This work deals with thermal cracking of slack wax produced as a byproduct from solvent dewaxing process of medium lubricating oil fraction in AL-Dura refinery. The thermal cracking process was carried out at a temperature ranges 480-540 ºC and atmospheric pressure. The liquid hourly space velocity (LHSV) for thermal cracking was varied between 1.0-2.5 . It was found that the conversion increased (61 - 83) with the increasing of reaction temperature (480 - 540) and decreased (83 - 63) with the increasing of liquid hourly space velocity (1.0 - 2.5).
The maximum gasoline yield obtained by thermal cracking process (48.52 wt. % of feed) was obtained at 500 ºC and liquid hour space velocity 1 . The obtaining liquid product at the best operating condition 500 ºC and LHSV 1 was fractionated into wide range fractions. Based on the determination of some properties for the distilled fractions and comparison (these properties with that required by standard requirements) it is possible to use the fractions of cracking products as a component for production of automobile gasoline, domestic kerosene, light diesel fuel and basic lubricating oils.
Pyogenic granuloma is one of the inflammatory hyperplasia seen in the oral cavity. The
present study included 10 patients with pyogenic granuloma, involving 4 males and 6 females with 1:1.5
male to female ratio. Patient ages ranged from 5 to 85 years (mean, 30 years) and half of the lesions had
pedunculated base, with surface ulceration in 10% of cases. Treatment consisted of resection, using 810
nm diode lasers. Eight patients were anesthetized during the surgical operation by local infiltration of
anesthesia. Only three patients reported mild post-operative pain within the first 24 hours of the healing
period. During the surgical operation there was no significant bleeding so clear surgical field. There was
no blee
Pyogenic granuloma is one of the inflammatory hyperplasia seen in the oral cavity. The
present study included 10 patients with pyogenic granuloma, involving 4 males and 6 females with 1:1.5
male to female ratio. Patient ages ranged from 5 to 85 years (mean, 30 years) and half of the lesions had
pedunculated base, with surface ulceration in 10% of cases. Treatment consisted of resection, using 810
nm diode lasers. Eight patients were anesthetized during the surgical operation by local infiltration of
anesthesia. Only three patients reported mild post-operative pain within the first 24 hours of the healing
period. During the surgical operation there was no significant bleeding so clear surgical field. There was
no blee
KE Sharquie, AA Noaimi, MS Al-Zoubaidi, Journal of Cosmetics, Dermatological Sciences and Applications, 2015 - Cited by 8
This study investigated the treatment of dairy wastewater using the electrocoagulation method with iron filings as electrodes. The study dealt with real samples collected from local factory for dairy products in Baghdad. The Response Surface Methodology (RSM) was used to optimize five experimental variables at six levels for each variable, for estimating chemical oxygen demand (COD) removal efficiency. These variables were the distance between electrodes, detention time, dosage of NaCl as electrolyte, initial COD concentration, and current density. RSM was investigated the direct and complex interaction effects between parameters to estimate the optimum values. The respective optimum value was 1 cm for the distance between electrodes, (6
... Show MoreGlassy polymers like Poly Mathyel Metha Acrylate are usually classified as non-porous materials; they are almost considered as fully transparent. Thin samples of these materials reflect color changing followed by porous formation and consequently cracking when exposed to certain level of ?-irradiation. The more the dose is the higher the effect have been observed. The optical microscope and UV-VIS spectroscopy have clearly approved these consequences especially for doped polymers.
Indium oxide In2O3 thin films fabricated using thermal evaporation of indium metal in vacuum on a glass substrate at 25oC using array mask, after deposition the indium films have been subjected to thermal oxidation at temperature 400 °C for 1h. The results of prepared Indium oxide reveal the oxidation method as a strong effect on the morphology and optical properties of the samples as fabricated. The band gap (Eg) of In2O3 films at 400 °C is 2.7 eV. Then, SEM and XRD measurements are also used to investigate the morphology and structure of the indium oxide In2O3 thin films. The antimicrobial activity of indium oxide In2O3 thin films was assessed against gram-negative bacterium using inhibition zone of bacteria which improved higher ina
... Show MoreThe effect of solution heat treatment on the mechanical properties of Aluminum-Copper alloy. (2024-T3) by the rolling process is investigated. The solution heat treatment was implemented by heating the sheets to 480 C° and quenching them by water; then forming by rolling for many passes. And then natural aging is done for one month. Mechanical properties (tensile strength and hardness) are evaluated and the results are compared with the metal without treatment during the rolling process. ANSYS analysis is used to show the stresses distribution in the sheet during the rolling process. It has been seen that good mechanical properties are evident in the alloy without heat treatment due to the strain hardening and also the mechanical
... Show MoreSteel fiber aluminum matrix composites were prepared by atomization technique. Different air atomization conditions were considered; which were atomization pressure and distance between sample and nozzle. Tensile stress properties were studied. XRF and XRD techniques were used to study the primary compositions and the structure of the raw materials and the atomized products. The tensile results showed that the best reported tensile strength observed for an atomization pressure equal to 4 mbar and sample to nozzle distance equal to 12 cm. Young modulus results showed that the best result occurred with an air atomization pressure equal to 8 mbar and sample to nozzle distance equal to 16cm