Preparing a New Type of Concrete Based on Sulfur-melamine Modifier
...Show More Authors

In this research work, a new type of concrete based on sulfur-melamine modification was introduced, and its various properties were studied. This new type of concrete was prepared based on the sulfur-melamine modification and various ingredients. The new sulfur-melamine modifier was fabricated, and its fabrication was confirmed by IR spectroscopy and TG analysis. The surface morphology resulted from this modifier was studied by SEM and EDS analysis. The components ratios in concrete, chemical and physical characteristics resulted from sulfur-melamine modifier, chemical and corrosion resistance of concrete, stability of concrete against water adsorption, stability of concrete against freezing, physical and mechanical properties and durability, modulus of elasticity, and thermal expansion coefficient of the studied sulfur concrete were investigated. The IR results confirmed the amino functional groups (attached melamine ring) and the formation of polymer sulfur chains. The sulfur-melamine modification thermic mass loss was one step. The mass loss processes of the modifier were endothermic processes. The obtained SEM results revealed that the sulfur-melamine modifier had a more porous structure, without any crystal forms. EDS analysis showed that the nitrogen atoms were accounted for 51.33% of total mass while the carbon was 30.94% of total mass. The stability of sulfur-melamine modifier-based concrete was very high in the various aggressive solutions. The low size of aggregates-based concrete had more density, i.e., 2417 kg\m3. The concrete density was decreased slowly with increase in the size of aggregate. The average deformation of studied concrete was (0.0030-0.0033), confirming that the deformation performance of concrete was better than the traditional concretes. The obtained results also confirmed that value of thermal expansion coefficient for sulfur-melamine modified concrete was 17.2×10-6\˚C.

Scopus Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Fri May 01 2020
Journal Name
Civil Engineering Journal
Post-Fire Behavior of Post-Tensioned Segmental Concrete Beams under Monotonic Static Loading
...Show More Authors

This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,

... Show More
View Publication Preview PDF
Scopus (1)
Crossref (1)
Scopus Clarivate Crossref
Publication Date
Sat Jan 01 2022
Journal Name
Structural Durability & Health Monitoring
Seismic Analysis of Reinforced Concrete Silos under Far-Field and Near-Fault Earthquakes
...Show More Authors

View Publication
Scopus (3)
Crossref (3)
Scopus Crossref
Publication Date
Wed Nov 28 2018
Journal Name
International Journal Of Engineering & Technology
Using Polyurethane Coating of Concrete Pipes with Acid Attack Resistance in Sewer Lines
...Show More Authors

One of the most important challenges facing the designers of the sewerage system is the corrosion of sewers due to the influence of sewerage contaminates which lead to failure of the main lines of sewers. In this study, a reference mix of 1: 1.5: 3 was used and the 4% Flocrete PC200 by weight of cement was added to the same mixing ratio in the second mixture. Twenty-four samples were tested for each mixture, 12 of which were used to compression strength test in ages (7, 14 and 28) day and six samples were submerged after 28 days of wet treatment at (5 and 10) % concentrations of sulfuric acid. The other six samples were painted after 28 days of wet treatment with coating Polyurethane and after 24 hours were flooded with a concentrat

... Show More
View Publication
Crossref
Publication Date
Mon Aug 01 2016
Journal Name
Journal Of Engineering
Structural Behavior of Confined Concrete Filled Aluminum Tubular (CFT) Columns under Concentric Load
...Show More Authors

This paper introduces an experimental study on the behavior of confined concrete filled aluminum tubular (CFT) column to improve strength design, ductility and durability of concrete composite structures under concentrically loaded in compression to failure. To achieve this: seven column specimens with same concrete diameter 100mm and without steel reinforcement have been examined through experimental testing, which are used to study the effects of the thickness of the aluminum tube encased concrete ( thickness : 0mm, 2mm, 3mm, 4mm and 5mm with same length of column 450mm), length of column (thickness 5mm and length of column 700mm) and durability (thickness 5mm and length of column 450mm) on the structural behavior of &

... Show More
View Publication Preview PDF
Publication Date
Mon Mar 01 2010
Journal Name
Journal Of Engineering
Short Term Deflection of Ordinary, Partially Prestressed and CFRP Bars Reinforced Concrete Beams
...Show More Authors

