The aim of this research is to employ starch as a stabilizing and reducing agent in the production of CdS nanoparticles with less environmental risk, easy scaling, stability, economical feasibility, and suitability for large-scale production. Nanoparticles of CdS have been successfully produced by employing starch as a reducing agent in a simple green synthesis technique and then doped with Sn in certain proportions (1%, 2%, 3%, 4%, and 5%).According to the XRD data, the samples were crystallized in a hexagonal pattern, because the average crystal size of pure CdS is 5.6nm and fluctuates in response to the changes in doping concentration 1, 2, 3, 4, 5 %wt Sn, to become 4.8, 3.9, 11.5, 13.1, 9.3 nm respectively. An increase in crystalline size has been noticed in the doped CdS than in the pure CdS. The particle size is within the range of 24-103 nm, according to SEM data from pure CdS and of the doped with Sn particles. The band gap's energy values, according to UV-Vis reflection spectroscopy were 3.06,2.61 ,2.63, 2.63, 2.66,2.69 eV for pure and doped with Sn 1%, 2%, 3%, 4%, 5% respectively. The grain size and roughness rate of pure CdS materials and doped with Sn are shown in AFM results 2.16,2.39,10.07,11.33, 12.47,18.56 nm and average diameter is 30.15, 11.71, 66.06, 48.27,82.011, 80.35 nm for pure and doped with tin 1%, 2%, 3%, 4%, 5% respectively.
New thermally stable aromatic poly(amide-imide)s ( PAI1- PAI4 ) were synthesized from direct polycondensation reaction of Terephthalic acid and Phthalic acid with two new different diamine monomers derivatives of 1,2,4,5-tetracarboxilic benzene dianhydride as a second diacides in a medium consisting of triphenyl phosphite (TPP) in N-methyl-2pyrrolidone (NMP) / pyridine solution containing dissolved calcium chloride CaCl2. The polymerization reaction produced a series of novel poly(amide-imide) in high yield. The new monomers were characterized by FTIR, 1H-NMR spectroscopy. The resulting polymers were typically characterized by means of FT-IR, 1H-NMR spectroscopy, and solubility tests. Thermal properties of the poly(amide-imide)s were als
... Show MoreBeryllium Zinc Oxide (BexZn1-xO) ternary nano thin films were deposited using the pulsed laser deposition (PLD) technique under a vacuum condition of 10-3 torr at room temperature on glass substrates with different films thicknesses, (300, 600 and 900 nm). UV-Vis spectra study found the optical band gap for Be0.2Zn0.8O to be (3.42, 3.51 and 3.65 eV) for the (300, 600 and 900nm) film thicknesses, respectively which is larger than the value of zinc oxide ZnO (3.36eV) and smaller than that of beryllium oxide BeO (10.6eV). While the X-ray diffraction (XRD) pattern analysis of ZnO, BeO and Be 0.2 Zn 0.8 O powder and nano-thin films indicated a hexa
... Show MoreCu X Zn1-XO films with different x content have been prepared by
pulse laser deposition technique at room temperatures (RT) and
different annealing temperatures (373 and 473) K. The effect of x
content of Cu (0, 0.2, 0.4, 0.6, 0.8) wt.% on morphology and
electrical properties of CuXZn1-XO thin films have been studied.
