Preferred Language
Articles
/
eYaLsoYBIXToZYALDrGr
Producing Sustainable Concrete using Nano Recycled Glass
...Show More Authors
Background:

Many tools and techniques have been recently adopted to develop construction materials that are less harmful and friendlier to the environment. New products can be achieved through the recycling of waste material. Thus, this study aims to use recycled glass bottles as sustainable materials.

Objective:

Our challenge is to use nano glass powder by the addition or replacement of the weight of the cement for producing concrete with enhanced strength.

Methods:

A nano recycled glass powder is prepared by crushing and storming a glass bottle to obtain a Blaine surface area of approximately 28 m2/g and conforming to the chemical requirements for natural pozzolana class N, according to ASTM C618. The outcome of using nano recycled glass for theaddition and replacement of ordinary Portland cement weight on the compressive and flexural strengths of concrete at 7, 28, and 90 days is investigated.

Results:

The concrete mixes with 2.5%, 5%, 7.5%, and 10% replacements of cement by nano recycled glass powder show improvements in compressive and flexural strengths of up to 12.77% and 7.66%, respectively, at 28 days. Meanwhile, mixes with the addition of 5% nano glass powder show best improvements in compressive and flexural strengths of up to 11.49% and 7.46%, respectively.

Scopus Crossref
Publication Date
Wed Mar 15 2023
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of a novel coating material on the microleakage of glass hybrid restoration in primary teeth – An in vitro study
...Show More Authors

Background: Glass ionomer restorations are widely employed in the field of pediatric dentistry. There is a constant demand for a durable restoration that remains functional until exfoliation. This study aimed to measure and compare the effect of a novel coating material (EQUIA Forte Coat) on the microleakage of glass hybrid restoration (EQUIA Forte HT) in primary teeth. Material and method: Thirty cavitated (class-II) primary molars were allocated randomly into two groups based on the coat application; uncoated (control) and coated group (experimental). Cavities were prepared by the use of a ceramic bur (CeraBur) and restored with EQUIA Forte HT with or without applying a protective coat (EQUIA Forte Coat). Samples went through the

... Show More
Crossref (1)
Crossref
Publication Date
Tue Aug 15 2023
Journal Name
Sumer 1
The effect of silver diamine fluoride on the microleakage of glass ionomer restoration in primary teeth at different time intervals
...Show More Authors

Silver diamine fluoride (SDF) has shown effectiveness in hardening tooth structure and killing bacteria. Therefore, it can be used to prevent and arrest dental caries. Riva Star (SDF) treatment alone will stop cavities but will not reverse the cavitation. The Silver Modified Atraumatic Procedure, often known as Smart, is the optimum technique for regaining the tooth's structure and function. Glass ionomer was introduced in (1972) as a new material that has become one of the most widely used materials in restorative dentistry. By releasing fluoride ions, this material has a therapeutic impact on the surrounding tooth structure. Microleakage is the ingress of bacteria, its byproducts, toxins, chemicals, oral fluids, and ions between t

... Show More
View Publication
Scopus (5)
Crossref (2)
Scopus Crossref
Publication Date
Sun Jan 13 2019
Journal Name
Iraqi Journal Of Physics
A Study of the effect of adding antimony oxide to the coating surfaces of steel and cast Iron by glass
...Show More Authors

The study included adding antimony oxide to mixtures of coating metal surfaces (Enameling), after it was selected ceramic materials used in the coating metal pieces of the type of steel and cast iron in two layers. The first is called a ground coat and the second is a cover coat.
Ceramic materials layer for ground coat have been melted down in
platinum crucible at a temperature of 1200oC to prepare the glass
mixture (Frit). It was coated on metals at a temperature of 780oC for
two minutes, while the second layer was prepared glass mixture
(Frit) at a temperature of 1200oC, but was coated at a temperature of
760oC for two minutes.
Underwent tests crystalline state of powders (Frits) and enameled samples using X-ray di

... Show More
View Publication Preview PDF
Crossref
Publication Date
Sun Apr 30 2017
Journal Name
Journal Of Engineering
Study the effect of microbial factor on the qualities and characteristics of Novolak composite material, reinforced glass fibers / Asbestos fibers.
...Show More Authors

The study was reflection of the impact of the widespread use of polymer Novolak composite reinforced  Glass fiber and Asbestos fiber once again with weight fraction 60% on the physical properties, which included (Hardness, Compressive deformation, compressive modulus of elasticity, Flexural modulus of elasticity, Resilience modulus, the maximum of Flexural strength, Flexural strain energy and Shear strength inner layers); it is known how much important the media as a source of bacterial contamination, which contributes directly or indirectly in the process of aging of these materials. These Novolak composite reinforced,  prepared by weight fraction of (10%) and (14%) of the Hexamethylene-tetraamine (HMTA) hardener material. It

