The thin films of SnO2,SnO2:TiO2 , SnO2:MoO3 , SnO2:WO3 , SnO2:Cr2O3 , and SnO2: Fe2O3 were prepared by pulsed laser deposition technique using (Nd:YAG) laser of λ=1064 nm average frequency (6) Hz and pulse duration (10 ns) under vacuum of 10 -2 mbar)deposited on glass, n-Si single crystals substrate room temperature with thickness of (100±10) nm. The structures of pure SnO2 and ,SnO2:TiO2 , SnO2:MoO3 , SnO2:WO3 , SnO2:Cr2O3 , SnO2:Co3O4 compounds were studied by X–ray diffraction .the results showed that there was red shift accompanied addition of MoO3 and TiO2 while a blue shift accompanied the addition of WoO3 , Cr2O3 , Fe2O3 to tin oxide . The gas sensing measurements of NO2 gas showed that SnO2:TiO2 thin films prepared on n- Si substrate have better sensitivity than thin films from the other binary compounds . Maximum sensitivity (231.4%) was obtained from SnO2:TiO2 thin film prepared on n- Si substrate at operating temperature 373K
In the present study, a powder mixture of elements Ti and Ni was mechanically alloyed in a high energy ball mill. Microstructure of the nanosized amorphous milled product in different stages of milling has been characterized by X- ray diffraction, scanning electron microscopy and differential thermal analysis. We found that time of mechanical alloying is more significant to convert all crystalline structure to the amorphous phase. Nanocrystalline phase was achieved as a result of the mechanical alloying process. The results also indicates that the phase transformation and the grain size occurs in these alloys are controlled by ball milling time
The proton-neutron interacting boson model (IBM-2) has been used to make a schematic study of the Ruthenium ( ) isotopes of mass region around with and . For each isotope of the values of the IBM-2 Hamiltonian parameters, which yield an acceptable results for excitation energies in comparison with those of experimental data, have been determined. Fixed values of the effective charges ( ) and of the proton and neutron g factors ( and ) have been chosen for all isotopes under study. The calculated electric quadrupole moments of state, transitions, the magnetic dipole moments transitions and mixing ratios are in reasonable agreement with the experimental data.
... Show MoreThis article reported the synthesis and characterization of new bent-shape liquid crystals compounds containing pyrimidine as a core unit and a 5H-thiazolo[3,4-b] [1, 3,4] thiadiazols ring with an amid group. This study includes reaction 5,5-diethylpyrim idine-2,4,6(1H,3H,5H)-trione and two moles of chloroacetylchloride in N, N-dimethyl formamide (DMF) and triethylamine (TEA) to product compound [I], then reacted the later compound with two moles of 4-hydroxybenzaldehyde to yield compound [II] then synthesis compound [III] by reaction compound[II] , thiosemicarbazide and mercap toacetic acid with sulfuric acid concentration, then the compound [III] reaction with deferent acid chlorides to product amid compounds [IV-VII]. The comp
... Show MoreA pulsed (TEA-0O2) laser was used to dissociate molecules of silane ethylene (C2I-14) and ammonia (NH3) gases, through collision assisted multiple photon dissociation (MPD) to deposit(SiC i_xNx) thin films, where the X-values are 0, 0.13 and 0.33, on glass substrate at T,----648 K. deposition rate of (0.416-0.833) nm/pulse and thickness of (500-1000)nm .Fourier transform infrared spectrometry (FT-IR) was used to study the nature of the chemical bonds that exist in the films. Results revealed that these films contain complex networks of the atomic (Si, C, and N), other a quantity of atomic hydrogen and chemical bonds such as (Si-N, C-N, C-14 and N-H).Absorbance and Transmittance spectra in the wavelength range (400-1100) nm were used to stud
... Show MorePure cadmium oxide films (CdO) and doped with zinc were prepared at different atomic ratios using a pulsed laser deposition technique using an ND-YAG laser from the targets of the pressed powder capsules. X-ray diffraction measurements showed a cubic-shaped of CdO structure. Another phase appeared, especially in high percentages of zinc, corresponding to the hexagonal structure of zinc. The degree of crystallinity, as well as the crystal size, increased with the increase of the zinc ratio for the used targets. The atomic force microscopy measurements showed that increasing the dopant percentage leads to an increase in the size of the nanoparticles, the particle size distribution was irregular and wide, in addition, to increase the surfac
... Show MoreThe neutron, proton, and matter densities of the ground state of the proton-rich 23Al and 27P exotic nuclei were analyzed using the binary cluster model (BCM). Two density parameterizations were used in BCM calculations namely; Gaussian (GS) and harmonic oscillator (HO) parameterizations. According to the calculated results, it found that the BCM gives a good description of the nuclear structure for above proton-rich exotic nuclei. The elastic form factors of the unstable 23Al and 27P exotic nuclei and those of their stable isotopes 27Al and 31P are studied by the plane-wave Born approximation. The main difference between the elastic form factors of unstable nuclei and the
... Show More