Nano-crystalline iron oxide nanoparticles (magnetite) was synthesized by open vessel ageing process. The iron chloride solution was prepared by mixing deionized water and iron chloride tetrahydrate. The product was characterized by X-Ray, Surface area and pore volume by Brunauer-Emmet-Teller, Atomic Force Microscope (AFM) and Fourier Transform Infrared Spectroscopy(FTIR) . The results showed that the XRD in compatibility of the prepared iron oxide (magnetite) with the general structure of standard iron oxide, and in Fourier Transform Infrared Spectroscopy, it is strong crests in 586 bands, because of the expansion vibration manner related to the metal oxygen absorption band (Fe–O bonds in the crystals of iron oxide). The results show that the prepared nano iron oxide is with average crystal size 75.92 nm, surface area was 85.97 m2/g and the pore volume was found equal to 0.1566 cm3/
In this work, composite materials were prepared by mixing different concentrations of ferrites with polyacrylonitrile (PAN) polymer. Using the electrospinning technique, these composites were deposited on a p-type silicon wafer. The prepared samples demonstrated nanofibers in both pure PAN polymers and their composites with ferrite. Prior to examining the humidity sensing effectiveness with a percentage of relative humidity at a frequency of 10 kHz, based on ambient temperature and a relative humidity range of 50–100%, the composite nanofibers demonstrated stronger humidity sensing compared to the pure PAN nanofibers, which demonstrated a powerful resistance response. More precisely, the PAN@ferrite nanocomposite showed a broad adsorption
... Show More4-Amino-N-(5-methyl-isaxazol-3-yl)-benzenesulfonamide, a new azo (LH) ligand, was synthesized by reacting the diazonium salt of Sulfamethoxazole with coupling compound 3-amino phenol. Spectroscopic techniques (UV-Vis, FTIR, 1H &13C-NMR, and LC-Mass) as well as micro elemental analyses (C.H.N.O) and TGA and SDC were used to identify the azo ligand. Complexes of (Zn(II), Cr(III), Cu(II) and VO(II)) were produced and characterized by atomic absorption, elemental microanalysis, infrared, LC-Mass, TGA, DSC and UV-Vis spectral techniques, as well as conductivity and magnetic quantifications. All the complexes had a 1:2 metal-ligand ratio, and non-electrolytes at all complexes and tetrahedral geometry suggested except Cr-complex, which demonstrate
... Show MoreNatural polymers are often non-toxic, biodegradable, biocompatible, and safe. A novel ligand was synthesized as a natural polymer using chitosan and oleander plant extract [(2R,3S,4R,5S)-5-(acetoxyamino)-4-hydroxy-3,6-dimethoxytetrahydro-2H-pyran-2-yl) methyl (16R)-3-(((2S,4S,5R)-4-methoxy-2,5-dimethyltetrahydro-2H-pyran-2-yl)oxy-10,13,16-trimethyl-17-(5-oxo-2,5-dihydrofuran-3-yl) hexadecahydro-14H-cyclopenta [a] phenanthren-14-yl) phthalate] (Chitosan-Ph-Oleander). This ligand and its complexes with several metals (Cr+3, Mn+2, Fe+3, Ni+2, Cu+2, Zn+2) were characterized using FTIR, UV-visible and 1H-NMR spectroscopy, as well as by molar conductivity, magnetic moment, and TGA analysis. The biological activity for the prepared polymer
... Show MoreDiazotization reaction between 1-(2,4,6-Trihydroxy-phenyl)-ethanone and diazonium salts was carried out resulting in ligand 4-(3-Acetyl-2,4,6-trihydroxy-phenylazo)-N-(5-methyl-isoxazol-3-yl)-benzenesulfonamide, this in turn reacted with the next metal ions (V4+ , Cr3+ , Mn2+ and Cu2+) forming stable complexes with unique geometries such as (Octahedral for both Cr3+ , Mn2+ and Cu2+ ,squar pyramidal for V4+). The creation of such complexes was detected by employing spectroscopic means involving ultraviolet-visible which proved the obtained geometries, fourier transfer proved the formation of azo group and and the coordination with metal ion through it. Pyrolysis (TGA & DSC) studies proved the coordination of water residues with me
... Show MoreA new series of 5-methoxy-2-mercapto benzimidazole derivatives were synthesized by the reaction of 5-methoxy- 2-mercaptobenzimidazole with chloroacetic acid and affords 2-((5-methoxy-1H-benzo[d]imidazol-2-yl)thio) acetic acid (1),which on cyclization with acetic anhydride and pyridine gives 7- methoxybenzo[4,5]imidazo[2,1-b]thiazol- 3(2H)-one(2), which on condensation with different aryl aldehydes in the presence of anhydrous sodium acetate in glacial acetic acid, furnishes a arylidene thiazolidinone. The purity of the synthesized compounds was confirmed by melting point and TLC.The structures were established by different spectral analysis such as FTIR,1HNMR, and CHN analysis. The newly synthesized compounds (3a-d) were in vivo evaluated f
... Show MoreGel polymer electrolytes (GPEs) have attracted considerable attention for rechargeable battery applications because of their high ionic conductivity, mechanical flexibility, and enhanced safety. In the present work, copper-ion-conducting PVA/HPMC gel polymer electrolytes were successfully prepared by the solution casting method using a 50:50 PVA/HPMC blend. Different CuSO₄ concentrations (10, 20, and 30 wt%) were incorporated into the polymer matrix, followed by the addition of 3 mL PANI/[BMIM][BF₄] polyionic liquid. The prepared electrolytes were characterized using scanning electron microscopy (SEM), differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), and electrochemical impedance spectroscopy (EIS). SEM analysi
... Show MoreIn this paper, CdS/Si hetrojunction solar cell has been made by
Chemical Bath Deposition (CBD) of CdS thin film on to
monocrystalline silicon substrate. XRD measurements approved that
CdS film is changing the structure of CdS films from mixed
hexagonal and cubic phase to the hexagonal phase with [101]
predominant orientation. I-V characterization of the hetrojunction
shows good rectification, with high spectral responsivity of 0.41
A/W, quantum efficiency 90%,and specific detectivity 2.9*1014
cmHz1/2W -1 .
This article includes the preparation of luminescence materials from rare earth (Eu ) ion doping Yttrium Oxide (Y2O3) 70% and SiO2 25% and study the characteristics of phosphors for ultraviolet to visible conversion. The phosphor materials have been synthesized by two steps: Preparing the powder by solid state method using Y2O3, SiO2 and Eu2O3 with doping materials concentration (70%, 25% and 5%) respectively and different calcination temperature (1000, 1200 and 1400 oC).
The second step is to prepare the colloid solution by dispersing the produced powder in a polyvinyl alcohol solution (4%) .
Powde