Polyaniline polymer has been prepared by chemical oxidation
polymerization method in laboratory successfully. The PANI and
(PVA+PVP) as a polymer blends in different percentage (30%, 50%,
70%) from Polyaniline was prepared. The sample was studies as
optical properties by UV-vis spectrophotometer at (400-700) nm.
The result of optical energy gap was 2.23 eV for pure (PVA+ PVP)
and with additive was increasing with increasing PANI concentration
to become (2.49 for 30% to 2.52 for 70%) PANI. The goal of this
project is prepare triple blend polymer and study the effect when add
conductive polymer (Polyaniline) on the optical properties and
calculate optical constant as energy gap, refractive index, dielectric
constant and dielectric losses for (PVA+PVP) blends.
The work in this paper focuses on the system quality of direct and coherent communication system for two computers. A system quality is represented by Signal to Noise ratio (SNR) and Bit Error Rate (BER). First part of the work includes implementation of direct optical fiber communication system and measure the system quality .The second part of the work include implementation both the( homodyne and heterodyne)coherent optical fiber communication system and measure the system quality . Laser diode 1310 nm wavelength with its drive circuit used in the transmitter circuit . A single mode of 62.11 km optical fiber is selected as transmission medium . A PIN photo detector is used in the receiver circuit. The optical D-coupler was u
... Show MoreSb-dopedAgInSe2 (AIS: 3%Sb)thin films were synthesized by thermal evaporation with a vacuum of 7*10-6torr on glass with (400+20) nm thickness. X-ray diffraction was used to show that Sb atoms were successfully incorporated into the AgInSe2 lattice. Then the thin films are annealed in air at 573 K. XRD shows that thin films AIS pure, AIS: 3%Sb and annealing at 573 K are polycrystalline with tetragonal structure with preferential orientation (112).raise the crystallinity degree. The Absorption spectra revealed that the average Absorption was more than 60% at the wavelength range of 400–700 nm. UV/Visible measure shows the lowering in energy gap to 1.4 eV forAIS: 3%Sb at 573 Kt his energy gap making these samples suitable for p
... Show MoreOptical fiber biomedical sensor based on surface plasmon resonance for measuring and sensing the concentration and the refractive index of sugar in blood serum is designed and implemented during this work. Performance properties such as signal to noise ratio (SNR), sensitivity, resolution and the figure of merit were evaluated for the fabricated sensor. It was found that the sensitivity of the optical fiber-based SPR sensor with 40 nm thick and 10 mm long Au metal film of the exposed sensing region is 7.5µm/RIU, SNR is 0.697, figure of merit is 87.2 and resolution is 0.00026. The sort of optical fiber utilized in this work is plastic optical fiber with a core diameter of 980 µm, a cladding of 20μm, and a numerical aperture of 0.
... Show MoreIn this work, a simple and new method is proposed to simultaneously improve the physical layer security and the transmission performance of the optical orthogonal frequency division multiplexing system, by combining orthogonal frequency division multiplexing technique with chaotic theory principles. In the system, a 2-D chaotic map is employed. The introduced system replaces complex operations such as matrix multiplication with simple operations such as multiplexing and inverting. The system performance in terms of bit error rate (BER) and peak to average ratio (PAPR) is enhanced. The system is simulated using Optisystem15 with a MATLAB2016 and for different constellations. The simulation results showed that the BE
... Show MoreThe electrical insulation of the manufacture sulfonated phenol-formaldehyde viscous material (product) has been studied with Polyvinyl-acetate (PVA) and toluene diisocyanate (TDI) blend has been prepared by fixing percentage by weight 3:1 and mixed with different percentages by weight of the product sulfonated phenol formaldehyde viscous mass (SPF). The Fourier transform infrared (FTIR) spectroscopy is done on (SPF) resin powder and prepared film of PVA-TDI-SPF viscous mass. The quality factor (Q), dissipation factor (D), parallel resistance (Rp), series resistance (Rs), parallel capacitance (Cp), series capacitance (Cs) and phase shift (?) are measured. The calculated maximum dielectric constant (??) is 3.49x107 at sample (1) wt.1% SPF vis
... Show MoreIn this research, a sensor for chemical solutions was designed and formed using optical fiber-based on a surface Plasmon resonance technology. A single-mode optical fiber with three different diameters (25, 45 and 65) µm was used, respectively. The second layer of the low refractive fiber was replaced by gold, which was electrically deposited at 40 µm thickness. For each of the three types of optical fiber, different saline concentrations (different index of refraction) were used to evaluate the performance of the refractive index sensor (chemical sensor) by measuring its sensitivity and resolutions. The highest values we could get for these two parameters were 240mm/RIU, and 6*10-5 RIU respectively, when the diameter of a
... Show MoreThis research investigates the dielectric properties (impedance, dielectric constant
and dielectric loss) of SiO2\ Ep :TiO2 \ Ep nanocomposite over the frequency range
of (102-106 Hz ) at room temperature. The dielectric material used is epoxy resin,
while nano-sized titanium dioxide (TiO2) with grain size ( 30nm) , oxide silicon
(SiO2) with grain size (12nm) in state volume ratio (0,0.05 ,0.1) .The effect of
gamma by using (CS137) for period time (17) day was studied Radiation caused
decreasing in real and imaginary parts of dielectric constant and impedance .
In this paper, a step-index fiber with core index 1.445 5 1 7 and cladding index 1.443 1 5 7 has been designed and studied. Multimode operation is achieved by using a fiber with core radius 25 μm operating at a wavelength of 1.3 μm. The mode parameters (effective refractive index, phase constant, fractional modal power in the core and cutoff wavelength) were calculated using RP fiber calculator (PRO version 2020). The shapes of the intensity and amplitude distribution of linearly polarized guided modes were shown.
In this work, the linear properties of Vitamin D3-5000IU soft gel were investigated by measuring its absorption and fluorescence spectra. It was observed that there was a shift towards longer wavelength within limits (75 nm), with quantitative efficiency equal to (33.58%). The values of absorbance were used to calculate the extinction coefficient, optical refractive index, optical conductivity and optical dielectric constant values.
The non-linear properties of Vitamin D3-5000IU soft gel was also studied using the Z-Scan technique by using Neodymium-doped Yttrium Garnet (Nd: YAG) continuous laser (CW) emitting in &n
... Show MoreIn this paper it was designed a new fractal optical modulation by using a new iteration of fractal function, the result was analyzed by MTF evaluation, and it compared with results of normal optical modulation.
The normal and fractal optical modulator is a circular disc which has a radius R=9cm, both of them consist of twenty sectors, ten sectors are opaque and the other ten sectors are transmitted for the light.
The fractal optical modulator contains two patterns, the pattern two can be used to detect the target, and pattern one can be used to lock the target
The best similarity of MTF behavior for normal and fractal Reticle was evaluating the power transparent depends on the size o
... Show More