, temperature, pH of the medium, and time of incubation were optimized to enhance the total protease production in shake flask culture of E.coli AJ55. The nutrient broth supplemented with 2% gluco
... Show MoreA total of 48 experiments were conducted to investigate the impact of slit weir dimensions and locations on the maximum scour depth and scour area created upstream. The slit weir model was a 110 mm slit opening, and it was installed at the end of the working section in a laboratory flume. The flume was 10.0 m long, 30 cm wide, 30 cm deep, and almost middle. It includes a 2 m working section with a mobile bed with 110 mm in thickness. In the mobile bed, two types of nonuniform sand (with a geometric standard deviation of 1.58 and 1.6) were tested separately. The weir dimensions and location were changed with flow rates. Then dimensions of the slit weir were changed from 60 x 110 mm to 60 x 70 mm (width x height), while th
... Show More