The corrosion behavior of mild sleet in saturated aerated and de-aerated Ca(OH)2 solution was investigated using electrochemical measurements. The work was carried out with small coupons immersed in solutions containing different quantities of NaCl in presence of various NaN02 concentrations as corrosion inhibitors. It has been found thal:(1 ) In presence of NaCl, the time required to reach O2 evolution potential in de-aerated Ca(OH)2 polarized at 10μA/cm 2 is function of inhibitor concentration and it becomes lass as NaN02 increases compared with zero presence indicating the effectiveness of NaN02 as anodic corrosion inhibitor. (2) In absence of NaCl, the Lime required to reach O2 evolution potential in de-aerated solutions is less that in aerated solutions when inhibitor increases from 0 to 0.3 wt. %. (3) In presence of sufficient chloride in de-aerated Ca(OH)i solution, the passive film may broken down locally.
The inhibitive action of Reactive Red (RR31) dye against corrosion of carbon steel in 1M acetic acid solution has been studied using gravimetric method at temperature ranged (288-318)K. The antibacterial activity for the different concentrations of RR31 dye against different bacterial species was studied. The experimental data indicates that this dye acts as a potential inhibitor for carbon-steel in acetic acid medium and the protection efficiency increase with increasing (RR31) dye. The adsorption of (RR31) dye on the carbon steel surface was found to follow Langmuir adsorption isotherm. Thermodynamic data for the adsorption process such as Gibbs free energy change ∆Gads, enthalpy change ∆Hads, and entropy change ∆Sads were estima
... Show MoreAdsorption of Acetone and 2-Butanone on Iraqi siliceouns rocks powder have been investigated. UV technique has been used to determine the adsorption isotherms. The results showed that the adsorption isotherms obeyed Freundlich adsorption equation. The results showed that the adsorption increases with increasing acidity of solutions. The adsorption was exothermic process, increasing temperature leads to decreasing adsorption. H, S, G were calculated
The study included adding antimony oxide to mixtures of coating metal surfaces (Enameling), after it was selected ceramic materials used in the coating metal pieces of the type of steel and cast iron in two layers. The first is called a ground coat and the second is a cover coat.
Ceramic materials layer for ground coat have been melted down in
platinum crucible at a temperature of 1200oC to prepare the glass
mixture (Frit). It was coated on metals at a temperature of 780oC for
two minutes, while the second layer was prepared glass mixture
(Frit) at a temperature of 1200oC, but was coated at a temperature of
760oC for two minutes.
Underwent tests crystalline state of powders (Frits) and enameled samples using X-ray di
Background: The demand for esthetic orthodontic appliances is increasing; so the esthetic orthodontic archwires were introduced. Among them, Teflon and Epoxy coated stainless steel archwires. The amount of force available from the archwire depends on the structural properties and susceptibility to corrosion. All metallic alloys are changed during immersion in artificial saliva, chlorhexidine mouthwash andtoothpaste, but their behaviors differ from one type to another. They corrode at different rates, which lead to decrease the amount of force applied to the teeth. This in vitro study was designed to evaluate the corrosion pits in stainless steel archwires coated with Teflon and with Epoxy in dry and after immersion in artificial saliva, chl
... Show MoreIn the present work, Response Surface Methodology (RSM) was utilized to optimize process variables and find the best circumstances for indirect electrochemical oxidation of mimicked wastewater to remove phenol contaminants using prepared ternary composite electrode. The electrodeposition process is used for the synthesis of a ternary composite electrode of Mn, Co, and Ni oxides. The selected concentrations of metal salts of these elements were 0.05, 0.1, and 1.5 M, with constant molar ratio, current density, and electrolysis time of 1:1:1, 25 mA/cm2, and 2 h. Interestedly, the gathered Mn-Co-Ni oxides were deposited at both the anode and cathode. X-ray diffraction (XRD) and scanning electron microscopy (SEM) facilitated the qualitative char
... Show MoreThe purpose of this paper is to apply different transportation models in their minimum and maximum values by finding starting basic feasible solution and finding the optimal solution. The requirements of transportation models were presented with one of their applications in the case of minimizing the objective function, which was conducted by the researcher as real data, which took place one month in 2015, in one of the poultry farms for the production of eggs
... Show MoreAnew mixed compound complexes derived from 2-phenyl-2-(o-tolylamino) Acetonitrile as primary ligand (L1) and histidine (L2) as secondary ligand have been prepared and characterized by conventional techniques, elemental microanalysis (C.H.N), Fourier transform infrared, ultra violet-visible spectra, , flame atomic absorption, molar conductivity, magnetic susceptibility measurement and 1H-NMR spectra. From IR data which appear chelating behavior of the amino acid ligand (L2) toward transition metal ions is via carboxylate oxygen, amino nitrogen and imidazol nitrogen as tridentate ligand while second ligand (L1) chelating through N-nitrile and N-aniline, according to all above technics the octahedral shapes were expected for these complexes as
... Show MoreThe synchronization of a complex network with optoelectronic feedback has been introduced theoretically, with use of 2×2 oscillators network; each oscillator considered is an optocoupler (LED coupled with photo-detector). Fixing the bias current (δ) and increasing the feedback strength (Ԑ) of each oscillator, the dynamical sequence like chaotic and periodic mixed mode oscillations has been observed. Synchronization of unidirectionally coupled of light emitting diodes network has been featured when coupling strength equal to 1.7×10-4. The transition between non-synchronization and synchronization states by means of the spatio-temporal distribution has been investigated.