This study synthesized nanocomposite photocatalyst materials from a mixture of Cu2O nanoparticles, ZnO nanoparticles, and graphene oxide (GO) through coprecipitation and hydrothermal methods. This study aims to determine the optimum composition of Cu2O/ZnO/GO nanocomposites in degrading methylene blue. The nanocomposite was synthesized in two steps: 1 the synthesis of Cu2O and ZnO nanoparticles through the coprecipitation method and the preparation of GO through the modified Hummer method. 2 The preparation of Cu2O and ZnO nanoparticles mixtures with GO through the hydrothermal method to form Cu2O/ZnO/GO nanocomposites. The adsorption-photocatalysis process of methylene blue was done with UV light from a halogen lamp. The characterization results indicated that the optimum composition was Cu2O/ZnO nanocomposite with a ratio of 1:2 and 10% of GO, which had a specific surface area of 35.874 m2 g-1, a pore radius of 19.073 nm, and a pore volume of 0.092 cm3 g-1, and a diameter crystalline of 31.19 nm. The degradation efficiency of methylene blue under UV light for 120 minutes were 82.0%, 86.0%, 91.4%, and 79.3% using the Cu2O/ZnO nanocomposites with GO of 1%, 3%, 5%, and 10%, respectively. These results indicated that Cu2O/ZnO/GO nanocomposites efficiently degrade methylene blue from textile dye waste.
Background: Elastomeric chains are used to generate force in many orthodontic procedures, but this force decays over time, which could affect tooth movement. This study aimed to study the force degradation of elastomeric chains. Data and Sources: An electronic search on Cochrane Central Register of Controlled Trials (CENTRAL), MEDLINE, LILACS, and PubMed was made, only articles written in English were included, up to January 2022.Study selection: Fifty original articles, systematic reviews, and RCTs were selected. Conclusion: Tooth movement, salivary enzymes, alcohol-containing mouthwash, whitening mouthwash, and alkaline and strong acidic (pH <5.4) solutions all have a significant impact on elastomeric chain force degradation. The fo
... Show MoreNew nanotechnology-based approaches are increasingly being investigated for enhanced oil recovery (EOR), with a particular focus on heavy oil reservoirs. Typically, the addition of a polymer to an injection fluid advances the sweep efficiency and mobility ratio of the fluid and leads to a higher crude oil recovery rate. However, harsh reservoir conditions, including high formation salinity and temperature, can limit the performance of such polymer fluids. Recently, nanofluids, that is, dispersions of nanoparticles (NPs) in a base fluid, have been recommended as EOR fluids; however, such nanofluids are unstable, even under ambient conditions. In this work, a combination of ZrO2 NPs and the polyacrylamide (PAM) polymer (ZrO2 NPs–PAM) was us
... Show MoreBackground: Elastomeric chains are one of the most commonly used force delivery systems. They have the ability to exert a continuous force, convenience of use, compatibility to oral environment and cost effectiveness but one of the inherited disadvantages is force degradation. Materials and methods: This in vitro study was designed to evaluate the effect of alcohol presence in mouthwashes on force decay of different configurations of clear elastomeric chains from (Ortho Technology company) which are: closed , short and long under the effect of time at (Initial, 1, 2, 3 and 4 weeks) intervals with exposure to different chemical solutions. A total (540) modules of elastomeric chains of three different types (long, short and closed) trans
... Show MoreThe synthesis of conducting polyaniline (PANI) nanocomposites containing various concentrations of functionalized single-walled carbon nanotubes (f-SWCNT) were synthesized by in situ polymerization of aniline monomer. The morphological and electrical properties of pure PANI and PANI/SWCNT nanocomposites were examined by using Fourier transform- infrared spectroscopy (FTIR), and Atomic Force Microscopy (AFM) respectively. The FTIR shows the aniline monomers were polymerized on the surface of SWCNTs, depending on the -* electron interaction between aniline monomers and SWCNTs. AFM analysis showed increasing in the roughness with increasing SWCNT content. The AC, DC electrical conductivities of pure PANI and PANI/SWCNT nanocomposite h
... Show MoreIn this paper, A.C conductivity of micro and nano grain size- TiO2 filled epoxy composites is measured. The dielectric material used is epoxy resin, while micro and nano-sized titanium dioxide (TiO2) of grain size (1.5μm, and 50nm) was used as filler at low filler concentrations by weight (3%, and 5%). Additionally the effect of annealing temperature range (293-373)º K and at a frequency range of 102-106 Hz on the A.C conductivity of the various specimens was studied.
The result of real permittivity for micro and nanocomposite show that the real permittivity increases with decreasing frequency at range of 102-106Hz. The micron-filled material has a higher real relative permittivity than the nano-filled this is true at all the temper
The non-isothermal crystallization kinetics and crystalline properties of nanocomposites poly butyleneterephthalate, [PBT] /multiwalled-carbon nanotubes (MWCNTs) were tested by differential scanning calorimetry (DSC). PBT/(MWCNTs) nanocomposite was prepared by ultrasonicated of MWCNTs (0.5, 1, 2, 4 wt %) in dichloromethane (DCM) and after that the powdered PBT polymer was added to the MWCNTs solution. The non-isothermal crystallization results show that increasing the MWCNTs contents, decreased the melting temperature (Tm) of PBT/(MWCNTs) nanocomposite as compared with pure PBT, while resulting in improving the degree of crystallinity. These results indicated that a little amount of MWCNTs can be evident strong nucleating agent in PBT na
... Show More