Characterization and Testing the properties of PEKK- Strontium- hydroxyapatite composite material
...Show More Authors

Polymers, being one of the most important materials in dentistry, offer great physical and mechanical qualities, as well as good biocompatibility. Aim of this study was done to evaluate the Polyetherketoneketone and Polyetherketoneketone polymer composite material used as dental implant through tensile strength, Fourier Transform Infrared analysis FTIR, and wettability). Polyetherketoneketone composites (Polyetherketoneketone and Strontium-containing hydroxyapatite) with selected weight percentage ratios of (0, 10%, 20%, 30%), were fabricated using a compression molding technique”, The study involved Samples preparation (sheets) shaped and form into the desired shape according to standard for tests which included tensile strength, Fourier Transform Infrared analysis FTIR, and wettability. The results obtained from the experiments showed slight increase in tensile strength of the polymer composite consisting from polyetherketoneketone and strontium hydroxaptatite nanofiller compared with pure Polyetherketoneketone, with increase the in concentration of Polyetherketoneketone composite (concentration 10%, 20%, 30%), improvement in the wettability value, with no effect in the chemical structure of Polyetherketoneketone composite comparing with the PEKK composite.

Scopus Crossref
View Publication
Publication Date
Sun Mar 04 2018
Journal Name
Iraqi Journal Of Science
Assessment of ISNAG fluorimeter (Total fluorescence measurements at+ 90° & - 90° using four solar cell on each side for 100mm distance at 2mm path length) with well-known fluorescent molecules via CFIA
...Show More Authors

Two well-known fluorescent molecules: fluorescein sodium salt (FSS) and 2,7-dichloro fluorescein (DCF) were tried to prove the efficiency, trustability and repeatability of ISNAG fluorimeter by using discrete and continuous flow injection analysis modes.A linear range of 0.002-1 mmol/L for FSS and 0.003-0.7 mmol/L was for DCF, with LOD 0.0018 mmol/L and 0.002 mmol/L for FSS and DCF respectively, were obtained for discrete mode of analysis. While the continuous mode gave a linear range of 0.002-0.7 mmol/L and 0.003-0.5 mmol/L for FSS and DCF respectively, the LOD were 0.0016mmol/L and 0.0018 mmol/L for FSS and DCF respectively. The results were compared with classical method at variable λex for both fluorescent molecules at 95

... Show More
View Publication Preview PDF
Publication Date
Wed Feb 12 2025
Journal Name
Journal Of Baghdad College Of Dentistry
Shear bond strength of stainless steel brackets bonded to porcelain surface treated with 1.23% acidulated phosphate fluoride gel compared to hydro fluoric acid with silane coupling agent (In vitro comparative study)
...Show More Authors

Background: With the increasing demands for adult orthodontics, a growing need arises to bond attachments to porcelain surfaces. Optimal adhesion to porcelain surface should allow orthodontic treatment without bond failure but not jeopardize porcelain integrity after debonding.The present study was carried out to compare the shear bond strength of metal bracket bonded to porcelain surface prepared by two mechanical treatments and by using different etching systems (Hydrofluoric acid 9% and acidulated phosphate fluoride 1.23%). Materials and Methods: The samples were comprised of 60 models (28mm *15mm*28mm) of metal fused to porcelain (feldspathic porcelain). They were divided as the following: group I (control): the porcelain surface left u

... Show More
View Publication Preview PDF