This work aimed to study the effect of laser surface treatment on the mechanical characteristics and corrosion behaviour of grey cast iron type A159. Many technical applications used conventional surface treatment, but laser surface hardening has recently been used to enhance the surface properties of many alloys. The mechanical characteristics, including microstructure, microhardness, and wear resistance of A159 grey cast iron, were studied, in addition to corrosion behaviour. The experimental laser parameters in this work were 0.9, 1.2, and 1.5 KW power with continuous wave carbon dioxide lasers with scanning speeds of 10 and 12 mm/s were used. The results found that phase-transitional alterations in microstructure were influenced by laser therapy. Also, the microhardness increased with increasing power, with the maximum reaching approximately 950 HV while the base metal has an average of approximately 260 HV. Also, we found the power laser increased corrosion resistance by lowering the corrosion rate (CR) from 21.10 for the untreated sample to 1.02 (m.p.y.), additionally, corrosion protection efficiency (CPE) increased to 95.27 percent.
In this research local wheat peel was used as an adsorbent surface for removal of Azure B (AB) dye from the aqueous solution. The adsorption process was performed at different experimental parameters, equilibrium time, temperature, ionic strength and solution pH. The isotherms of adsorption are of H-type as compared with Giles curves and the adsorption data were coincide with Freundlich equation. The adsorption kinetic data were analyzed using pseudo- first and second order kinetic models. The effect of temperature was studied and the amount of dye adsorbed was found to increase with the increasing of temperature from 25 to 50 oC. The values of thermodynamic functions like enthalpy and entropy have been estimated. The quantity of adso
... Show MoreBackground: Dental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60
... Show MoreBackground: Dental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60
... Show MoreDental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60 test block w
... Show MoreThis study reports the fabrication of tin oxide (SnO2) thin films using pulsed laser deposition (PLD). The effect of 60Co (300, 900, and 1200 Gy) gamma radiation on the structural, morphological, and optical features is systematically demonstrated using X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), atomic force microscopy (AFM), and ultraviolet-visible light analysis (UV-Vis), respectively In XRD tests, the size of the crystallites decreased from 45.5 to 40.8 nm for the control samples and from 1200 Gy to 60Co for the irradiated samples. Using FESEM analysis, the particle diameter revealed a similar trend to that attained using XRD; in particular, the average diameters were 93.8 and
... Show MoreThe major aim of this research is study the effect of the type of lightweight aggregate (Porcelinite and Thermostone), type and ratio of the pozzolanic material(SF and HRM) and the use of different ratios of w/cm ratio(0.32 and 0.35) on the properties of SCLWC in the fresh and hardened state. SF and HRM are used in three percentage 5%,10%, and 15% as a partial replacement by weight of
cement for all types of SCLWC. The requirements of self-compatibility for SCC are fulfilled by using the high performance superplasticizer (G51) at 1.2liter per 100 kg of cement. The values of air dry density and compressive strength at age of 28 days within the limits of structural lightweight concrete. The air dry density and compressive strength at a
Abstract
Locally natural occurring Iraqi rocks of Bauxite and Porcelanite (after pre calcinations at 1000oC for 1hr) were used, with the addition of different proportions of MgO and Al2O3, to prepare refractory materials. The effects of these additives on the physical and thermal properties of the prepared refractories were investigated.
Many batches of Bauxite/MgO, Bauxite/Al2O3, Bauxite/MgO/Al2O3, and Porcelanite/ MgO/Al2O3 were prepared. The mixture is milled and classified into different size fractions; fine (less than 45μm) 40%, middle (45-75μm) 40%, and coarse (75-106μm) 20% .
... Show MoreA series of liquid crystals comprising a heterocyclics dihydro pyrrole and 1,2,3-triazole rings [VII]-[X] were synthesized by many steps starting from a reaction of 3,3'-dimethyl-[1,1'-biphenyl]- 4,4'-diamine with chloroacetyl chloride in a mixture of solutions DMF and TEA to synthesise the compounds [I], then the compounds [I] reacted with malononitrile in 1,4-dioxane and TEA solutions to produce compounds [II], then the first step is repeated with compound [II] where it reacted with chloroacetyl chloride in mixture of DMF and TEA to give compound [III], this compound reacted with sodium azide in the presence of sodium chloride and DMF as solvent to produce the compound [IV], which reacted with acrylic acid by a 1.3 dipolar reaction in sol