Preferred Language
Articles
/
ijcpe-388
POLYVINYL ALCOHOL/POLYVINYL CHLORIDE (PVA/PVC) HOLLOW FIBER COMPOSITE NANOFILTRATION MEMBRANES FOR WATER TREATMENT
...Show More Authors

Two different polyvinyl alcohol/polyvinyl chloride (PVA/PVC) hollow fiber composite nanofiltration membranes were prepared after PVC hollow fiber membranes were coated using dip-coating method with PVA aqueous solution, which was composed of PVA, fatty alcohol polyoxyethylene ether (AEO9), and water [PVA/AEO9/water (4:0.5:95.5) wt%]. Effect of two different PVC hollow fiber immersion times in coating solution were studied. Cross-section, internal and external surfaces of the PVC hollow fibers and PVA/PVC composite nanofiltration membranes structures were characterized by scanning electron microscopy (SEM), pure water permeation flux and solutes rejection. It was found that, the coating layer thickness on the outer surface of the 19 wt% PVC hollow fiber was thin and about (6μm), while the coating solution penetrates through the outer edge of the PVC hollow fiber and it looks like sponge-like structure with increase of the dip-coating time from 20 to 30 sec. Besides, the pure water permeation flux decreases and solutes rejection increases with an increase of the coating time from 20 to 30 sec for the two PVA/PVC composite nanofiltration membranes. Molecular weight cut-off (MWCO) of the PVA/PVC composite nanofiltration membranes were in the range of NF (i.e. 200-3000 Mw).

View Publication Preview PDF
Quick Preview PDF
Publication Date
Tue Dec 01 2020
Journal Name
Iop Conference Series: Materials Science And Engineering
Effect of Adding Chopped Carbon Fiber (CCF) on the Improvement of Gypsum Plaster Characteristicssss
...Show More Authors
Abstract<p>The current work studies the effect of adding chopped carbon fiber (CCF) on gypsum plaster properties (precisely the compressive strength and the modulus of rupture). The research plan consists of using six mixes of gypsum plaster; these mixes are divided into two groups according to the (Water/Gypsum) ratios (0.5 & 0.6). Each group was divided into three subgroups according to CCF volume fraction (Vf): 0.0%, 0.2% and 0.4%. Three cubic (50×50×50) mm and three prismatic (40×40×160) mm samples were performed for each mix. It was found that, the addition of CCF to the gypsum plaster mixes increases both the compressive strength and the modulus of rupture for both (W/G) ratios, an</p> ... Show More
View Publication
Scopus (9)
Crossref (13)
Scopus Crossref
Publication Date
Sat Jan 02 2021
Journal Name
Al-qadisiyah Journal For Engineering Sciences
Improving the Moisture Damage Resistance of HMA by Using Ceramic Fiber and Hydrated Lime
...Show More Authors

The Moisture damage is considered as one of the main challenge for the experts in the field of asphalt pavement design. The aims of the present study is to modify moisture resistance of the asphalt concrete by utilizing ceramic fibers as a type of reinforcement incorporated with hydrated lime. For this purpose, a penetration grade of the asphalt cement (40-50) was utilized as a binder with an aggregate of the maximum nominal size of 12.5mm and mineral filler limestone dust. A series of specimens has been fabricated by utilizing 0.50, 1.0, 1.5, and 2.0 percentages of ceramic fibers. For each of these contents, another subsequent group of specimens with hydrated lime with 0.0, 1.0, 1.5, and 2.0 percentages were moulded. For the additi

... Show More
Crossref (1)
Crossref
Publication Date
Sat Aug 01 2020
Journal Name
Journal Of Constructional Steel Research
Demountable steel-concrete composite beam with full-interaction and low degree of shear connection
...Show More Authors

It is suitable to use precast steel-concrete composite beams to quickly assemble a bridge or a building, particularly in isolated regions where cast-in-situ concrete is not a practical option. If steel-concrete composite beams are designed to allow demountability, they can also be extremely useful in the aftermath of natural disasters, such as earthquakes or flooding, to replace damaged infrastructure. Furthermore, rapid replacement of slabs is extremely beneficial in case of severe deterioration due to long-term stressors such as fatigue or corrosion. The only way to rapidly assemble and disassemble a steel-concrete composite structure is to use demountable shear connectors to connect/disconnect the steel beams to/from the concrete slab. I

... Show More
View Publication
Scopus (47)
Crossref (37)
Scopus Clarivate Crossref
Publication Date
Sat Feb 27 2021
Journal Name
Journal Of Engineering
Effect of Web Stiffeners on The Flexural Behavior of Composite GFRP- Concrete ‎Beam Under Impact Load
...Show More Authors

In this paper, numerical and experimental studies on the elastic behavior of glass fiber reinforced ‎polymer (GFRP) with stiffeners in the GFRP section's web (to prevent local buckling) are presented. ‎The GFRP profiles‎ were connected to the concrete deck slab by shear connectors. Two full-scale simply supported ‎composite beams (with and without stiffeners) were tested under impact load (three-point load) to ‎assess its structural response. The results ‎proved that the maximum impact force, maximum ‎deflection, damping time, and ‎damping ratio of the composite beam were affected by the GFRP ‎stiffeners‎. The experimental results indicated that the damping ratio and deflection were diminished compare

