The corrosion of low carbon steel boiler tubes in demi water had been investigated. The purpose of this investigation was to determine the change produced in corrosion behavior of the carbon steel as a result of the specific presence of chloride and copper ions in the water under different temperatures. For low carbon steel experiments, the temperature was taken in three levels (125, 175, and 215°C) under about 27 bar pressure and 1500 rpm in autoclave. Using weight loss technique, the corrosion rate ranges from (85 to 789 gmd) for low carbon steel boiler tubes.
This research was carried out to determine the impact of heat shock, electric shock and seeds in soaking nitrous acid mutagen solution on three cultivars of faba beans plant (Zaina, Aguadulce and Local) at the year 2012-2013. Factorial experiment was arranged in randomized complete block design (RCBD) with three replicates were used. The results showed that heat shock lead to early plants of 50% in flowering and an increase in the number of branches/plant and the number of seeds/pod compared to other treatments, whereas the seeds soaked in nitrous acid mutagen solution gave the highest plant height, leaf area index, number of pods/plant, seed weight, seed yield kg/ha, and did not differ significantly with treatment of electric shock in the
... Show MoreThe electric quadrupole moments for some scandium isotopes (41, 43, 44, 45, 46, 47Sc) have been calculated using the shell model in the proton-neutron formalism. Excitations out of major shell model space were taken into account through a microscopic theory which is called core polarization effectives. The set of effective charges adopted in the theoretical calculations emerging about the core polarization effect. NushellX@MSU code was used to calculate one body density matrix (OBDM). The simple harmonic oscillator potential has been used to generate the single particle matrix elements. Our theoretical calculations for the quadrupole moments used the two types of effective interactions to obtain the best interaction compared with the exp
... Show MoreThis research investigates manganese (Mn) extraction from Electric Arc Furnace Steel Slag (EAFS) by using the Liquid-liquid extraction (LLE) method. The chemical analysis was done on the slag using X-ray fluorescence, X-ray diffraction, and atomic absorption spectroscopy. This work consisted of two parts: the first was an extensive study of the effect of variables that can affect the leaching process rate for Mn element from slag (reaction time, nitric acid concentration, solid to liquid ratio, and stirring speed), and the second part evaluates the extraction of Mn element from leached solution. The results showed the possibility of leaching 83.5 % of Mn element from the slag at a temperature of 25°C, nitric acid co
... Show MoreThe heavy metals Cd, Cu, Fe, pb, and Zn were determined in dissolved and particulate phases of the water,in addition to exchangeable and residual phases of the sediment and in the selected organs of the fish Cyprinus carpio collected from the Euphrates River near Al-Nassiriya city center south of Iraq during the summer period / 2009 .Also sediment texture and total organic carbon(TOC) were measured. Analysis emploing a flam Atomic Absorption Spectrophotometers . The mean regional concentrations of the heavy metals in dissolved (µg/l) and particulate phases (µg/gm) dry weight were Cd (0.15,16.13) ,Cu (0.59,24.48) ,Fe (726,909.4) ,Pb (0.20, 49.95) and Zn (2.5,35.62) respectively,and those for exchangeable and residual phases of the
... Show MoreKS Ismaeil, BR Jawad, Journal of Physical Education, 2023
Electrochemical corrosion of hydroxyapatite (HAP) coated performance depends on various parameters like applied potential, time, thickness and sintering temperature. Thus, the optimum parameters required for the development of stable HAP coatings was found by using electrophoretic deposition (EPD) technique. This study discusses the results obtained from open circuit potential-time measurements (OCP-time), potentiodynamic polarisation and immersion tests for all alloy samples done under varying experimental conditions, so that the optimum coating parameters can be established. The ageing studies of the coated samples were carried out by immersing them in Ringer’s solution for a period of 30 days indicates the importance of stable HAP c
... Show MoreInternal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone
... Show More