AFM measurements showed that the average grain size values for
CuXZn1-xO thin films at RT and different annealing temperatures
(373, 473) K decreases, while the average Roughness values increase
with increasing x content. The D.C conductivity for all films
increases as the x content increase and decreases with increasing the
annealing temperatures. Hall measurements showed that there are
two
In present work, the nonlinear optical properties of pure polyaniline and Ag/polyaniline nanocomposite thin films, deposited by plasma jet on glass substrate, were studied through open and closed Z-scan technique using pulse second harmonic Nd:YAG laser of wavelength 532nm, pulse duration of 30 ns and input energy 30mJ. The nonlinear optical properties of pure polyaniline thin films and silver polyaniline nanocomposite thin films prepared at constant gas flow rate 1lm-1 and different silver weight concentration 4, 5, and 10% were studied. The closed aperture Z-scan data indicates that the sign of the refraction nonlinearity is negative for pure polyaniline thin films n2 =11×10-3 cm2/MW and positive nonlinearity for Ag/polyaniline nanoco
... Show MoreDifferent thicknesseses of polycrystalline ZnTe films have been deposited on to glass substrates by vacuum evaporation technique under vacuum 2.1x10-5 mbar. The structural characteristics studied by X-ray diffraction (XRD) showed that the films are polycrystalline and have a cubic (zinc blende ) structure. The calculated microstructure parameters revealed that the crystallite size increases with increasing film thicknesses. The optical measurements on the deposited films were performed in different thicknesseses [ 400 , 450 and 500]nm, to determine the transmission spectrum and the absorption spectra as a function of incident wavelength. The optical absorption coefficient (α) of the films was determined from transmittance spectra in t
... Show MorePolyaniline Multi walled Carbon nanotubes (PANI/MWCNTs) nanocomposite thin films have been prepared by non-equilibrium atmospheric pressure plasma jet on glass substrate with different weight percentage of MWCNTs 1, 2, 3, 4%. The diameter of the MWCNTs was in the range of 8-55 nm and length - - 55 55 μm. the nanocomposite thin films were characterized by UV-VIS, XRD, FTIR, and SEM. The optical studies show that the energy band gap of PANI/MWCNTs nanocomposites thin films will be different according to the MWCNTs polyaniline concentration. The XRD pattern indicates that the synthesized PANI/MWCNTs nanocomposite is amorphous. FTIR reveals the presence of MWCNTs nanoparticle embedded into polyaniline. SEM surface images show that the MWCNT
... Show MoreTiO2 thin films have been deposited at different concentration of
CdO of (x= 0.0, 0.05, 0.1, 0.15 and 0.2) Wt. % onto glass substrates
by pulsed laser deposition technique (PLD) using Nd-YAG laser
with λ=1064nm, energy=800mJ and number of shots=500. The
thickness of the film was 200nm. The films were annealed to
different annealing (423 and 523) k. The effect of annealing
temperatures and concentration of CdO on the structural and
photoluminescence (PL) properties were investigated. X-ray
diffraction (XRD) results reveals that the deposited TiO2(1-x)CdOx
thin films were polycrystalline with tetragonal structure and many
peaks were appeared at (110), (101), (111) and (211) planes with
preferred orientatio
A thermal evaporation technique was used to prepare ZnO thin films. The samples were prepared with good quality onto a glass substrate and using Zn metal. The thickness varied from (100 to 300) ±10 nm. The structure and optical properties of the ZnO thin films were studied. The results of XRD spectra confirm that the thin films grown by this technique have hexagonal wurtzite, and also aproved that ZnO films have a polycrystalline structure. UV-Vis measurement, optical transmittance spectra, showed high transmission about 90% within visible and infrared range. The energy gap is found to be between 3.26 and 3.14e.V for 100 to 300 nm thickness respectivly. Atomic Force Microscope AFM (topographic image ) shows the grain size incre
... Show MoreZinc Oxide transparent thin films (ZnO) with different thickness from (220 to 420)nm
±15nm were prepared by thermal evaporation technique onto glass substrates at 200 with
the deposition rate of (10 2) nm sec
-1
, X-ray diffraction patterns confirm the proper phase
formation of the material. The investigation of (XRD) indicates that the (ZnO) film is
polycrystalline type of Hexagonal and the preferred orientation along (002) plane. The Optical
properties of ZnO were determined through the optical transmission method using ultraviolet-visible spectrophotometer with wavelength (300 – 1100) nm. The optical band gap values of
ZnO thin films were slightly increased from (2.9 - 3.1) eV as the film thickn