The limitations of conventional cement mortar as a widely used construction material include low tensile capacity, high permeability, and susceptibility to chemical degradation. The increasing demand for durable and sustainable construction materials has led to increased attention in modifying cementitious materials through nanotechnology. This study investigates the influence of nano-silica (NS) and nano-alumina (NA) on the physical, strength-related, and durability characteristics of cement mortar to determine the optimum nanomaterial type and dosage for performance enhancement. Six mortar mixes, in addition to a reference mix, were designed and prepared by adding 1%, 1.5%, and 2% of the cement weight with NS and NA separately, and were evaluated for flowability, setting time, density, porosity, sorptivity, compressive and flexural strength, rapid chloride penetration, acid resistance, and energy-dispersive X-ray spectroscopy analysis. Both NS and NA slightly reduced flowability but enhanced strength and durability. Incorporation of 1.5% NS yielded the highest 28-day compressive strength (95 MPa), around 12% higher than the control mix, whereas 1% NA resulted in the greatest early-age strength gain. Both nanomaterials enhanced matrix densification, leading to reductions in porosity (up to 22%) and chloride permeability (up to 44%) for NS. In summary, these findings demonstrate that NS outperforms NA in terms of reactivity and durability. Optimal dosages were identified as 1.5% for NS and 1% for NA, providing the best balance of workability, mechanical enhancement, and durability improvements. These results highlight the effectiveness of nanomaterial incorporation as a promising approach to developing high-performance, durable cement mortars suitable for advanced infrastructure applications.
The bauxite produced from Al-Ga 'ara area in Al-Enbar containing 50.4 wt. percentages Al2O3 was used for a- alumina production.
For α-alumina pro
... Show MoreThe reinforced fiberglass in cement slurry reflects the effect on its properties compared to usual additives. Fiberglass is typically used in cement slurry design for one or another of the following goals: (Earth earthquake, bearing storage, and with differential stresses, to enhance cement durability and increase its compressive strength). The main goal is to use glass fiber and ground fiberglass to improve the tensile strength and moderate compressive strength significantly. On the other hand, the use of glass fibers led to a slight increase in the value of thickening time, which is a desirable effect. Eleven glass fiber samples and milled glass fiber were used to show these materials' effect on Iraqi cement with (0.125, 0.25, 0.5
... Show MoreAmong all the common mechanical transmission elements, gears still playing the most dominant role especially in the heavy duty works offering extraordinary performance under extreme conditions and that the cause behind the extensive researches concentrating on the enhancement of its durability to do its job as well as possible. Contact stress distribution within the teeth domain is considered as one of the most effective parameters characterizing gear life, performance, efficiency, and application so that it has been well sought for formal gear profiles and paid a lot of attention for moderate tooth shapes. The aim of this work is to investigate the effect of pressure angle, speed ratio, and correction factor on the maxi
... Show MoreAbstract:In this research we prepared nanofibers by electrospinning from poly (Vinyl Alcohol) / TiO2. The spectrum of the solution (Emission) was studied at 772 nm. Several process parameter were Investigated as concentration of PVA, the effect of distance from nozzle tip to the grounded collector (gap distance), and final the effect of high voltage. We find the optimum condition to prepare a narrow nanofibers is at concentration of PVA 16gm, the fiber has 20nm diameter.
Nanostructured Al2O3has been applied as a protective coating against corrosion of the carbon steel (C.S) in seawater environment (3.5% NaCl) at temperatures range (298-328)K. Aluminananoparticles were deposited on carbon steel substrates by cathodic electrophoretic deposition (EPD) with ethanol as suspension medium and poly(acrylic acid) (PAA) as polymeric charging agent. Meanwhile, thesurface morphology was examined using Atomic-force microscopy (AFM). The cross-section AFM showed that the particles sizes for the Al2O3 NPs is around 60-80 nm. The anticorrosion behaviour of coated C.S was investigated in 3.5% NaCl at temperature range 298-328 K by potentiodynamic polarization measurements. Results show that using PAA in suspension coat incr
... Show MoreIn this research, geopolymer mortar had to be designed with 50% to 50% slag and fly ash with and without 1% micro steel fiber at curing temperature of 240℃. The molarity of alkaline solution adjusted with 12 molar sodium hydroxid to sodium silicate was 2 to 1, reaspectivly. The heat of curing increased the geopolymerization proceses of geoplymer mortar, which led to increasing strength, giving the best result and early curing age. The heat was applied for two days by four hours each day. It was discovered in the impact test that the value first crack of each mix was somewhat similar, but the failure increased 72% for the mixture that did not contain fiber. For the energy observation results it was shown that the mixt
... Show MoreThe research was carried out in lathhouse on one-year-old apple seedlings of the Ibrahimi variety in the Karma-Fallujah region for the 2021 growing season to study the effect of methods of adding nano-fertilizer and humic acid on seedling growth. A two-factor experiment was designed according to a randomized complete block design, with three replicates and two seedlings per experimental unit, so the number of seedlings was 54. The first factor includes NPK nanofertilizer at three levels (0- and 2-ml L-1 foliar spray and 5 ml L-1 soil application). The second factor is humic acid at three levels (0 and 5 g of seedlings - 1 foliar spray and 10 g of seedlings - 1 soil application). The results of the study show that the NPK nano-fertil
... Show More