Iodine-doped polythiophene thin films are prepared by aerosol assisted plasma jet polymerization at atmospheric pressure and room temperature. The doping of iodine was carried out in situ by employing iodine crystals in thiophene monomer by weight mixing ratios of 1%, 3%, 5% and 7%. The chemical composition analyses of pure and iodine-doped and heat-treated polythiophene thin films are carried out by FTIR spectroscopy studies. The optical band gaps of the films are evaluated from absorption spectrum studies. Direct transition energy gaps are determined from Tauc plots. The structural changes of polythiophene upon doping and the reduction of optical band gap are explained on the basis of the results obtained from FTIR spectroscopy, UV–VIS absorption studies, X-ray diffraction and atomic force microscope (AFM) analysis. The energy band gap will be different according to the concentration of polythiophene iodine. It can be concluded that iodine-doped polythiophene thin films can be prepare by aerosol assisted plasma jet polymerization and control the optical energy band gap regulars by controlling the thiophene -iodine weight mixing ratios.
The work demonstrates the effect of cold atmospheric plasma (CAP) on adult female rats suffering from osteoporosis, the used plasma was generated by a floating electrode-dielectric barrier discharge system with an electrode diameter of 3 cm. The output power was from (12-20) watts. The effect of non-thermal plasma was observed on rats with various exposure times of 20, 30, and 40 sec. It was noted that the blood calcium percentage of animals exposed to cold plasma increased, as well as an increase in the level of vitamin D3 at the same time, it is noted that there is no effect on parathyroid hormone level. For the thyroid gland, it is noticed an increase in the level of T3, and T4 hormones in the blood during the period of induction for
... Show MoreThe paper reports the influence of the thickness on the some optical properties of Fe2O3 thin films,which were prepared by chemical Spray pyrolysis technique on glass substrate heated to 400˚c.The thickness of thin films (250,280,350)nm were measured by using weighting method. The optical properties include the absorbance and reflectance spectra,extinction coefficient,and real and imaginary part of the dielectric constant.The result showed that the optical constant(k,εr,εi)decreased with the increase of the thickness.
Thin films of tin disulphide SnS2 with different thicknesses (2500,4000,5000)A0 have been prepared by chemical spray pyrolises technique on substrate of glass with temperature (603)K . The effect of thickness on the optical properties of SnS2 has been studied.the optical study that includes the absorptance and transmittance spectra in the wavelength range (300900)nm demonstrated that the value of absorption coefficient (α) ) was greater than (104 cm-1) the electronic transitions at the fundamental absorption edge were of the indirect kind whether allowed and forbidden . Absorption edge shift slightly towards higher wave length.The value of energy gaps (Eg) for all the films prepared are decreased with inc
... Show MoreA thin CdS Films have been evaporated by thermal evaporation technique with different thicknesses (500, 1000, 1500 and 2000Å) and different duration times of annealing (60, 120 180 minutes) under 573 K annealing temperature, the vacuum was about 8 × 10-5 mbar and substrate temperature was 423 K. The structural properties of the films have been studied by X- ray diffraction technique (XRD). The crystal growth became stronger and more oriented as the film thickness (T) and duration time of annealing ( Ta) increases.
In this study, the surface of the epoxy/Al composite is treated using a dielectric barrier discharge (DBD) plasma in the presence of air. The epoxy composite was prepared by mixing 0.1g and 0.3 g aluminum powder with epoxy resin and its hardener in a ratio of 3:1. The surface epoxy/Al composite as a dielectric barrier layer (DB) is studied at an applied frequency of 8 kHz and at three exposure times 0, 2, and 4 min. The UV degradation process has been studied using UV-Visible spectroscopy, for these polymers. The absorbance intensity in the UV region (200–320 nm) was high. The absorbance level decreased after 2 minutes and increased after 4 min exposure time. Before exposure to plasma, the epoxy/Al composite at 0.1 g Al ha
... Show MoreIn this work, thin films of undoped and Al-doped CdO with (0.5, 1 and 2) wt.% were prepared by using thermal vacuum evaporation on glass substrate at room temperature. The optical absorption coefficient (α) of the films was determined from transmittance spectra in the range of wavelength (400-1100) nm. The spectral transmission and the optical energy band gap decrease from 75% and 2.24 eV to 20% and 2.1 eV respectively depending upon the Al content in the films, also our studies include the calculation of the optical constants (refractive index, extinction coefficient, real and imaginary part of dielectric constant) as a function of photon energy. It is evaluated that the optical band gap of
... Show MoreIn this research, a type of gram negative bacteria was exposed to non-thermal plasma at a distance of (2 and 3 cm) from the plasma flow nozzle, with the use of an alternating power supply (5KHz), where exposure was made at two different voltages (4.9 and 8 kV). A negative gram of Pseudomonas aeruginosa bacteria was isolated and exposed to non-thermal plasma at different flow rates of argon gas whose value ranged from (1-5) liters/minute. The results showed that bacterial killing rate is directly proportional to distance while exposing the samples to non-thermal plasma, and the best factors by which a complete killing rate was obtained were at a distance of 2 cm with a voltage of 8 kV and a gas flow rate of 5 liters/min,
... Show MoreCadmium Oxide films have been prepared by vacuum evaporation technique on a glass substrate at room temperature. Structural and optical properties of the films are studied at different annealing temperatures (375 and 475) ËšC, for the thickness (450) nm at one hour. The crystal structure of the samples was studied by X- ray diffraction. The highest value of the absorbance is equal to (78%) in the wavelength (530) nm, at annealing temperature (375) ËšC. The value of at a rate of deposition is (10) nm/s. The value of optical energy gap found is equal to (2.22) eV.
In this research, the study effect of irradiation on structural and optical properties of thin film (CdO) by spray pyrolysis method, which deposited on glasses substrates at a thickness of (350±20)nm , The flow rate of solution was 5 ml/min and the substrate temperature was held constant at 400˚C.The investigation of (XRD) indicates that the (CdO) films are polycrystalline and type of cubic. The results of the measuring of each sample from grain size, micro strain, dislocation density and number of crystals the grain size decreasing after irradiation with gamma ray from(27.41, 26.29 ,23.63)nm . The absorbance and transmittance spectra have been recorded in the wavelength range (300-1100) nm in order to study the optical properties.
... Show MoreSome of structural ,and electrical properties of pure and zinc (Zn) doped cadmium telluride thin films with impurity percentages (0.5, 1, 1.5)%, deposited on hot glass substrate (temperature equals to 423K) of thickness of 300nm and rate deposition of 0.5 nm.s-1 by thermal co-evaporation technique under vacuum of (2×10-5)Torr have been investigates. The structural properties for the prepared films were studied before and after. doping process by analysis of the X-ray diffraction, and it appeared that pure and dopant CdTe thin films are polycrystalline and have the cubic structure with preferential orientation in the [111] direction, and the crystal structure of the films were improved due to doping process. From d.c
... Show More