Publication Date
Wed Oct 09 2019
Journal Name
Engineering, Technology & Applied Science Research
Numerical Analysis of Segmental Post Tensioned Concrete Beams Exposed to High Fire Temperature
...Show More Authors

The main objective of this study is to characterize the main factors which may affect the behavior of segmental prestressed concrete beams comprised of multi segments. The 3-D finite element program ABAQUS was utilized. The experimental work was conducted on twelve simply supported segmental prestressed concrete beams divided into three groups depending on the precast segments number. They all had an identical total length of 3150mm, but each had different segment numbers (9, 7, and 5 segments), in other words, different segment lengths. To simulate the genuine fire disasters, nine beams were exposed to high-temperature flame for one hour, the selected temperatures were 300°C (572°F), 500°C (932°F) and 700°C (1292°F) as recomm

... Show More
View Publication Preview PDF
Crossref (6)
Crossref
Publication Date
Thu Jan 01 2015
Journal Name
Journal Of Engineering
Reinforcement of Asphalt Concrete by Polyester Fibers to Improve Flexural Bending Fatigue Resistance
...Show More Authors

Reinforcing asphalt concrete with polyester fibers considered as an active remedy to alleviate the harmful impact of fatigue deterioration. This study covers the investigation of utilizing two shapes of fibers size, 6.35 mm by 3.00 mm and 12.70 mm by 3.00 mm with mutual concentrations equal to 0.25 %, 0.50 % and 0.75 % by weight of mixture. Composition of asphalt mixture consists of different optimum (40-50) asphalt cement content, 12.50 mm nominal aggregate maximum size with limestone dust as a filler. Following the traditional asphalt cement and aggregate tests, three essential test were carried out on mixtures, namely: Marshall test (105 cylindrical specimens), indirect tensile strength test (21 cylindrical specimens)

... Show More
View Publication
Publication Date
Mon Aug 01 2016
Journal Name
Journal Of Engineering
Behavior of Reinforced Concrete Deep Beams Strengthened with Carbon Fiber Reinforced Polymer Strips
...Show More Authors

This research is concerned to investigate the behavior of reinforced concrete (RC) deep beams strengthened with carbon fiber reinforced polymer (CFRP) strips. The experimental part of this research is carried out by testing seven RC deep beams having the same dimensions and steel reinforcement which have been divided into two groups according to the strengthening schemes. Group one was consisted of three deep beams strengthened with vertical U-wrapped CFRP strips. While, Group two was consisted of three deep beams strengthened with inclined CFRP strips oriented by 45o with the longitudinal axis of the beam. The remaining beam is kept unstrengthening as a reference beam. For each group, the variable considered

... Show More
View Publication Preview PDF
Publication Date
Wed Jun 01 2016
Journal Name
Journal Of Engineering
Recycling of Reclaimed Asphalt Concrete Using Warm Asphalt Mixture and Emulsified Asphalt Cationic
...Show More Authors

Warm asphalt mixture (WMA) and reclaimed asphalt pavement (RAP) are the most memorable sustainable materials in world of asphalt concrete pavements . This research aims to study the warm asphalt mixture for different types of filler materials such as ordinary cement and limestone dust. Beside, this research focused on the test of emulsified asphalt properties by evaluating the performance of warm asphalt mixture by Marshall Stability properties as well as moisture sensitivity. The results of this experiment provided many important points. First, The cationic emulsified asphalt is suitable with RAP aggregate for production warm asphalt mixtures .Second, The effective mixing procedure for warm asphalt mixtures consists hea

... Show More
View Publication Preview PDF
Publication Date
Wed Jul 04 2018
Journal Name
Civil Engineering Journal
Finite Element Analysis of Concrete Beam under Flexural Stresses Using Meso-Scale Model
...Show More Authors

Two dimensional meso-scale concrete modeling was used in finite element analysis of plain concrete beam subjected to bending. The plane stress 4-noded quadrilateral elements were utilized to model coarse aggregate, cement mortar. The effect of aggregate fraction distribution, and pores percent of the total area – resulting from air voids entrapped in concrete during placement on the behavior of plain concrete beam in flexural was detected. Aggregate size fractions were randomly distributed across the profile area of the beam. Extended Finite Element Method (XFEM) was employed to treat the discontinuities problems result from double phases of concrete and cracking that faced during the finite element analysis of concrete beam. Crac

... Show More
Crossref (6)
Clarivate Crossref