The object of this work is to investigate the effect of the addition of methanol on the shelf life and color characteristics of novolak resin. Different percentages were added and two mechanisms were suggested for the addition. High ortho structure (1, 2-3) novolak resin was prepared and used in the above investigation. Experimental determination using FT-IR and UV-spectroscopy showed that on the addition of 30% of methanol and according to the second mechanism of addition novolak shelf life increased to 12 months without obvious decomposition and color change. It is suggested that methanol plays an important role in the inhabitation of the reactive sites on the resin that are responsible for the oxidation of the polymer when exposed to atmospheric or storage conditions.
This paper presents an investigation to the effect of the forming speed on healing voids that inhabit at various size in an ingot. The study was performed by using finite element method with bilinear isotropic material option, circular type voids were considered. The closure index was able to predict the minimum press force necessary to consolidate voids and the reduction. The simulation was carried out, on circular cross-section lead specials containing a central void of different size. At a time with a flat die, different ratio of inside to outside radius was taken with different speed to find the best result of void closure.
Abstract
In the present study, composites were prepared by Hand lay-up molding. The composites constituents were epoxy resin as a matrix, 6% volume fractions of glass fibers (G.F) as reinforcement and 3%, 6% volume fractions of preparation natural material (Rice Husk Ash, Carrot Powder, and Sawdust) as filler. Studied the erosion wear behavior and coating by natural wastes (Rice Husk Ash) with epoxy resin after erosion. The results showed the non – reinforced epoxy have lower resistance erosion than natural based material composites and the specimen (Epoxy+6%glass fiber+6%RHA) has higher resistance erosion than composites reinforced with carrot powder and sawdust at 30cm , angle 60
... Show MoreThis research is devoted to study the effect of different in weight percentage of Sio2 particles and glass fibers (5, 10, 15, 20) wt. % on the wear rate epoxy resin. The results show that the value of hardness increase with the increase for the weight percentage of reinforcing particles and fibers, while the wear rate decrease with the increase the load level of the reinforcing particles and fibers . The largest value of the hardness, and the lowest value of the wear rate for epoxy reinforced with 20% of SiO2, the wear rate increase in general with increasing the applied load.
The D.C electrical and thermoelectrically properties of randomly mixed isolator – electrolyte system as (Al/ PVC – LiF/Al) junction consisting of polyvinyl chloride (PVC)resin reinforced with Lithium Fluoride (LiF) powder were studied. A comparison is made the properties of (PVC) material with varying percentage of (LiF) powder (0%, 30%, 50%, 80%)to find out the effect of reinforcement of isolator material. The composites dissolving in 10ml form tettraHaedroflourn (THF) and Solution were the castled in Petri dish and Laved it dry in the air, The out coming Sample were disc - Like shape of a diameter of about 3cm and thickness reneged between (0.01- 0.018) cm . The composites dissolving in 10ml form tettraHaedroflourn (THF) a
... Show MoreThe presence of heavy metals in the environment is major concern due to their toxicity. In the present study a strong acid cation exchange resin, Amberlite IR 120 was used for the removal of lead, zinc and copper from simulated wastewater. The optimum conditions were determined in a batch system of concentration 100 mg/L, pH range between 1 and 8, contact time between 5 and 120 minutes, and amount of adsorbent was from 0.05 to 0.45 g/100 ml. A constant stirring speed, 180 rpm, was chosen during all of the experiments. The optimum conditions were found to be pH of 4 for copper and lead and pH 6 for zinc, contact time of 60 min and 0.35 g of adsorbent. Three different temperatures (25, 40 and 60°C) were selected to investigate the effect
... Show MoreIn this work , the effect of chlorinated rubber (additive I), zeolite 3A with chlorinated rubber (additive II), zeolite 4A with chlorinated rubber (additiveIII), and zeolite 5A with chlorinated rubber (additive IV), on flammability for epoxy resin studied, in the weight ratios of (2, 4, 7,10 & 12%) by preparing films of (130x130x3) mm in diameters, three standard test methods used to measure the flame retardation which are ; ASTM : D-2863 , ASTM : D-635 & ASTM : D-3014. Results obtained from these tests indicated that all of them are effective and the additive IV has the highest efficiency as a flame retardant.
In this research, a group of complexes were prepared which were derived from Schiff base ligands, which is called (1E,1'E)-1,1'-(1,2-phenylene)bis(N-(2,4-dichlorophenyl) methanimine) (L) with ortho-phenanthroline (o-phen).The prepared complexes areM(II) [Co(II),Ni(II),Cu(II), Zn(II), Cd(II),and Hg(II)].A range of spectroscopic and technical techniques have been used to characterizethese materials, including:The FTIR, 1H-NMR, LC-Mass Spectrum, UV-Visbale, molar conductance, and magnaticmoment, atomic absorbtion, chlorid contents. Spectral results obtainedare showen that (ortho-phen) and (L) behave as neutral coordinating to the central metal ion by the donatingatoms(N2)of the both compounds. The geometry sha
... Show MoreBackground: Implant stability is considered one of the most important factors affecting healing and successful osseointegration of dental implants. The aims of the study were to measure the implant stability quotient (ISQ) values during the healing period and to determine the factors that affect implant stability. Materials and methods: Thirty patients enrolled in the study (17 female, 13 male). They received 44 Implantium® Dental Implants located as the following: 22 implants in maxillary jaw, 22 implants in mandibular jaw from them 17 implants in anterior segment and 27 in posterior segment. The bone density determined using interactive CT scan and classified according to the Misch bone density classification (29 implants in (D3), 15 i
... Show More