Porous silicon (PS) layers were formed on n-type silicon (Si) wafers using Photo- electrochemical Etching technique (PEC) was used to produce porous silicon for n-type with orientation of (111). The effects of current density were investigated at: (10, 20, 30, 40, and50) mA/cm2 with etching time: 10min. X-ray diffraction studies showed distinct variations between the fresh silicon surface and the synthesized porous silicon. The maximum crystal size of Porous Silicon is (33.9nm) and minimum is (2.6nm) The Atomic force microscopy (AFM) analysis and Field Emission Scanning Electron Microscope (FESEM) were used to study the morphology of porous silicon layer. AFM results showed that root mean square (RMS) of roughness and the grain size of porous silicon decreased as etching current density increased and FESEM showed that a homogeneous pattern and confirms the formation of uniform porous silicon. The chemical bonding and structure were investigated by using Fourier transformation infrared spectroscopy (FTIR). The band gap of the samples obtained from photoluminescence (PL). These results showed that the band gap of porous silicon increase with increasing porosity.
In this work, magnesium aluminate spinel (MA) (MgO 28 wt%, Al2O3 72 wt%) stoichiometric compound , were synthesized via solid state reaction (SSR) Single firing stage, and the impact of sintering on the physical properties and thermal properties as well as the fine structure and morphology of the ceramic product were examined. The Spinel samples were pressed at of (14 MPa) and sintering soaking time (2h). The effect of adding oxide titania (TiO2) was studied. The obtained powders were calcined at a temperature range of 1200 and 1400 °C. The calcined samples spinel were characterized by XRD, it showed the presence of developed spinel phase end also showed that the best catalyst is titania. The SEM image showed the high sintering temperat
... Show MoreMost of the mosques in the Islamic world fall under specific and known forms and patterns to a large extent, and such patterns have grown and evolved from the few basic and uniform models, but they changed slowly due to the impact with a mixture of changing functional requirements and cultural landscapes because of the variables of time and place to form patterns known and famous in this day across parts of the Islamic world and its borders. There was no exception to these patterns, but small numbers of mosques that were probably the result of personal experiences or improvisational resolutions, or in response to specific or temporary stimuli. However, the emergence of a specific pattern which does not belong to any of these patt
... Show MoreIn this work, production of silicon metal at high purity of 99% by using Iraqi–starting materials (Iraqi sand and plant coal)was reported, electric arc–furnaces assembly was manufactured inside, the graphite electrodes were made from graphite scrap, this system is operate to produce about 800 gm /6hr of silicon metal to meet the need for manufacturing silicon oils, resins, solar cells, and electronic parts. The procedure, equipments and analysis data were described as well.
This research analyzes the level of the short circuit effect of the Iraqi super network and decides the suitable location for the High Voltage Direct Current (HVDC) connections in order to obtain the best short circuit reduction of the total currents of the buses in the network. The proposed method depends on choosing the transmission lines for Alternating current (AC) system that suffers from high Short Circuit Levels (SCLs) in order to reduce its impact on the transmission system and on the lines adjacent to it and this after replacing the alternating current (AC) line by direct current (DC) line. In this paper, Power System Simulator for Engineering (PSS/E) is used to model two types of HVDC lines in an effective regi
... Show MoreThis study investigated the shear performance of concrete beams with GFRP stirrups vs. traditional steel stirrups. Longitudinal glass fiber‐reinforced polymer (GFRP) bars were used to doubly reinforce the tested beams at both the top and bottom of their cross sections. To accomplish this, several stirrup spacings were provided. Eight beam specimens, measuring 300 × 250 × 2400 mm, were used in an experimental program to test under a two‐point concentrated load with an equal span‐to‐depth ratio until failure. Four beams in Group I have standard mild steel stirrups of 8 mm diameter, while four beams in Group II have GFRP stirrups with the same adopted diameter. The difference betwe
This study investigated the shear performance of concrete beams with GFRP stirrups vs. traditional steel stirrups. Longitudinal glass fiber‐reinforced polymer (GFRP) bars were used to doubly reinforce the tested beams at both the top and bottom of their cross sections. To accomplish this, several stirrup spacings were provided. Eight beam specimens, measuring 300 × 250 × 2400 mm, were used in an experimental program to test under a two‐point concentrated load with an equal span‐to‐depth ratio until failure. Four beams in Group I have standard mild steel stirrups of 8 mm diameter, while four beams in Group II have GFRP stirrups with the same adopted diameter. The difference betwe
the current study Included, evaluation the impact of Nitrofurantoin drug on liver in albino mice, 128 male albino mice have been used . Animals treared with (150,200 Mg/Kg) for 8 weeks . NFI caused histological changes in liver represented by , swelling of hepatocytes, disappearance of radial arrangement , vaculation of liver cells , increasing of kupffer cells and appearance of giant cells. NFT caused Congestion of blood vessels and infiltration of inflammatory cells in liver in all used concentrations.
In this work, the optical properties of Cu2S with different thickness
(1400, 2400, 4400) Ǻ have been prepared by chemical spray pyrolys
is method onto clean glass substrate heated at 283 oC ±2. The effect
of thickness on the optical properties of Cu2S has been studied. It
was found that the optical properties of the electronic transitions on
fundamental absorption edge were direct allowed and the value of the
optical energy gap of Cu2S (Eg) for direct transition decreased from
(2.4-2.1) eV with increasing of the thickness from (1400 - 4400)Ǻ
respectively. Also it was found that the absorption coefficient is
increased with increasing of thicknesses. The optical constants such<