... Show More
View Publication Preview PDF
Crossref (14)
Crossref
Publication Date
Thu Mar 31 2016
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
Synthesis and Characterization of Nanocrystalline Micro-Mesoporous ZSM-5/MCM-41 Composite Zeolite
...Show More Authors

Nanocrystalline micro-mesoporous ZSM/MCM-41 composite was synthesized using alkaline treatment method and two step of crystallization in poly tetraflouroethylene (PTFE) lined autoclave. The synthesized zeolites was characterized by X-Ray diffraction (XRD), Scanning electron microscopy (SEM), Transmission electron microscopy (TEM), Atomic force microscopy (AFM), Fourier transport infrared (FTIR), and N2 adsorption-desorption (BET). It was approved that the best results for alkaline leaching can be got with 1.5M NaOH solution. High surface (BET) area of 630 m2/g with pore volume of 0.55 cm3/g has been got. AFM reports showed a nano-level size for average particle size of 50nm.

View Publication Preview PDF
Publication Date
Fri Apr 01 2022
Journal Name
Separation And Purification Technology
Application of central composite design approach for optimisation of zinc removal from aqueous solution using a Flow-by fixed bed bioelectrochemical reactor
...Show More Authors

View Publication
Scopus (19)
Crossref (15)
Scopus Clarivate Crossref
Publication Date
Fri Apr 01 2022
Journal Name
Separation And Purification Technology
Application of central composite design approach for optimisation of zinc removal from aqueous solution using a Flow-by fixed bed bioelectrochemical reactor
...Show More Authors

View Publication
Scopus (19)
Crossref (15)
Scopus Clarivate Crossref
Publication Date
Thu Sep 15 2022
Journal Name
Journal Of Baghdad College Of Dentistry
12- months color stability of direct resin composite veneers in anterior teeth: Clinical trial
...Show More Authors

Background: This clinical trial aims to evaluate the color changes of direct resin composite veneer (DCV) restorations based on spectrophotometric analysis of 4 different types of resin composites between the baseline immediately after polishing and after one year of follow-up. Materials and methods: 28 patients were assessed for eligibility for participation, aged between 18 and 38 years old, who indicated for DCV restorations in anterior maxillary teeth were considered for participation in this study. In total, 25 patients who met the inclusion criteria were selected (6 males and 19 females, mean age: 20.9 at the time of restoration placement), and 3 patients were excluded. Partic

... Show More
View Publication Preview PDF
Scopus (4)
Crossref (3)
Scopus Crossref
Publication Date
Wed Nov 01 2023
Journal Name
Ecological Engineering &amp; Environmental Technology
Synthesis of Mn-Co-Ni Composite Electrode by Anodic and Cathodic Electrodeposition for Indirect Electro-oxidation of Phenol – Optimization of the Removal by Response Surface Methodology
...Show More Authors

In the present work, Response Surface Methodology (RSM) was utilized to optimize process variables and find the best circumstances for indirect electrochemical oxidation of mimicked wastewater to remove phenol contaminants using prepared ternary composite electrode. The electrodeposition process is used for the synthesis of a ternary composite electrode of Mn, Co, and Ni oxides. The selected concentrations of metal salts of these elements were 0.05, 0.1, and 1.5 M, with constant molar ratio, current density, and electrolysis time of 1:1:1, 25 mA/cm2, and 2 h. Interestedly, the gathered Mn-Co-Ni oxides were deposited at both the anode and cathode. X-ray diffraction (XRD) and scanning electron microscopy (SEM) facilitated the qualitative char

... Show More
View Publication Preview PDF
Scopus (4)
Crossref (3)
Scopus Crossref
Publication Date
Fri Dec 31 2021
Journal Name
Iraqi Journal Of Market Research And Consumer Protection
ADSORPTION POTENTIAL FOR A MIXTURE OF CHEMICALLY AND THERMALLY TREATED CLAYS TO REMOVE ORANGE G DYE FROM WASTE-WATER: ADSORPTION POTENTIAL FOR A MIXTURE OF CHEMICALLY AND THERMALLY TREATED CLAYS TO REMOVE ORANGE G DYE FROM WASTE-WATER
...Show More Authors

This study examined the adsorption behavior of anionic dye (orange G) from aqueous solution onto the raw and activated a mixture of illite, kaolinite and chlorite clays from area of Zorbatiya (east of Iraq).The chemical treatment involved alkali and acid activation. The alkali activation obtained by treated the raw clay (RC) with 5M NaOH (ACSO) and the acid activation founded by treated it with 0.25M HCl (ACH) and 0.25M  (ACS). The thermal treatment carried out by calcination the produce activated clay at 750oC for acid activation and 105oC for alkali activation. Batch

... Show More