PbxCd1-xSe compound with different Pb percentage (i.e. X=0,
0.025, 0.050, 0.075, and 0.1) were prepared successfully. Thin films
were deposited by thermal evaporation on glass substrates at film
thickness (126) nm. The optical measurements indicated that
PbxCd1-xSe films have direct optical energy gap. The value of the
energy gap decreases with the increase of Pb content from 1.78 eV to
1.49 eV.
Background: Lack of durability of the bond of the dental adhesive systems to tooth structure is one of the most important problems in tooth colored restorative work. This in vitro study was performed to evaluate the effect of 2% chlorhexidine gluconate(CHX) on dentin bond strength by using total etch adhesive system at twenty-four hours and three months of water storage. Material and methods:A flat dentin surface was prepared for forty sound human maxillary premolar teeth which were acid etched with 36% phosphoric acid gel after being divided randomly into four groups of ten teeth each according to storage time and CHX application, theCHX was applied for 60 seconds before adhesive application for groups I and III which were tested after twe
... Show MoreIn order to evaluate the effect of seed size, plant growth regulators and some chemical materials on seed vigour and seedling growth of rice (Oryza sativa L.) an experiment was conducted in 2015 at Laboratories of Agriculture and Marshes College, University of Thi-Qar. Factorial experiment in CRD was used with four replications in two factors. The first factor included three seed sizes (4.6-5.1, 5.2-5.7 and 5.8-6.3 mm). The second factor was seeds soaking treatments (KNO3 6 gl-1, CaCl2 20 gl-1, salicylic acid 20 mg l-1, cytokinin 40 mg l-1, gibberllic acid 400 mg l-1, ascorbic acid 40 mg l-1 and seeds soaked in distilled water). The results showed that the largest seed size influenced significantly and gave the higher averages of germinatio
... Show MoreBackground: Healing of a tooth extraction socket is a complex process involving tissue repair and regeneration. It involves chemotaxis of appropriate cells into the wound, Transformation of undifferentiated mesenchymal cells to osteoprogenitor cells, proliferation and differentiation of committed bone forming cells, extracellular matrix synthesis, mineralization of osteoid, maturation and remodeling of bone. These cellular events are precisely controlled and regulated by specific signaling molecules. Some of these like transforming growth factor beta (TGF-?), vascular endothelial growth factor (VEGF), bone morphogenetic proteins (BMP) and insulin like growth factors (IGF) are well conserved proteins involved in the initial response to injur
... Show MoreObjectives: To evaluate the effect of non-pharmacological pain relief methods on duration of labor stage.
Methodology: A quasi-experimental study design was conducted during the period of (4th July 2018 through 24th October 2018) on non-probability of (60) women (30) of them were a control group and (30) were the study group whom admitted to Al-Elwyia Maternity Teaching Hospital suffering from labor pain. A questionnaire was used as a tool of data collection Descriptive& Inferential statistical analyses were used to analyze the data.
Result: The highest percentages of study and control groups were in age group (< 20) years old, primary schools graduates, housewife, from "urban area", within low category of socioeconomic scal
RG Majeed, AS Ahmed, Jornal of Al-Muthanna for Agricultural Sciences, 2023
The effect of short range correlations on the inelastic longitudinal Coulomb form
factors for the lowest four excited 2+ states in 18O is analyzed. This effect (which
depends on the correlation parameter β) is inserted into the ground state charge
density distribution through the Jastrow type correlation function. The single particle
harmonic oscillator wave function is used with an oscillator size parameter b. The
parameters β and b are, considered as free parameters, adjusted for each excited state
separately so as to reproduce the experimental root mean square charge radius of
18O. The model space of 18O does not contribute to the transition charge density. As
a result, the inelastic Coulomb form factor of 18