... Show More
View Publication Preview PDF
Publication Date
Sat Feb 27 2021
Journal Name
Journal Of Engineering
Assessing the Marshall Properties of Porous Asphalt Concrete
...Show More Authors

Porous asphalt paving is a modern design method that differs from the usual asphalt pavements' traditional designs. The difference is that the design structure of porous pavements allows the free passage of fluids through their layers, which controls or reduces the amount of runoff or water accumulated in the area by allowing the flow of rain and surface runoff.  The cross-structure of this type of paving works as a suitable method for managing rainwater and representing groundwater recharge. The overall benefits of porous asphalt pavements include environmental services and safety features, including controlling the build-up of contaminated metals on the road surface, rainwater management, resistance to slipping ac

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Sat Oct 31 2020
Journal Name
International Journal Of Integrated Engineering
Behavior of High Strength Hybrid Reinforcement Concrete Beams
...Show More Authors

Six proposed simply supported high strength-steel fiber reinforced concrete (HS-SFRC) beams reinforced with FRP (fiber reinforced polymer) rebars were numerically tested by finite element method using ABAQUS software to investigate their behavior under the flexural failure. The beams were divided into two groups depending on their cross sectional shape. Group A consisted of four trapezoidal beams with dimensions of (height 200 mm, top width 250 mm, and bottom width 125 mm), while group B consisted of two rectangular beams with dimensions of (125 ×200) mm. All specimens have same total length of 1500 mm, and they were also considered to be made of same high strength concrete designed material with 1% volume fraction of steel fiber.

... Show More
View Publication
Scopus (4)
Crossref (2)
Scopus Clarivate Crossref
Publication Date
Sun Jan 01 2012
Journal Name
7th Rilem International Conference On Cracking In Pavements
Mechanistic Evaluation of Lime-Modified Asphalt Concrete Mixtures
...Show More Authors

Frequently, Load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some sections poorly drained are the main failure types found in some of the newly constructed road within Baghdad as well as other cities in Iraq. The use of hydrated lime in pavement construction could be one of the possible steps taken in the direction of improving pavement performance and meeting the required standards. In this study, the mechanistic properties of asphalt concrete mixes modified with hydrated lime as a partial replacement of limestone dust mineral filler were evaluated. Seven replacement rates were used; 0, 0.5, 1, 1.5, 2, 2.5 and 3 percent by weight of aggregate. Asphalt concrete mixes were prepared at their

... Show More
View Publication
Crossref (9)
Crossref
Publication Date
Thu Dec 03 2020
Journal Name
Civileng
Evaluation of Concrete Material Properties at Early Age
...Show More Authors

This article investigates the development of the following material properties of concrete with time: compressive strength, tensile strength, modulus of elasticity, and fracture energy. These properties were determined at seven different hydration ages (18 h, 30 h, 48 h, 72 h, 7 days, 14 days, 28 days) for four pure cement concrete mixes totaling 336 specimens tested throughout the study. Experimental data obtained were used to assess the relationship of the above properties with the concrete compressive strength and how these relationships are affected with age. Further, this study investigates prediction models available in literature and recommendations are made for models that are found suitable for application to early age conc

... Show More
View Publication
Crossref (19)
Crossref
Publication Date
Sat Apr 08 2000
Journal Name
Dirasat Journal [natural And Engineering Sciences Division]
Tension Stiffening in Partially Prestressed Concrete Flexural Members
...Show More Authors

Publication Date
Thu Dec 01 2011
Journal Name
Journal Of Engineering
MECHANISTIC EVALUATION OF LIME-MODIFIED ASPHALT CONCRETE MIXTURES
...Show More Authors

Frequently, Load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some sections poorly drained are the main failure types found in some of the newly constructed road within Baghdad as well as other cities in Iraq. The use of hydrated lime in pavement construction could be one of the possible steps taken in the direction of improving pavement performance and meeting the required standards. In this study, the mechanistic properties of asphalt concrete mixes modified with hydrated lime as a partial replacement of limestone dust mineral filler were evaluated. Seven replacement rates were used; 0,0.5, 1, 1.5, 2, 2.5 and 3 percent by weight of aggregate. Asphalt concrete mixes were prepared at their

... Show More
View Publication Preview PDF
Crossref