The Q-switched Nd:YAG laser shock processing effects on mechanical properties of C86400 Cu-Zn alloy: Q-switched Nd:YAG laser shock processing effects on mechanical properties of C86400 Cu-Zn alloy
...Show More Authors

The aim of this paper is to investigate the effects of Nd:YAG laser shock processing (LSP) on micro-hardness and surface roughness of 86400Cu-Zn alloy. X-ray fluorescence technique was used to analyze the chemical composition of this alloy. LSP treatment was performed with a Q-switched Nd: YAG laser with a wavelength of 1064 nm. The results show that laser shock processing can significantly increase. The micro-hardness and surface roughness of the LSP-treated sample. Vickers diamond indenter was used to measure the micro-hardness of all samples with different laser pulse energy and the different number of laser pulses. It is found that the metal hardness can be significantly increased to more than 80% by increasing the laser energy and the number of laser pulse irradiated per unit area. The relationship between laser pulse energy and the value of surface roughness is a proportionality due to the increase in ablation processes which are associated with LSP at sample surface caused by the increasing of laser pulse energy.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Sun Jan 13 2019
Journal Name
Iraqi Journal Of Physics
Effect of tempering on thermal analysis of Al-Ti-Si alloy and its composites
...Show More Authors

The investigation of the effect of tempering on thermal analysis of
Al-Ti-Si alloy and its composites with MgO and SiC particles was
performed. Thermal analysis was performed before and after
tempering by DSC scan. Optical microscopy was used to identify the
phases and precipitations that may be formed in base alloy and
composites. X-ray diffraction test indicated that the Al3Ti is the main
phase in Al-Ti-Si alloy in addition to form Al5Ti7Si12 phase. Some
chemical reactions can be occurred between reinforcements and
matrix such as MgO.Al2O3 in Al-Ti/MgO, and Al4C3 and Al(OH)3 in
Al-Ti/SiC composite. X-ray florescence technique is used to
investigate the chemical composition of the fabricated specimens.
H

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Tue Mar 01 2022
Journal Name
Iraqi Journal Of Physics
Effect of Copper on Tensile and Hardness of Al-Si Alloy in Automotive Application
...Show More Authors

In current research Copper was employed for preparing a ternary system of Al–Si alloy in different (0.2–2.5 wt. %) the best was taken is (1.5%wt) of copper that circumstances of solidification for improving the mechanical performance of the available in aluminium alloy. Cast iron molds were prepared to obtain tensile strength testing specimens. Alloys were prepared by employing gas furnaces. The molten metal was poured into a preheated cast-iron mold. The obtained alloy structures were studied using an X-ray diffractometer and optical microscopy. The mechanical performance of the prepared alloys was examined under the influence of different hardening conditions in both heat and non-heat-treated conditions. The outcomes showed at the

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Fri Dec 29 2023
Journal Name
Iraqi Journal Of Agricultural Sciences
EFFECT OF ORGANIC FERTILIZER AND BORON FOLIAR ON QUANTITATIVE AND QUALTITATIVE TRAITS POTATO FOR PROCESSING
...Show More Authors

A field experiment was carried out at University of Baghdad, College of Agricultural Engineering Sciences during fall season of 2020 and spring season of 2021. This study was aimed evaluate the effect of the organic fertilizer and boron foliar on the yield of potatoes for processing. The factorial experiment (5*4) within RCBD and three replicates. The organic fertilizer as palm peat at four levels (0, 12, 24 and 36 ton. ha-1) in addition to the chemical fertilizer recommendation treatment. Boron at four Concentrations 0, 100, 150 and 200 mg. L-1 . The results revealed significant different among application of organic fertilizer at the level of 24 ton. ha-1 and the foliar application of boron at a concentration of 100 mg. L-1 in the

... Show More
Scopus (3)
Crossref (3)
Scopus Crossref
Publication Date
Mon Jun 30 2008
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
The Effect of Temperature and pH on the Removal / Recovery of ZN++ from Solution by Chemical Coagulation
...Show More Authors

This work was conducted to study the treatment of industrial waste water, and more particularly those in the General Company of Electrical Industries.This waste water, has zinc ion with maximum concentration in solution of 90 ppm.
The reuse of such effluent can be made possible via appropriate treatments, such as chemical coagulation, Na2S is used as coagulant.
The parameters that influenced the waste water treatment are: temperature, pH, dose of coagulant and settling time.
It was found that the best condition for zinc removal, within the range of operation used ,were a temperature of 20C a pH value of 13 , a coagulant dose of 15 g Na2S /400ml solution and a settling time of 7 days. Under these conditions the zinc concentrat

