Cadmium sulfide (CdS) nanocrystalline thin films have been prepared by chemical bath deposition (CBD) technique on commercial glass substrates at 70ºC temperature. Cadmium chloride (CdCl2) as a source of cadmium (Cd), thiourea (CS(NH2)2) as a source of sulfur and ammonia solution (NH4OH) were added to maintain the pH value of the solution at 10. The characterization of thin films was carried out through the structural and optical properties by X-ray diffraction (XRD) and UV-VIS spectroscopy. A UV-VIS optical spectroscopy study was carried out to determine the band gap of the nanocrystalline CdS thin film and it showed a blue shift with respect to the bulk value (from 3.9 - 2.4eV). In present work effects of thickness on the structural and optical properties of CdS nanocrystalline thin films were discussed.
This work aimed PVA nanofibers in a range of concentrations were successfully manufactured via electrospinning. PVA NFs/Si was effectively prepared using the electrospinning process. The structural, morphological, optical and electrical properties of the prepared PVA were studied using XRD, FE-SEM, UV-Vis spectrophotometer and I-V characteristics, respectively. The amorphous structure of PVA nanofibers was observed. The optical energy gap from ultraviolet to visible was between (2.75 and 2.41) eV, making this compound highly sensitive to visible orange light at 610 nm, with a photosensitivity of 66%. The optical energy gap of PVA/Si heterojunction was utilized to modify this film from the UV to the visible spectrum. As show in the results,
... Show MoreThe optical properties for the components CuIn(SexTe1-x)2 thin films with both values of selenium content (x) [0.4 and 0.6] are studied. The films have been prepared by the vacuum thermal evaporation method with thickness of (250±5nm) on glass substrates. From the transmittance and absorbance spectra within the range of wavelength (400-900)nm, we determined the forbidden optical energy gap (Egopt) and the constant (B). From the studyingthe relation between absorption coefficient (α) photon energy, we determined the tails width inside the energy gap.
The results showed that the optical transition is direct; we also found that the optical energy gap increases with annealing temperature and selenium content (x). However, the width of l
In this work, spinel ferrites (NiCoFe2O4) were prepared as thin films by dc reactive dual-magnetron co-sputtering technique. Effects of some operation parameters, such as inter-electrode distance, and preparation conditions such as mixing ratio of argon and oxygen in the gas mixture, on the structural and spectroscopic characteristics of the prepared samples were studied. For samples prepared at inter-electrode distance of 5 cm, only one functional group of OH- was observed in the FTIR spectra as all bands belonging to the metal-oxygen vibration were observed. Similarly, the XRD results showed that decreasing the pressure of oxygen in the gas mixture lead to grow more crystal planes in the samples prepare
... Show MoreCarbon nanotubes (CNTs) were synthesized via liquefied petroleum gas (LPG) as precursor using flame fragments deposition (FFD) technique. In vitro, biological activates of carbon nanotubes (CNTs) synthesized by FFD technique were investigated. The physiochemical characterizations of synthesized CNTs are similar to other synthesized CNTs and to the standard sample. Pharmaceutical application of synthesized CNTs was studied via conjugation and adsorption with different types of medicines as promote groups. The conjugation of CNTs was performed by adsorption the drugs such as sulfamethoxazole (SMX) and trimethoprim (TMP) on CNTs depending on physical properties of both bonded parts. The synthesized CNTs almost have the same performance in a
... Show MoreThis work describes, selenium (Se) films were deposited on clean glass substrates by dc planar magnetron sputtering technique.The dependence of sputtering deposition rate of Se film deposited on pressure and DC power has been studied. The optimum argon pressure has range (4x10-1 -8x10-2 )mbar. The optical properties such as absorption coefficient (α) was determined using the absorbance and transmission measurement from UnicoUV-2102 PC spectrophotometer, at normal incidence of light in the wavelength range of 200-850 nm. And also we calculated optical constants(refractive index (n), dielectric constant (εi,r), and Extinction coefficient (κ) for selenium films.
This study describe the effect of temperature on the optical
properties of nickel(ii) phthalocyanine tetrasulfonic acid tetrasodium
salt (NiPcTs) organic thin films which are prepared by spin coating
on indium tin oxide (ITO-glass). The optical absorption spectra of
these thin films are measured. Present studies reveal that the optical
band gap energies of NiPcTs thin films are dependent on the
annealing temperatures. The optical band gap decreases with increase
in annealing temperature, then increased when the temperature rising
to 473K. To enhance the results of Uv-Vis measurements and get
more accurate values of optical energy gaps; the Photoluminescence
spectra of as-deposited and annealed NiPcTs thin fi