This study presents a comprehensive set of laboratory works for the examined soil layers extracted from Baghdad city (specifically from Alkadhimya, Alaitaifiya, and Alhurriya) to illustrate their engineering properties. The researchers have adopted the unified soil classification system for soil classification purposes. Also, the direct shear test was performed for soil samples with various degrees of saturation (0%, 25%, 50%, 75%, and 100%). The test results have shown a significant reduction in cohesion property with higher moisture content within soil samples. Also, a noticeable reduction in angle of internal friction value has occurred with such changes. Furthermore, it has been found that the bearing capacity of unsaturated soils ranged between 2000 and 3000 KPa, and about 500-700 KPa for the soaked soil samples.
Background: Directly observed therapy-short course (DOTS) had been adopted by World Health Organization (WHO) as hopeful strategy for treatment of tuberculosis (TB) since early nineties. Iraqi health authorities started DOTS implementation since 2001 in Baghdad. Coverage expanded gradually till 100% in 2004. War and unstable security condition hit Iraq since March 2003. Objective: The objective of this study was To evaluate the DOTS implementation program in Baghdad in different periods including 2 unstable periods for proper assessment of war and instability on treatment of TB. Patients and methods: This study had been conducted in Baghdad during four different periods (before and during 2003 war, after war; without and with DOTS). Dire
... Show MoreA factorial experiment (2× 3) in randomized complete block design (RCBD) with three replications was conducted to examine the effect of honeycomb selection method using three interplant distances on yield and its components of two cultivars of bean, Bronco and Strike. Interplant distances used were 75× 65 cm, 90× 78 cm, and 105× 91 cm (row× plant) represent short (high plant density), intermediate (intermediate plant density), and wide (low plant density) distance, respectively. Parameters used for selection were number of days from planting to the initiation of first flower, number of nodes formed prior to first flower, and number of main branches. Results showed significant superiority of the Bronco cultivar represented in the number
... Show MoreResults of a study of alloys and films with various Pb content have been reported and discussed. Films of of thickness 1.5
In this work, ZnO nanostructures for powder ZnO were synthesized by Hydrothermal Method. Size and shape of ZnO nanostructureas can be controlled by change ammonia concentration. In the preparation of ZnO nanostructure, zinc nitrate hexahydrate [Zn(NO3)2·6H2O] was used as a precursor. The structure and morphology of ZnO nanostructure have been characterized by scanning electron microscopy (SEM), atomic force microscopy (AFM), X-ray diffraction (XRD). The synthesized ZnO nanostructures have a hexagonal wurtzite structure. Also using Zeta potential and Particle Size Analyzers and size distribution of the ZnO powder
In this work, (CdO)1-x (CoO)x thin films were prepared on glass slides by laser-induced plasma using Nd:YAG laser with (λ=1064 nm) and duration (9 ns) at different laser energies (200-500 mJ) with ratio (x=0.5), The influence of laser energy on structural and optical properties has been studied. XRD patterns show the films have a structure of polycrystalline wurtzite. As for AFM tests results for the topography of the surface of the film, where the results showed that the grain size and the average roughness increase with increasing laser energy. The optical properties of all films were also studied and the results showed that the absorption coefficient for within the wavelength range (280-1100 nm), The value of the optical power gap fo
... Show MoreThin films of (CdO)x (CuO)1-x (where x = 0.0, 0.2, 0.3, 0.4 and 0.5) were prepared by the pulsed laser deposition. The CuO addition caused an increase in diffraction peaks intensity at (111) and a decrease in diffraction peaks intensity at (200). As CuO content increases, the band gap increases to a maximum of 3.51 eV, maximum resistivity of 8.251x 104 Ω.cm with mobility of 199.5 cm2 / V.s, when x= 0.5. The results show that the conductivity is ntype when x value was changed in the range (0 to 0.4) but further addition of CuO converted the samples to p-type.