In this work copper nanopowder was created at different liquid
medias like DDDW, ethylene glycol and Polyvinylpyrrolidone
(PVP). Copper nanopowder prepared using explosion wire process
and investigated the effects of the exploding energy, wire diameter,
the type of liquid on the particle size, and the particles size
distribution. The nanoparticles are characterized by x-ray diffraction,
UV-visible absorption spectroscopy and transmission electron
microscopy (TEM). The x-ray diffraction results reveal that the
nanoparticles continue to routine lattice periodicity at reduced
particle size. The UV-Visible absorption spectrum of liquid solution
for copper nanoparticles shows sharp and single surface Plasmon
resonance (SPR) peak centered at a wavelength of 590 nm in
ethylene glycol media, but don’t have peak in PVP fluid. This peak
indicated the production of pure and spherical copper nanoparticle.
Protection study of the corrosion behavior of Copper surface was conducted with several concentrations of drug. Experimentally, voltammetric measurements were used to check the inhibition efficiency (% IE) in saline solution of 3.5% NaCl. The results showed an increase in the inhibition efficiency with increasing the concentration of the drug was 95.90%. Theoretical treatment of the drug in the gas phase was performed using the (hyperchem-8.07) program for molecular mechanics and semi-empirical computations. The (PM3) approach was used to determine the heat of formation (1H˚f), binding energy (1Eb), and total energy (ET
الصيغة العامة للمعقدات الجديدة [M2(BDS)Cl4] الناتجة من تفاعل الليكاند الجديد] ن1,ن4-ثنائي(1أ –بنزو]د[ اميدازول-2-يل)-ن1,ن4-ثنائي(4-ثنائي مثيل امينو) بنزيل) سكسنمايد[ (BDS) مع الايونات الفلزية الكادميوم, الكوبلت, الزئبق, النحاس والنيكل. تم اشتقاق هذا الليكاند من تفاعل المواد الثلاث 4-(ثنائي ميثيل أمينو) بنزالدهيد، 2-أمينو بنزيميدازول، وكلوريد السكسينيل. تم تشخيص المركبات باستخدام مطيافية طيف الاشعة تحت الحمراء وطيف الرن
... Show MoreGold nanoparticles AuNPs have proven to be powerful tools in various nanomedicine applications, because of their photo-optical distinctiveness and biocompatibility. Noble metal gold nanoparticles was prepared by pulsed laser ablation method (1064-Nd: YAG with various Laser power from 200 to 800 mJ and 1 Hz frequency) in distil water. The process was characterized using UV-VIS absorption spectroscopy. Morphology and average size of nanoparticles were estimated using AFM and X-ray diffraction (XRD) analysis which show the nature of gold nanoparticles (AuNPs). Antibacterial activity of gold nanoparticles as a function of particles concentration against gram negative bacterium Escherichia coli and gram positive bacterial Staphylococcus aureu
... Show MoreAcinetobacter baumannii is highly adapted to hospital environments, causing persistent chronic infections due to its ability to form biofilms. In this work, the antibiofilm activity of AuNPs with a subMIC concentration of 9.34 μg/ml was investigated by the microtiter plate method against 80 clinical isolates of A. baumannii. The results revealed that the biofilm was significantly (P< 0.05) reduced by 48.2 – 82.1%.
Ni-Co-Mn-Mg ferrite nanoparticles with the formula (Ni,Co)xMn0.25-xMg0.75Fe2O4 were synthesized in this work by employing the sol-gel auto-combustion process, with nitrates used as the cations source and citric acid (C6H8O7) as the combustion agent. X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray (EDX), and a vibrating sample magnetometer (VSM) were used to characterize the structural, morphological, and magnetic properties of ferrite powders. The XRD measurements showed crystallite sizes ranging between 24 - 28 nm. The FE-SEM images show the presence of agglomeration as well as a non-homogeneous distribution of the samples. On the other hand, the stoichiometry of the react
... Show MoreMicrobial antibiotics resistance is considered a serious health issue in the Middle East and developing countries. In this study, the Fe2O3 nanoparticles was prepared chemically, and the particles size and shape were analyzed by using Scan electron microscope (SEM) and X-Ray diffraction (XRD). Different concentration of Fe2O3 nanoparticles were used and examined on E.coli and S. aureus. Using liquid dilution and in vitro cytotoxicity assay by microplate toxicity test (MTT). The microbial cell metabolic activity was measured on gram-negative, gram-positive bacteria and fungi after treating with different concentrations of Fe2O3 nanoparticl
... Show MoreNanoparticles have gained considerable interest in recent times for oil recovery purposes owing to significant capabilities in wettability alteration of reservoir rocks. Wettability is a key factor controlling displacement efficiency and ultimate recovery of oil. The present study investigates the influence of zirconium (IV) oxide (ZrO2) and nickel (II) oxide (NiO) nanoparticles on the wetting preference of fractured (oil-wet) limestone formations. Wettability was assessed through SEM, AFM and contact angle. The potentials of the nanoparticles to alter oil-wet calcite substrates water wet, was experimentally tested at low nanoparticle concentrations (0.004–0.05 wt%). Quite similar behaviour was observed for both nanoparticles at the same
... Show More