PVA, Starch/PVA, and Starch/PVA/sugar samples of different
concentrations (10, 20, 30 and 40 % wt/wt) were prepared by casting
method. DSC analysis was carried; the results showed only one glass
transition temperature (Tg) for the samples involved, which suggest
that starch/PVA and starch/PVA/sugar blends are miscible. The
miscibility is attributed to the hydrogen bonds between PVA and
starch. This is in a good agreement with (FTIR) results. Tg and Tm
decrease with starch and sugar content compared with that for
(PVA). Systematic decrease in ultimate strength, due to starch and
sugar ratio increase, is attributed to (PVA), which has more hydroxyl
groups that made its ultimate strength higher than that for
starch/PVA, and starch/PVA/sugar blends. It is observed from water
uptake tests that the solubility time decreases with starch ratio; it is
attributed to decrease in hydroxyl groups caused by PVA ratio
decrease. The inter- and inter-molecular bonds of the hydroxyl
groups enhanced the solubility process of the starch/PVA blends in
water. The water immersion causes hydrogen bonds (inter and
intermolecular bonds) to decompose, that increases the film
solubility. Water absorption and capacity of degradability are most
important in biodegradable materials. The results suggest the samples
that have undergone investigation, can be used for shopping, and
food packaging.
The study of soil burial for the sample at (3cm) depth, and at (13cm)
depth has exhibited weight loss increase with soil burial time. The
biodegradability rapidly increases at the first (6-7) weeks; it is found
that the weight loss at (3cm) depth is greater than that at (13cm) that
was attributed to the differences in the availability of oxygen ratio. It
is found that PVA undergoes lowest weight loss, the weight loss
changes with starch, and sugar content. In dry soil, the weight loss is
lower. The results proved that the biodegradation decreases with soil
burial time after seven weeks of burial. It is concluded that the
samples involved are biodegradable material that can be used for
packaging applications and biologically friendly synthetic polymer
blends to solve the solid waste accumulation problem.
The present study aimed to identify the therapeutic evaluation of chitosan extracted from the fungus cushroom and pure chitosan on glucose and lipid profile in the blood of 35 male rabbits with hyperlipidemia induced experimentally by cholesterol. The tests included estimation of glucose levels, total cholesterol, triglycerides, high-density lipoproteins, low-density lipoproteins, and very low-density lipoproteins. hyperlipidemia was induced in the male rabbits used in the study which was administered orally with cholesterol 150mg/kg body weight for a week. rabbits were divided into seven groups: control, cholesterol, pure chitosan, mushroom chitosan, cholesterol and pure chitosan, cholesterol and mushroom chitosan and cholestero
... Show MoreThe effect of different doping ratio (0.3, 0.5, and 0.7) with thickness in the range 300nmand annealed at different temp.(Ta=RT, 473, 573, 673) K on the electrical conductivity and hall effect measurements of AgInTe2thin film have and been investigated AgAlxIn(1-x) Te2 (AAIT) at RT, using thermal evaporation technique all the films were prepared on glass substrates from the alloy of the compound. Electrical conductivity (σ), the activation energies (Ea1, Ea2), Hall mobility and the carrier concentration are investigated as a function of doping. All films consist of two types of transport mechanisms for free carriers. The activation energy (Ea) decreased whereas electrical conductivity increases with increased doping. Results of Hall Effect
... Show MoreObjective(s): Biocompatibility, non-toxicity, minimal allergenicity, and biodegradability are all characteristics of chitosan. Other biological properties of chitosan have been reported, including antitumor, antimicrobial and antioxidant activities. This research aim is the synthesis of drug compounds by preparation and characterization of polymer chitosan Schiff base and chitosan Schiff base / Poly vinyl alcohol / poly vinyl pyrrolidone Nanocomposite and study applications (anticancer cell line, antimicrobial agents). Methods: Chitosan Schiff base was prepared from the reaction of chitosan with carbonyl group of 4-nitro benzaldehyde. Polymer blend have been prepared by solution casting method. Chitosan Schiff base mixing with PVA and PVP
... Show MoreThe place in which the person lives and his geographical and social environment have a great impact on building his personality, belief and culture, Islam has alerted the importance of the Muslim to make sure to choose the appropriate place in which he resides and dwells in that it is compatible with his religion and belief in order to ensure communication with Islamic knowledge in a way that enhances his belief Arabization occurs when a person makes himself an Arab by living the life of the Bedouins, and creates the morals of the Bedouins from the inhabitants of the Badia with its harshness, cruelty, ignorance and lack of understanding in religion and far from the sources of knowledge of Islamic knowledge. Blasphemy and polytheism, and
... Show MoreThe evaluation of banks plays an important role in maintaining the interests of customers with the bank as well as providing continuous supervision and control by the Central Bank. The Central Bank of Iraq conducted an assessment of the Iraqi banks through the implementation of the CAMEL model during a certain period. This evaluation did not continue. The research provides continuity to the Central Bank's assessment and as a step to continue the evaluation process for all banks through the use of the CAMEL model. ROA and ROE by using the regression model for four Iraqi banks registered in the Iraqi market for securities during the period 2010-2016. The results showed that the capital and profitability indicators have a significan
... Show MoreThe paper include studies the effect of solvent of dye doped in polymeric laser sample which manufactured in primo press way, which is used as an active (R6G) tunable dye lasers. The remarks show that, when the viscosity of the solvent (from Pure Water to Ethanol), for the same concentration and thickness of the performance polymeric sample is increased, the absorption spectrum is shifts towards the long wave length (red shift), & towards short wave length (blue shift) for fluorescence spectrum, also increased the quantum fluorescence yield. The best result we obtained for the quantum fluorescence yield is (0.882) with thickness (0.25mm) in Ethanol solvent in concentration (2*10-3mole/liter), while when we used the Pure Water as a solvent,
... Show MoreMany extracted material were used as mouthwash to settle different kinds of oral fungi and bacteria. In this study an extractive of Cyperus rotundus plant E.C.R. which is very active as a mouthwash, was used in concentration range (10-25) ppm in artificial saliva at pH=6.4 and temperature range (288-318) K, to study it’s inhibitory effect on the corrosion of dental amalgam. Potentiostatic and cyclic polarization were used to follow this study. The presence of E.C.R. lead to shift the corrosion potential to the active direction and decreased the corrosion rate to about 98.87%, the inhibition action of E.C.R. resulting from the adsorption of C.R.E. layer between amalgam and saliva as FTIR spectrums shows, where the variety of FTIR adsorptio
... Show MoreThe paper include study the effect thickness of the polymeric sample which is manufactured by thermo press way. The sample was used as an active tunable R6G laser media. The remarks show that, when the thickness of the samples is increased, with the same concentration, the spectrum will shift towards the short wavelength, & the quantum fluorescence yield will increased. The best result we obtained for the quantum fluorescence yield is (0.68) at the sample, with thickness (0.304mm) in Ethanol solvent, while when we used the Pure Water as a solvent, we found that the best quantum fluorescence yield is (0.63) at (0.18mm) thickness of the sample.
The performance and lifetime of the flexible asphalt pavement are mainly dependent on the interfacial bond strength between layer courses. To enhance the bond between layers, adhesive materials, such as tack coats, are used. The tack coat itself is a bituminous material, which is applied on an existing relatively non-absorbent surface to ensure a strong bond between the old and newly paved layer. The primary objective of this study was to evaluate the effects of various types of tack coat materials on interlayer bond strength and to determine the optimal application rate for each type. The tack coat types used in this paper were RC-70, RC-250, and CSS-1h. Both laboratory-prepared and field-constructed hot mix asphalt concrete pavements usin
... Show More