... Show More
View Publication Preview PDF
Publication Date
Sat May 01 2021
Journal Name
Journal Of Physics: Conference Series
Violet Laser Irradiation Effect on The Optical Properties of Cobalt oxide (CoO<sub>2</sub>) Thin Films deposited via Semi-Computerized Spraying System
...Show More Authors
Abstract<p>The existing investigation explains the consequence of irradiation of violet laser on the optic properties of (CoO<sub>2</sub>) films. The film was equipped by the utilization of semi-computerized spray pyrolysis technique (SCSPT), it is the first time that this technique is used in the preparation and irradiation using a laser in this technique. From the XRD analysis, the crystalline existence with trigonal crystal system was when the received films were processed by continuous violet laser (405 nm) with power (1W) for different laser irradiation time using different number of times a laser scan (0, 6, 9, 12, 15 and 18 times) with total irradiation time(0,30,45,60,75,90 min</p> ... Show More
View Publication Preview PDF
Scopus Crossref
Publication Date
Tue May 01 2018
Journal Name
Journal Of Physics: Conf. Series
Composition, Characterization and Antibacterial activity of Mn(II), Co(II),Ni(II), Cu(II) Zn(II) and Cd(II) mixed ligand complexes Schiff base derived from Trimethoprim with8- Hydroxy quinoline
...Show More Authors

New Schiff base ligand 2-((4-amino-5-(3, 4, 5-trimethoxybenzyl) pyrimidin- 2-ylimino) (phenyl)methyl)benzoic acid] = [HL] was synthesized using microwave irradiation trimethoprim and 2-benzoyl benzoic acid. Mixed ligand complexes of Mn((ІІ), Co(ІІ), Ni(ІІ), Cu(ІІ), Zn(ІІ) and Cd(ІІ) are reacted in ethanol with Schiff base ligand [HL] and 8-hydroxyquinoline [HQ] then reacted with metal salts in ethanol as a solvent in (1:1:1) ratio. The ligand [HL] is characterized by FTIR, UV-Vis, melting point, elemental microanalysis (C.H.N), 1H-NMR, 13C-NMR, and mass spectra. The mixed ligand complexes are characterized by infrared spectra, electronic spectra, (C.H.N), melting point, atomic absorption, molar conductance and magnetic moment me

... Show More
Publication Date
Sun Oct 01 2017
Journal Name
Journal Of Engineering
Comparison the Physical and Mechanical Properties of Composite Materials (Al /SiC and Al/ B4C) Produced by Powder Technology
...Show More Authors

In this investigation, metal matrix composites (MMCs) were manufactured by using powder technology. Aluminum 6061 is reinforced with two different ceramics particles (SiC and B4C) with different volume fractions as (3, 6, 9 and 12 wt. %). The most important applications of particulate reinforcement of aluminum matrix are: Pistons, Connecting rods etc. The specimens were prepared by using aluminum powder with 150 µm in particle size and SiC, B4C powder with 200 µm in particle size. The chosen powders were mixed by using planetary mixing setup at 250 rpm for 4hr.with zinc stearate as an activator material in steel ball milling. After mixing process the powders were compacted by hydraulic

... Show More
View Publication Preview PDF
Publication Date
Wed Aug 16 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Study the improvement of thermo - mechanical properties for polyester adhesive by using different fibers (glass, kevelar, and carbon).
...Show More Authors

The   mechanical    properties   of   fiber-reinforced-polymer   (FRP)

composites are dependent on the type amount, and orientation of fiber that is selected for a particular service. There are many commercially available reinforcement forms to meet the design requirements of the user. The ability of failure in the fiber architecture allows for optimized performance of a product that saves both weight and cost ( 12).

A modem technology is adopted to produce fibers (glass, kevelar,

and carbon) reinforced composite by using unsaturated polyester, where different volume fraction  of these fibers are used  (0, 0.2, 0.4, 0.6, 0.8,  I)

reinfor

... Show More
View Publication Preview PDF
Publication Date
Wed Jan 01 2020
Journal Name
Medico-legal Update
Flexible ureterorenoscopy versus extracorporeal shock wave lithotripsy for treatment of lower pole renal stones
...Show More Authors

Scopus (1)
Scopus
Publication Date
Sun Apr 08 2018
Journal Name
Al-khwarizmi Engineering Journal
Microstructural Characterization and Mechanical Properties of Similar and Dissimilar Al Alloys Joined using Friction Stir Welding
...Show More Authors

The influence of pre- shot peening and welding parameters on mechanical and metallurgical properties of dissimilar and similar aluminum alloys AA2024-T3 and AA6061-T6 joints using friction stir welding have been studied. In this work, numbers of plates were equipped from sheet alloys in dimensions (150*50*6) mm then some of them were exposed to shot peening process before friction stir welding using steel ball having diameter 1.25 mm for period of 15 minutes. FSW joints were manufactured from plates at three welding speeds (28, 40, 56 mm/min) and welding speed 40mm/min was chosen at a rotating speed of 1400 rpm for welding the dissimilar pre- shot plates. Tow joints were made at rotational speed of 1000 rpm and welding speed of 40m/min f

... Show More
View Publication Preview PDF
Crossref (1)
Crossref