One of the Iraqi geotechnical problems is the presence of gypseous soils covering about (27-36) percentage of Iraq soils containing gypsum between (10-70) ratios. The main reason for soil problematic is the gypsum dissolution when these soils are inundated. However, the soluble gypsum can be leached out of the soil particles, so these problems can be led to cracking, tilting, and collapsing the related soil structure and changing the soil properties. The aim of this work is to investigate the performance of under-reamed piles as a new, improved method to reduce the moisture sensitive and the primary triggering mechanism for the volume reduction of collapsible soil, which is considered as a non-elastic deformation; this was done by carrying series of inundation these soil with using different types of under reamed piles to arrive the best and suitable type useful in gypseous soils. The piles with reams are concrete piles with one or more ream, so under-reamed piles are suitable in weak soils where sizable ground movement, variations, filed up ground, silty clay, and loose sand which has the advantage to increase the soil strength. This paper includes the experimental model of under-reamed piles under static load simulated by a steel plate on the pile cap, then the load-settlement curve, friction force, and bearing force founded from the investigation of different patterns of reamed. It was found that a number of bulbs had a significant reduction on settlement reach to 93% in case of using triple under-reamed pile which is the greatest results in comparison with other patterns and reference pile of the uniform cross-section in the wet state.
A field experiment was conducted during the spring season 2020 in Karbala proving/ Al-Sharia Distrit, located at latitude N 32° 42' 13.8" and longitude E 43° 54' 36.6" and at an altitude of 27 m above sea level. The experiment included a study of two factors: the first, Irrigation Interval, three treatments were used: irrigation treatment every 2 days, Irrigation treatment every 4 days, and Irrigation treatment every 6 days. The second factor is the addition of soil conditioners, in which four treatments were used: the control treatment without any addition, the treatment of adding bio-organic fertilizers, the treatment of adding water-conserving technology (polymer), and the treatment of adding water-conserving technology + fertilizers O
... Show MoreSustainable vegetative management plays a significant role in improving soil quality in degraded agricultural landscapes by enhancing soil microbial biomass. This study investigated the effects of grass buffers (GBs), biomass crops (BCs), grass waterways (GWWs), and agroforestry buffers (ABs) on soil microbial biomass and soil organic C (SOC) compared with continuous corn (
Isolated Bacteria from the roots of barley were studied; two stages of processes Isolated and screening were applied in order to find the best bacteria to remove kerosene from soil. The active bacteria are isolated for kerosene degradation process. It has been found that Klebsiella pneumoniae sp. have the highest kerosene degradation which is 88.5%. The optimum conditions of kerosene degradation by Klebsiella pneumonia sp. are pH5, 48hr incubation period, 35°C temperature and 10000ppm the best kerosene concentration. The results 10000ppm showed that the maximum kerosene degradation can reach 99.58% after 48 h of incubation. Higher Kerosene degradation which was 99.83% was obtained at pH5. Kerosene degradation was found to be maximum at 3
... Show MoreIsolated Bacteria from the roots of barley were studied; two stages of processes Isolated and screening were applied in order to nd the best bacteria to remove kerosene from soil. The acve bacteria are isolated for kerosene degradaon process. It has been found that Klebsiella pneumoniae sp. have the highest kerosene degradaon which is 88.5%. The opmum condions of kerosene degradaon by Klebsiella pneumonia sp. are pH5, 48hr incubaon period, 35°C temperature and 10000ppm the best kerosene concentraon. The results 10000ppm showed that the maximum kerosene degradaon can reach 99.58% aer 48 h of incubaon. Higher Kerosene degradaon which was 99.83% was obtained at pH5. Kerosene degradaon was found
... Show MoreRecently, wireless communication environments with high speeds and low complexity have become increasingly essential. Free-space optics (FSO) has emerged as a promising solution for providing direct connections between devices in such high-spectrum wireless setups. However, FSO communications are susceptible to weather-induced signal fluctuations, leading to fading and signal weakness at the receiver. To mitigate the effects of these challenges, several mathematical models have been proposed to describe the transition from weak to strong atmospheric turbulence, including Rayleigh, lognormal, Málaga, Nakagami-m, K-distribution, Weibull, Negative-Exponential, Inverse-Gaussian, G-G, and Fisher-Snedecor F distributions. This paper extensive
... Show MoreThis research concerns study the crack growth in the wall of pipes made of low carbon steel under the impact load and using the effect of hygrothermal (rate of moisture 50% and 50℃ temperature). The environmental conditions were controlled using high accuracy digital control with sensors. The pipe have a crack already. The test was performed and on two type of specimens, one have length of 100cm and other have length 50cm. The results were, when the humidity was applied to the pipe, the crack would enhance to growth (i.e. the number of cycles needed to growth the crack will reduce). In addition, when the temperature was increase the number of cycles needed to growth the crack are reduced because the effect of heat on the mechanical pro
... Show MoreThis search concerns study the crack growth in the wall of pipes made of low carbon steel under the impact load and using the effect of moisture (rate of moisture 50%). The environmental conditions were controlled using high accuracy digital control with sensors. The pipe has a crack already. The test was performed and on two type of specimens, one has a length of 100cm and other have length 50cm. The results were, when the humidity was applied to the pipe, the crack would enhance to grow (i.e. the number of cycles needed to grow the crack will reduce). In addition, when the test performed on the specimens of length 50cm the number of cycles needed to grow the crack is increased due to the effect of bending stress on the
... Show MoreSolvents are important components in the pharmaceutical and chemical industries, and they are increasingly being used in catalytic reactions. Solvents have a significant influence on the kinetics and thermodynamics of reactions, and they can significantly change product selectivity. Solvents can influence product selectivity, conversion rates, and reaction rates. However, solvents have received a lot of attention in the field of green chemistry. This is due to the large amount of solvent that is frequently used in a process or formulation, particularly during the purification steps. However, neither the solvent nor the active ingredient in a formulation is directly responsible for the reaction product's composition. Because these ch
... Show MoreThe digital camera which contain light unit inside it is useful with low illumination but not for high. For different intensity; the quality of the image will not stay good but it will have dark or low intensity so we can not change the contrast and the intensity in order to increase the losses information in the bright and the dark regions. . In this search we study the regular illumination on the images using the tungsten light by changing the intensities. The result appears that the tungsten light gives nearly far intensity for the three color bands(RGB) and the illuminated band(L).the result depend on the statistical properties which represented by the voltage ,power and intensities and the effect of this parameter on the digital
... Show MoreCarbon fibre reinforced polymers are widely used to strengthen steel structural elements. These structural elements are normally subjected to static, dynamic and fatigue loadings during their life-time. A number of studies have focused on the characteristics of CFRP sheets bonded to steel members under static, dynamic and fatigue loadings. However, there is a gap in understanding the bonding behaviour between CFRP laminates and steel members under impact loading. This paper shows the effect of different load rates from quasi-static to 300 × 103 mm/min on this bond. Two types of CFRP laminate, CFK 150/2000 and CFK 200/2000, were used to strengthen steel joints using Araldite 420 epoxy. The results show a significant bond strength enhancemen