Background. Material tribology has widely expanded in scope and depth and is extended from the mechanical field to the biomedical field. The present study aimed to characterize the nanocoating of highly pure (99.9%) niobium (Nb), tantalum (Ta), and vanadium (V) deposited on 316L stainless steel (SS) substrates which considered the most widely used alloys in the manufacturing of SS orthodontic components. To date, the coating of SS orthodontic archwires with Nb, Ta, and V using a plasma sputtering method has never been reported. Nanodeposition was performed using a DC plasma sputtering system with three different sputtering times (1, 2, and 3 hours). Results. Structural and elemental analyses were conducted on the deposited coatings using XRD, FESEM, and EDS showing a unique phase of coating metals over their substrates with obvious homogeneous even deposition. A highly significant positive correlation was found between sputtering time and thickness of the achieved coatings. AFM revealed a reduction in the surface roughness of 316L SS substrates sputtered with all coating materials, significantly seen in V coatings. Conclusions. Sputtering time and coating material play a significant role in terms of microstructure and topography of the achieved coatings being the best in the Ta group; moreover, surface roughness was significantly improved by V coatings. Likewise, it is found to be sputtering time independent for all used coatings.
Roughness length is one of the key variables in micrometeorological studies and environmental studies in regards to describing development of cities and urban environments. By utilizing the three dimensions ultrasonic anemometer installed at Mustansiriyah university, we determined the rate of the height of the rough elements (trees, buildings and bridges) to the surrounding area of the university for a radius of 1 km. After this, we calculated the zero-plane displacement length of eight sections and calculated the length of surface roughness. The results proved that the ranges of the variables above are ZH (9.2-13.8) m, Zd (4.3-8.1) m and Zo (0.24-0.48) m.
Background. “Polyetheretherketone (PEEK)” is a biocompatible, high-strength polymer that is well-suited for use in dental applications due to its unique properties. However, achieving good adhesion between PEEK and hydrophilic materials such as dental adhesives or cement can be challenging. Also, this hydrophobicity may affect the use of PEEK as an implant material. Surface treatment or conditioning is often necessary to improve surface properties. The piranha solution is the treatment of choice to be explored for this purpose. Methods. PEEK disks of 10 mm diameter and 2 mm thickness were used in this study. Those samples were divided into five groups (each group has five samples). The first is the control group, in which no
... Show MoreTitanium alloy (Ti-6Al-4V) samples were nitrided in low pressure (1.3, 3 mbar) dc-glow discharge plasmas of nitrogen. The treating time was 5, 10 and 15 hour and the temperatures range of the samples during the nitriding process was close to 800oC. The obtained microstructures of the nitride layers were studied by x-ray diffraction and optical microscopy. The ε –Ti2N, ζ-Ti3N3-x and η-Ti3N2-x.phases were formed and addition to the solid solution of nitrogen in titanium, α (Ti,N). Micro hardness measurements exhibit an increment for the Ti-alloy specimens which nitrided at 800oC for 10 and 15h.Corrosion measurements were obtained for the Ti-6Al-4V alloy in Ringer solution after plasma nitriding. The clear improving in the corrosion r
... Show MoreBackground: To evaluate the ISO depth of cure of bulkfill composites and depth of cure which determined by Vickers microhardness test. Materials and Methods: Bulkfill resin composite specimens (n=150) were prepared of three bulkfill composite materials (TetricEvo Ceram, Quixfil and SDR) and light cured by Flash max p3 for 3, 10, 20 seconds and by wood pecker for 10, 20 seconds respectively, a mold was filled with one of the three bulkfill composites and light cured. The specimens removed from the mold and scraped by plastic spatula and the remaining length (absolute length) was measured which represent the ISO depth of cure. After that the specimens were returned into the mold and a microhardness indentation device applied on the specimen
... Show MoreBackground: The aim of the study was to investigate the effect of surface treatments of zirconia (grinding and sandblast with 50μm, 100 μm) on shear bond strength between zirconia core and veneering ceramic. Material and methods: Twenty-eight presintered Y-TZP ceramic specimens (IPS e.max ZirCAD, Ivoclar vivadent) were fabricated and sintered according to manufacturer’s instructions. The core specimens were divided randomly in to 4 groups, group 1: no surface treatment, group2: zirconia specimens were ground with silicon carbide paper up to1200 grit under water cooling, group3: zirconia specimens were ground and sandblast with 100 μm alumina, group 4: zirconia specimens were ground and sandblast with 50 μm alumina. Surfa
... Show MoreIn this research, a sensor for chemical solutions was designed and formed using optical fiber-based on a surface Plasmon resonance technology. A single-mode optical fiber with three different diameters (25, 45 and 65) µm was used, respectively. The second layer of the low refractive fiber was replaced by gold, which was electrically deposited at 40 µm thickness. For each of the three types of optical fiber, different saline concentrations (different index of refraction) were used to evaluate the performance of the refractive index sensor (chemical sensor) by measuring its sensitivity and resolutions. The highest values we could get for these two parameters were 240mm/RIU, and 6*10-5 RIU respectively, when the diameter of a
... Show MoreBackground: This study was conducted to evaluate the surface roughness and dimensional accuracy of commercially obtainable alginate impression material in terms of imbibition after immersion in two different media. Materials and method: Two disinfecting agents, ethanol 70% and povidone-iodine 4%, were used to access the dimensional accuracy and surface roughness of alginate impression material. Weights of specimen discs of alginate impressions were measured before and immediately after immersion to gain a measure of imbibition. For surface roughness, disinfected specimens rectangle was examined before and after disinfection. Results: Minimal changes in weight were observed after disinfection, but a statistically non-significant differenc
... Show MoreBackground: Adjustment of any premature occlusal contact of any zirconia restoration requires its polishing or glazing in order to restore the smoothness of the restoration. The objective of this in vitro study was to evaluate the effects of different polishing systems and glazing on the surface roughness of full-contour zirconia. Material and methods: Forty disks (diameter: 8 mm, thickness: 6.4 mm) were prepared from pre-sintered full-contoured zirconia block; they were colored and sintered in a high-temperature furnace at 1500ËšC for 8 hours. The specimens were then leveled and finished using grinding and polishing machine and adjusted using diamond disk. The specimens were then randomly divided into four groups (n=10), group I involves
... Show MoreIn this work, monitoring of monthly variation (from May 2016 to October 2016) in the concentration of the metals (Co, Zn, Cd, Pb, Ni and Fe) from Al-Diwaniya city of Iraq. Investigation about the pollution with these metals was achieved from five selected sites locate in study area by flame atomic absorption spectroscopy. The results showed a wide variation in the levels of heavy metals from site to site and from month to month. A total of 180 surface soil samples were analyzed to detecting the pollution with selected samples. The resultsshowed that the highest concentration with Ni was 6.290 mg kg-1 while the lowest concentration detected with Ni was 0.080 mg kg-1. The results of pollution index (enrichment factor, contamination factor, po
... Show MoreCarbonized nonwoven nanofibers composite were fabricated using the electrospinning method of a polymeric solution composite followed by heat treatment including stabilization and calcination steps. The spun polymeric solution was a binary polymer mixture/organic solvent. In this study, two types of polymers (Polymethylmethacrylate (PMMA) and Polyethylene glycol (PEG)) were used separately as a copolymer with the base polymer (Polyacrylonitrile (PAN)) to prepare a binary polymer mixture in a mixing ratio of 50:50. The prepared precursor solutions were used to prepare the precursor nanofibers composite (PAN: PMMA) and (PAN: PEG). The fabricated precursors nonwoven fibers composite were stabilized and carbonized to produce carbon nonw
... Show More