Back ground: Glass ionomer materials lack resistance to wear and pressure and are susceptible to moisture during the initial stages of setting and dehydration. So this study was done to assess diametral tensile strength and microhardness of glass ionomer reinforced by different amounts of hydroxyapatite. Materials and methods: In this study a hydroxyapatite material was added to glass monomer cement at different ratios: 10%, 15%, 20%, 25% and 30% (by weight). The diametral tensile strength test described by the British standard specification for zinc polycarboxylate cement was used in this study and the microhardness test was performed using Vickers microhardness testing machine and the microhardness values were calculated and statistical comparison was performed on the tested groups. Results: The group of glass ionomer cement that contains 20% hydroxyapatite has higher diametral tensile strength and microhardness values than other groups of this study. Also the results showed that the group of glass ionomer cement without hydroxyapatite has the lowest values of diametral tensile strength and microhardness than other groups. The groups of glass ionomer cement with 10%, 15%, 25% and 30% hydroxyapatites also showed increasing in diametral tensile strength and microhardness values in comparison with group of glass ionomer cement without hydroxyapatite. Conclusion: The addition of hydroxyapatite to conventional glass ionomer cement will increase its diametral tensile strength and microhardness
Background: the aim of this study was to evaluate the effect of different surface acids treatments (37%phospjoric acid, 5%hydrofluoric acid, 1.23 acidulated phosphate fluoride) of feldspathic ceramic VITA 3D MASTER , and the effect of thermocycling on shear bond strength using a ceramic repair kit (ivoclar/vivadent). Material and Methods: sixty Nickel-Chromium metal base plates were prepared(9mm diameter,3mm depth) using lost wax technique, 2mm thick layer of ceramic(VITA 3D MASTER) fused to metal plates, all specimens were embedded in acrylic resin blocks except their examined surfaces and divided into 3 main groups 20 specimens each, Grp A: treatment with 37%phosphoric acid for 2 mins, Grp B: etching with 5% hydrofluoric acid for 2mins,
... Show MoreObjective: Evaluate the effects of different storage periods on flexural strength (FS) and degree of conversion (DC) of Bis-Acryl composite and Urethane dimethacrylate provisional restorative materials. Material and Methods: A total of 60 specimens were prepared from four temporary crown materials commercially available and assigned to four tested groups (n = 15 for each group): Prevision Temp, B&E CROWN, Primma Art, and Charm Temp groups. The specimens were stored in artificial saliva, and the FS was tested after 24 h, 7 d, and 14 d. A standard three-point bending test was conducted using a universal testing machine. Additionally, the DC was determined using a Fourier transform infrared spectroscopy (FTIR) device. The data were analyzed st
... Show MoreThis work characterizes the fractographic features of the neat epoxy and ZrO2 epoxy nanocomposites. All samples were subjected to a tensile test to determine the tensile strength and tensile modulus. SEM images were used to study the morphology of the fractured surface. The fractographic of the fracture surfaces were studied by microstructure analysis program (j-images) to specify the effect of ZrO2 nanoparticles on tensile performance and failure mechanism for ZrO2 epoxy nanocomposites. The tensile test results show that the addition of ZrO2 nanoparticles (2, 4, 6, 8, and 10 vol.%) to the epoxy matrix leads to increase the tensile strength about 40% for optimal content of ZrO2 nanop
... Show MoreBackground and objectives: This study aimed at testing the effect of plastic sleeve or barrier, used to cover the guide of the light cure unit to prevent cross-infection, on the shear bond strength and site of bond failure of stainless steel and ceramic orthodontic brackets. Materials and methods: Forty orthodontic brackets; twenty stainless steel and twenty ceramic brackets bonded to forty extracted human maxillary first premolars using light cure adhesive cured with and without the use of a protective plastic barrier on the guide. Comparing the effect of this barrier on the shear bond strength and adhesive remnant index was performed using an independent t-test and Chi-square test. Results: The protective barrier had decreased the shear b
... Show MoreThe reinforced fiberglass in cement slurry reflects the effect on its properties compared to usual additives. Fiberglass is typically used in cement slurry design for one or another of the following goals: (Earth earthquake, bearing storage, and with differential stresses, to enhance cement durability and increase its compressive strength). The main goal is to use glass fiber and ground fiberglass to improve the tensile strength and moderate compressive strength significantly. On the other hand, the use of glass fibers led to a slight increase in the value of thickening time, which is a desirable effect. Eleven glass fiber samples and milled glass fiber were used to show these materials' effect on Iraqi cement with (0.125, 0.25, 0.5
... Show MoreIn this study the thermal conductivity of the epoxy composites were characterized as function of volume fraction, particle size of fillers and the time of immersion(30,60,90)days in water .Composites plates were prepared by incorporating (bi-directional) (0º-90º) glass fiber and silicon carbide (SiC) particles of (0.1,0.5,1)mm as particle size at (10%,20%,30%,40%) percent volume in epoxy matrix.
The composites shows slightly increase of the thermal conductivity with increasing volume fraction, particle size and increase with increasing the days of immersion in water. The maximum thermal conductivity (0.51W/m.K) was obtained before the immersion in water at 90 days for epoxy reinforcement by bi-directional glass fiber and SiC particl
The In this experimental study, natural stone powder was utilized to improve a cohesive soil’s compaction and strength properties. According to the significant availability of limestone in the globe, it has been chosen for the purpose of the study, in addition to considering the existing rock industry massive waste. Stone powder was used in percentages of 4, 8, 12, 16% replaced from the soil weight in dry state. Some of cohesive soil’s consistency, shear, and compaction properties were depicted after improvement. The outcomes yielded in significant amendments in the experimented geotechnical properties after stone powder addition considering 60 days curing period. Cohesion and friction angle were notably increased by
... Show MoreIn this work, a CW CO2 laser was used for cutting samples of the fiber-reinforced
plastics (FRP) of three different types of reinforcing material; aramide, glass and carbon.
Cutting process was investigated throughout the variation of some parameters of cutting
process and their effects on cutting quality as well as the effect of an inert gas exist in the
interaction region and finally using a mechanical chopper in order to enhance the cutting
quality. Results obtained explained the possibility to perform laser cutting with high
quality in these materials by good control of the parameters and conditions of the process.