Background. Material tribology has widely expanded in scope and depth and is extended from the mechanical field to the biomedical field. The present study aimed to characterize the nanocoating of highly pure (99.9%) niobium (Nb), tantalum (Ta), and vanadium (V) deposited on 316L stainless steel (SS) substrates which considered the most widely used alloys in the manufacturing of SS orthodontic components. To date, the coating of SS orthodontic archwires with Nb, Ta, and V using a plasma sputtering method has never been reported. Nanodeposition was performed using a DC plasma sputtering system with three different sputtering times (1, 2, and 3 hours). Results. Structural and elemental analyses were conducted on the deposited coatings using XRD, FESEM, and EDS showing a unique phase of coating metals over their substrates with obvious homogeneous even deposition. A highly significant positive correlation was found between sputtering time and thickness of the achieved coatings. AFM revealed a reduction in the surface roughness of 316L SS substrates sputtered with all coating materials, significantly seen in V coatings. Conclusions. Sputtering time and coating material play a significant role in terms of microstructure and topography of the achieved coatings being the best in the Ta group; moreover, surface roughness was significantly improved by V coatings. Likewise, it is found to be sputtering time independent for all used coatings.
The optimum conditions for production of fibrinolytic protease from an edible mushroom Pleurotus ostreatus grown on the solid medium , Sus medium, composed of Sus wastes (produced from extracted medicinal plant Glycyrrhiza glabra) were determined. Addition of 5% of Soya bean seeds meal in Sus medium recorded a maximum fibrinolytic protease activity resulting in 7.7 units / ml. The optimum moisture content of Sus medium supplemented with 5% Soya bean seeds meal was 60% resulting in 7.2 units / ml.Pleurotus ostreatus produced a maximum fibrinolytic protease activity when the spawn rate,pH of medium and incubation temperature were 2,6 and 30°C, respectively. The maximum fibrinolytic protease activity was 7.6 units / ml when incubat
... Show MoreBackground: This in vitro study was carried out to evaluate the effect of various endodontic irrigants (sodium hypochlorite, ethylene diaminetetracetic acid and normal saline) on sealing ability of (Biodentine, mineral trioxide aggregate, and amalgam) used to repair furcal perforations. Material and methods: One hundred and twenty extracted human molars with divergent roots were used in this study. A standard root canal access cavity was prepared in each tooth and furcal perforation was made and was standardized by using k file size 100 instrument to get a perforation of (1.32mm) in diameter .The teeth were randomly divided in to three groups of 40 teeth according to the type of material used to repair the perforations (Group A: The furcal
... Show More
Abstract
The aim of the present work is to control of metal buried corrosion by alteration the media method. This method depended on the characteristics of each media. The corrosion rates in different media (soil, sand, porcelanite stone and gravel) for specimens of low carbon steel were measured by two methods weight loss method and polarization method, weight loss measured by buried specimens in these medias separately for 90 days. The polarization method includes preparing of specimen and salt solutions have electrical resistivity equivalent electrical resistivity of these media. The corrosion rate of two method results in (soil > sand> porcelainte stone> gravel). The lower corrosion rate happene
... Show MoreSynthesis three organic inhibitors for carbon steel corrosion: 2-(propylthio)-1H-benzo[d]imidazole (PTBI), 2-(allylthio)- 1H-benzo[d]imidazole (ATBI) and 2-(prop-2-ynylthio)-1H-benzo[d]imidazole (YTBI) were prepared from reaction of 2-mercapto benzimidazole with different alkyl halide. The melting point and TLC were used to confirm the purity of the inhibitors as well as using the [FTIR, 1H-NMR and 13C-NMR] for the identify structures. The synthesized inhibitors were examined by potentiostatic polarization measurement as corrosion inhibitors of carbon steel in acidic media [1M H2SO4 ].The polarization measurement results showed that the mixed type inhibitors. In addition, the efficiency of inhibitors (YTBI) were studied at different con
... Show MoreThe driving idea for the present work was to combine the effect of polyvinyl alcohol (PVA) as corrosion inhibitor with the distance between the anodic and cathodic elements of the galvanic cell, beside their area ratio, in scope of synergistic suppression of galvanic corrosion on Cu/Fe model couple, using weight loss method. The performance affecting galvanic corrosion process has been tested for three major factors affect the process:
1. Four PVA inhibitor concentrations were selected to be (0, 1000, 4000 and 7000 ppm) in simulated cooling water.
2. Two cathode: anode area ratios as 1:1 and 2.4:1.
3. Two distances apart cathode – anode as 3 and 7 cm.
Maximum corrosion inhibition achieved was 86% which indicates that increa
A novel demountable shear connector is proposed to link a concrete slab to steel sections in a way that resulting steel-concrete composite floor is demountable, i.e. it can be easily dismantled at the end of its service life. The proposed connectors consist of two parts: the first part is a hollow steel tube with internal threads at its lower end. The second part is a compatible partially threaded bolted stud. After linking the stud to the steel section, the hollow steel tube can be fastened over the threaded stud, which create a complete demountable shear connector. The connector is suitable for use in both composite bridges and buildings, and using cast in-situ slabs, precast solid slabs, or hollow-core precast slabs. A series of push-off
... Show MoreThe traction property is one of the important mechanical properties, especially the rotary parts which are subjected to constant and variable loads There are many methods used to improve this property, and the shoot peening by metal balls is considered the most critical one. the study focuses on this characteristic of steel CK35 used in many engineering applications as the rotating shafts and railway This study shows that the fatigue strength is improved by14% after shoot peening with metal balls. The study includs the rehabilitation of damaged samples as a result of fatigue corrosion. The standard solution adopted was 36% MgCl2 with a 30 days immersion period. These samples has been improved by 6% after it decreased by18% d
... Show MoreEnvironmental sustainability is described as one that avoids the depletion or deterioration of natural resources, while also allowing for the preservation of long-term environmental quality. By practicing environmental sustainability, we may assist to guarantee that the requirements of today’s population are satisfied without risking the capacity of future generations to meet their own needs in the future. Engineers in the field of concrete production are becoming increasingly interested in sustainable development, which includes the utilization of the locally available materials in addition to using the agricultural and industrial waste in construction industry as one of the possib
Shear lag is the phenomenon that occurs when a supported slender member undergoes deformation from lateral loading, causing in-plane non-uniform distribution of stresses that results in reducing the member’s minimum strength capacity. This paper investigates the behaviour of shear distribution in steel I-section and box girders when subjected to both static and impact loadings. Three-dimensional finite element analysis models were prepared in Strand7 and validated against experimental results providing a basis for further comparison research into shear lagging effects. A parametric study was conducted comparing the effects of impact loading through certain specified velocities at the midspan of restrained ends. It provided new ins
... Show MoreBackground: Plaque retention during fixed orthodontic therapy is an important cause of developing enamel demineralization. The purpose of this study was to evaluate the effect of different brackets types on the count of Streptococcus Mutans in orthodontic patients using conventional fluoridated toothpaste. Materials and Methods: Plaque samples were collected from maxillary 1st premolar teeth of twenty right handed patients (using split mouth technique) before bonding, after 48 hrs of bonding using tooth brush only, and after 2 weeks of using fluoridated toothpaste. Stainless steel bracket was bonded on right first premolar while the left one was bonded with sapphire bracket. The calculation of the Streptococcus Mutans count was done usin
... Show More