CdS and CdS:Sn thin films were successfully deposited on glass
substrates by spray pyrolysis method. The films were grown at
substrate temperatures 300 C°. The effects of Sn concentration on the
structural and optical properties were studied.
The XRD profiles showed that the films are polycrystalline with
hexagonal structure grown preferentially along the (002) axis. The
optical studies exhibit direct allowed transition. Energy band gap
vary from 3.2 to 2.7 eV.
In the present work, the focusing was on the study of the x-ray diffraction, dielectric constant, loses dielectric coefficient, tangent angle, alter- natively conductivity and morphology of PET/BaTio3. The PET/BaTio3 composite was prepared for polyethylene terephthalate PET polymer composite containing 0, 10, 20, 30, 40, 50, and 60 wt. % from Barium titanate BaTi03 powder. The composite of two materials leads to form mixing solution and hot-pressing method. The effect of BaTio3 on the structure and dielectric properties with morphology was studied on PET matrix polymer using XRD, LCR meter and SEM.
In this work ,glass-metal apparatus was designed and manufactured which used for preparing ahigh purity uranium. The reaction is simply take place between iodine vapour and uranium metal at 500C in closed system to form uranium tetra iodide which is decomposed on hot wire at high temperature around 1100C. Also another apparatus was made from Glass and used for preparing ahigh purity of UI4 more than 99.9% purity.
Carbon nanospheres (CNSs) were successfully prepared and synthesized by Catalytic Chemical Vapor Deposition (CCVD) by using camphor as carbon source only, over iron Cobalt (Fe-Co) saturated zeolite at temperature between (700 oC and 900 °C), with different concentrations of camphor, and reaction time. The synthesized CNSs were characterized using Scanning Electron Microscopy (SEM), X-ray diffraction spectroscopy (XRD), and Fourier Transform Infrared (FTIR). The carbon spheres in different sizes between 100 nm and 1000 nm were investigated. This work has done by two parts, first preparation of the metallic catalyst and second part formation CNSs by heat treatment.
The effect of adding different volume of coumarin dye (5, 15, 25 and 35) ml on optical properties of Poly (Methyl Meth Acrylate) was studied. Films of pure PMMA and PMMA with different volume of coumarin dye (5, 15, 25 and 35) ml were prepared using the casting technique. Transmission and absorption of the films were measured by using UV-VIS spectrometer technique type (100 Conc), in order to assess the type of transmission which was found an indirect transition. An optical energy gap of pure PMMA is (4.95e v) and after adding coumarin with volume (25, 35) ml, the energy gap for PMMA decrease by (0.05) compere to pure PMMA films and addition energy gap appear equal to (4.1 e v). It was found that the absorption coefficient, extinction coeff
... Show MoreIn the present study, a powder mixture of elements Ti and Ni was mechanically alloyed in a high energy ball mill. Microstructure of the nanosized amorphous milled product in different stages of milling has been characterized by X- ray diffraction, scanning electron microscopy and differential thermal analysis. We found that time of mechanical alloying is more significant to convert all crystalline structure to the amorphous phase. Nanocrystalline phase was achieved as a result of the mechanical alloying process. The results also indicates that the phase transformation and the grain size occurs in these alloys are controlled by ball milling time
This work aimed PVA nanofibers in a range of concentrations were successfully manufactured via electrospinning. PVA NFs/Si was effectively prepared using the electrospinning process. The structural, morphological, optical and electrical properties of the prepared PVA were studied using XRD, FE-SEM, UV-Vis spectrophotometer and I-V characteristics, respectively. The amorphous structure of PVA nanofibers was observed. The optical energy gap from ultraviolet to visible was between (2.75 and 2.41) eV, making this compound highly sensitive to visible orange light at 610 nm, with a photosensitivity of 66%. The optical energy gap of PVA/Si heterojunction was utilized to modify this film from the UV to the visible spectrum. As show in the results,
... Show MorePyrolysis of virgin polyethylene plastics was studied in order to produce hydrocarbon liquid fuel. The pyrolysis process carried out for low and high-density polyethylene plastics in open system batch reactor in temperature range of 370 to 450°C.
Thermo-gravimetric analysis of the virgin plastics showed that the degradation ranges were between 326 and 495 °C. The results showed that the optimum temperature range of pyrolysis of polyethylene plastics that gives highest liquid yield (with specific gravity between 0.7844 and 0.7865) was 390 to 410 °C with reaction time of about 35 minutes. Fourier Transform Infrared spectroscopy gave a quite evidence that the produced hydrocarbon liquid fuel consisted ma
... Show More