Back ground: Glass ionomer materials lack resistance to wear and pressure and are susceptible to moisture during the initial stages of setting and dehydration. So this study was done to assess diametral tensile strength and microhardness of glass ionomer reinforced by different amounts of hydroxyapatite. Materials and methods: In this study a hydroxyapatite material was added to glass monomer cement at different ratios: 10%, 15%, 20%, 25% and 30% (by weight). The diametral tensile strength test described by the British standard specification for zinc polycarboxylate cement was used in this study and the microhardness test was performed using Vickers microhardness testing machine and the microhardness values were calculated and statistical comparison was performed on the tested groups. Results: The group of glass ionomer cement that contains 20% hydroxyapatite has higher diametral tensile strength and microhardness values than other groups of this study. Also the results showed that the group of glass ionomer cement without hydroxyapatite has the lowest values of diametral tensile strength and microhardness than other groups. The groups of glass ionomer cement with 10%, 15%, 25% and 30% hydroxyapatites also showed increasing in diametral tensile strength and microhardness values in comparison with group of glass ionomer cement without hydroxyapatite. Conclusion: The addition of hydroxyapatite to conventional glass ionomer cement will increase its diametral tensile strength and microhardness
Methods: 112 placentae samples were investigated during the period from August 2007 to August 2008 under light microscopefor mother aged 15 - 45 years old.Results: It was found that normal placental shapes had no correlation to mother age, while abnormal shapes were found more inyoung age groups. The better placental measured parameters were found in mother age 20-24 years. The percentages ofabnormal umbilical cord insertion were very high compared to other studies. Babies’ gender had a correlation with theplacental thickness; male babies have thicker placentae than females. Male babies have longer umbilical cords with widerdiameter than females. Light microscope picture showed the chorionic villi with isolated fetal blood vessel were hig
... Show MoreBackground: The ideal maxillofacial prosthesis should have fine and thin boundaries that bindwith the surrounding facial structures and possess high tear strength.This study aims to determinethe best percentages of nanofiller (TiO2) and intrinsic pigment (silicone functional intrinsic) thatcould be mixed in as additives to improve the tear strength of Cosmesil M511 andVST50F siliconeelastomers with the least effect on their hardness.Materials and Methods: In this in vitro experimental study, a total of 80 samples, 40 for eachelastomer, were fabricated. Each elastomer sample was split into two equal groups to test for tearstrength and Shore A hardness. Each group consisted of 20 samples, including 10 control sampleswithout additives and 10 e
... Show MoreAutorías: Ghassan Adeeb Abdulhasan, Talib Faisal Shnawa, Yasir Wajih Qaddoori. Localización: Revista iberoamericana de psicología del ejercicio y el deporte. Nº. 6, 2022. Artículo de Revista en Dialnet.
The present work aimed to study the effect of Grave's disease on the different tissues and organs of the body by using Wayne Thyrotoxicosis Diagnostic Index (WTDI) and Basel Metabolic Index (BMI). To reach such aim, (35) patients were involved (25 females and 10 males). A control group of (15) healthy individuals (10 females and 5 males) was selected for comparison , as well as , the following: 1- Wayne Thyrotoxicosis Diagnostic Index (WTDI) applied on patient group and control group under the supervision of specialist medical team , this index include (19) sign and symptom , the appearance of one of them may be lead to the others. The sings and symptoms of the index appear only on the patients. There is no Significant di
... Show MoreBackground: Heat-cured poly (methyl methacrylate) the principal material for the fabrication of denture base have a relatively poor mechanical properties. The aim of this study was to investigate the effect of glass flakes used as reinforcement on the surface hardness and surface roughness of the heat-processed acrylic resin material. Material and method: Glass flakes (product code: GF002) pretreated with silane coupling agent were added to Triplex® denture base powder using different concentrations. A total of 100 specimens of similar dimensions (65 x 10 x 2.5) mm were prepared, subdivided into 2 main groups of 50 specimens for each of the study tests. Ten specimens for the control group and 40 specimens for each of the experimental gro
... Show MoreThe shear strength of soil is one of the most important soil properties that should be identified before any foundation design. The presence of gypseous soil exacerbates foundation problems. In this research, an approach to forecasting shear strength parameters of gypseous soils based on basic soil properties was created using Artificial Neural Networks. Two models were built to forecast the cohesion and the angle of internal friction. Nine basic soil properties were used as inputs to both models for they were considered to have the most significant impact on soil shear strength, namely: depth, gypsum content, passing sieve no.200, liquid limit, plastic limit, plasticity index, water content, dry unit weight, and initial
... Show MoreOne of the most important problems that faces the concrete industry in Iraq is the deterioration due to internal sulfate attack , since it reduces the compressive strength and increases the expansion of concrete. Consequently, the concrete structure may be damage .The effects of total and total effective sulfate contents on high strength concrete (HSC) have been studied in the present study.
The research studied the effect of sulfate content in cement , sand and gravel , as well as comparing the total sulfate content with the total effective SO3 content. Materials used were divided into two groups of SO3 in cement ,three groups of SO3 in sand ,and two groups of SO
... Show MoreThe present investigation considers the effect of curing temperatures (30, 40, and 50˚C) and curing compound method on compressive strength development of high performance concrete, and compares the results with concrete cured at standard conditions and curing temperature (21˚C). The experimental results showed that at early ages, the rate of strength development at high curing temperature is greater than at lower curing temperature, the maximum increasing percentage in compressive strength is 10.83% at 50C˚ compared with 21C˚ in 7days curing age. However, at later ages, the strength achieved at higher curing temperature has been less, and the maximum percentage of reduction has been 5.70% at curing temperature 50C˚ compared with 21
... Show More