The deposition process and investigation of the physical properties of tungsten trioxide (WO3) thin films before and after gamma irradiation are presented in this paper. The WO3 thin films were deposited, using the pulse laser deposition technique, on glass substrates at laser energies of 600mJ and 800mJ. After deposition, the samples were gamma irradiated with Co60. The structural and optical properties of polycrystalline WO3 thin films are presented and discussed before and after 5kGy gamma irradiation at the two laser energies. X-ray diffraction spectra revealed that all the films consisted of WO3 crystallized in the triclinic form; the dislocation density and lattice strain increased with the absorbed dosage of gamma irradiation. The optical constants, the average diameter and the surface roughness of the WO3 films were calculated before and after gamma irradiation and for the two laser energies. It was found that the WO3 thin films conductivity increased by γ-irradiated and with the increase of the laser energy.
We investigated at the optical properties, structural makeup, and morphology of thin films of cadmium telluride (CdTe) with a thickness of 150 nm produced by thermal evaporation over glass. The X-ray diffraction study showed that the films had a crystalline composition, a cubic structure, and a preference for grain formation along the (111) crystallographic direction. The outcomes of the inquiry were used to determine these traits. With the use of thin films of CdTe that were doped with Ag at a concentration of 0.5%, the crystallization orientations of pure CdTe (23.58, 39.02, and 46.22) and CdTe:Ag were both determined by X-ray diffraction. orientations (23.72, 39.21, 46.40) For samples that were pure and those that were doped with
... Show MoreThe aim of this work was directed to measure the cosmic ray (CR)
flux and the background (BG) absorbed dose rate for districts of
Baghdad city. The maximum values of CR flux was 2.01
(particle/cm2.s) registered for several Baghdad districts and the
minimum was 0.403 (particle/cm2.s) belonging to Al-kadhimiya
district, whereas the overall average value was 1.24 (particle/cm2.s).
The BG measurements showed that the maximum absorbed dose was
25 nSv/h belonging to Noab AL-Dhbat district and the minimum
absorbed was 19.01 nSv/h observed in Al-Ghadeer district, while
the overall average was 22.56 nSv/h, and this value is small than the
Iraqi permissible limit, which is restricted by Iraqi Center of
Radiation Pr
Thin films of CdTe were prepared with thickness (500, 1000) nm on the glass substrate by vacuum evaporation technique at room temperature then treated different annealing temperatures (373,473,and 573)K for one hour. Results of the Hall Effect and the electrical conductivity of (I-V) characteristics were measured in darkness and light.at different annealing temperature results show that the thin films have ability to manufacture solar cells, and found that the efficient equal to (2.18%) for structure solar cell (Algrid / CdS / CdTe /glass/ Al) and the efficient equal to (1.12%) for structure solar cell (Algrid / CdS / CdTe /Si/ Al) with thick ness of (1000) nm with CdTe thin films at RT.
Iodine-doped polythiophene thin films are prepared by aerosol assisted plasma jet polymerization at atmospheric pressure and room temperature. The doping of iodine was carried out in situ by employing iodine crystals in thiophene monomer by weight mixing ratios of 1%, 3%, 5% and 7%. The chemical composition analyses of pure and iodine-doped and heat-treated polythiophene thin films are carried out by FTIR spectroscopy studies. The optical band gaps of the films are evaluated from absorption spectrum studies. Direct transition energy gaps are determined from Tauc plots. The structural changes of polythiophene upon doping and the reduction of optical band gap are explained on the basis of the results obtained from FTIR spectroscopy, UV–V
... Show MoreSlow cinema is a modern phenomenon conceptually. It is one of the most important contemporary features of the development of film art. Despite its roots extending back to previous cinematic schools, it is unique in its distinctive intellectual and visualaudio structures that tend towards slowness, simplicity, monotony, and calm in shaping the cinematic material it presents to the recipient, prompting them to contemplate and reflect on it, rather than receiving it passively. Thus, slow cinema becomes a revolutionary trend linked to philosophical structures broader than the world of film, attempting to resist the ideology of speed that dominates our contemporary lives. Based on this importance of slow cinema, the researcher definedthe topic o
... Show MoreChalcopyrite thin films were one-step potentiostatically deposited onto stainless steel plates from aqueous solution containing CuSO4, In2(SO4)3 and Na2S2O3.The ratio of (In3+:Cu2+) which involved in the solution and The effect of cathodic potentials on the structural had been studied. X-ray diffraction (XRD) patterns for deposited films showed that the suitable ratio of (In3+:Cu2+) =6:1, and suitable voltage is -0.90 V versus (Ag/AgCl) reference electrode
The spectroscopic properties, potential energy curve, dipole moments, total charge density, Electrostatic potential as well as the thermodynamic properties of selenium diatomic halides have been studied using code Mopac.7.21 and hyperchem, semi-empirical molecular orbital of MNDO-method (modified neglected of differential overlap) of parameterization PM3 involving quantum mechanical semi-empirical Hamiltonian. The relevant molecular parameters like interatomic distance, bond angle, dihedral angle and net charge were also calculated.
Steel fiber aluminum matrix composites were prepared by atomization technique. Different air atomization conditions were considered; which were atomization pressure and distance between sample and nozzle. Tensile stress properties were studied. XRF and XRD techniques were used to study the primary compositions and the structure of the raw materials and the atomized products. The tensile results showed that the best reported tensile strength observed for an atomization pressure equal to 4 mbar and sample to nozzle distance equal to 12 cm. Young modulus results showed that the best result occurred with an air atomization pressure equal to 8 mbar and sample to nozzle distance equal to 16cm