Preferred Language
Articles
/
bsj-689
Preparation of phenolic resin complexes
...Show More Authors

in this worl three types of complexed phenolic resins were prepared using various additives such as and improving the aim of this work higher mechanical properties this work is done

View Publication Preview PDF
Quick Preview PDF
Publication Date
Thu Jun 01 2023
Journal Name
Iraqi Journal Of Physics
Preparation of SiO2:TiO2 for High-Performance Double Layer Anti-Reflection Coating
...Show More Authors

        In this work, an anti-reflection coating was prepared in the region (400-1000) nm of wavelength, with a double layer of silicon dioxide (SiO2) as an inner layer and the second layer of the mixture (SiO2) and titanium dioxide (TiO2) with certain ratios, as an outer layer using the chemical spraying method with a number of 6 sprays of layer SiO2 and 12 sprays of layer SiO2 - TiO2. Using the method of chemical spraying deposited on the glass as a substrate with a different number of sprays of SiO2, and a fixed number of TiO2-SiO2. The optical and structural properties were determined using UV-Vis spectroscopy and atomic force mi

... Show More
View Publication Preview PDF
Crossref (5)
Crossref
Publication Date
Sun Jan 01 2023
Journal Name
Dental Hypotheses
Effect of Amoxicillin and Azithromycin Suspensions on Microhardness of Sliver Reinforced and Nano Resin-Modified Glass Ionomers: An In Vitro Study
...Show More Authors

We aimed to examine the effect of amoxicillin and azithromycin suspensions on the microhardness of sliver-reinforced glass ionomer and nano-resin modified glass ionomer (GI). Method: Thirty discs (2mm height x 4mm diameter) of each type of GI were prepared, which were randomly assigned to amoxicillin, azithromycin, and artificial saliva groups. Microhardness was evaluated by Vickers hardness test before and after three immersion cycles. Results: The overall model (P < 0.001), before/after intervention (P < 0.001), intervention group (type of antibiotic) (P=0.013), and type of glass ionomer (P < 0.001) showed significant differences among study groups (P < 0.001). Post hoc test showed only non-significant before/after difference for Azithrom

... Show More
View Publication Preview PDF
Crossref (5)
Clarivate Crossref
Publication Date
Fri Mar 15 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Assessment of the correlation between the tensile and diametrical compression strengths of 3D-printed denture base resin reinforced with ZrO2 nanoparticles
...Show More Authors

Background: The mechanical properties of 3D-printed denture base resins are crucial factors for determining the quality and performance of dentures inside a patient’s mouth. Tensile strength and diametral compressive strength are two properties that could play significant roles in assessing the suitability of a material. Although they measure different aspects of material behavior, a conceptual link exists between them in terms of overall material strength and resilience. Aim: This study aims to investigate the correlation between tensile strength and diametral compressive strength after incorporating 2% ZrO2 nanoparticles (NPs) by weight into 3D-printed denture base resin. Methods: A total of 40 specimens (20 dumbbell-shaped and

... Show More
Scopus (7)
Crossref (4)
Scopus Crossref
Publication Date
Mon Nov 05 2018
Journal Name
Iraqi National Journal Of Nursing Specialties
Effect of Mechanical Surface Treatment on the Tensile Bond Strength of Repaired Acrylic Denture Base Resin Cured by Two Different Techniques
...Show More Authors

Objective: To evaluate and compare the effect of mechanical surface treatment (groove, aluminum oxide particles)
with 45 degree bevel type of joint on tensile bond strength of acrylic specimens repaired by two curing methods
(microwave and water both).
Methodology: Eighty specimens (80) were prepared from pink heat cure acrylic resin. They were divided into two
main groups (40 specimen repaired by microwave energy and 40 specimens repaired by water bath method).Each
group can be divided into four subgroups of ten according to the surface treatment. The control group A was left
intact, group B received no surface treatment, group C and D received surface treatment by (groove, 50 m aluminum
oxide particles). Specimens

... Show More
View Publication Preview PDF
Publication Date
Mon Jun 01 2009
Journal Name
Al-khwarizmi Engineering Journal
Study the Effect Different Radioactive Dose on Mechanical Properties of Composite Material from Novolak Resin Exposure to High – Energy Radiation
...Show More Authors

The research involves using phenol – formaldehyde (Novolak) resin as matrix for making composite material, while glass fiber type (E) was used as reinforcing materials. The specimen of the composite material is reinforced with (60%) ratio of glass fiber.

      The impregnation method is used in test sample preparation, using molding by pressure presses.

      All samples were exposure to (Co60) gamma rays of an average energy (2.5)Mev. The total doses were (208, 312 and 728) KGy.

      The mechanical tests (bending, bending strength, shear force, impact strength and surface indentation) were performed on un irradiated and irrad

... Show More
View Publication Preview PDF
Publication Date
Fri Jul 01 2022
Journal Name
Operative Dentistry
Interfacial Bond Strength and Morphology of Sound and Caries-affected Dentin Surfaces Bonded to Two Resin-modified Glass Ionomer Cements
...Show More Authors
SUMMARY<sec> <title>Objective

To evaluate the shear bond strength and interfacial morphology of sound and caries-affected dentin (CAD) bonded to two resin-modified glass ionomer cements (RMGICs) after 24 hours and two months of storage in simulated body fluid at 37°C.

Methods and Materials

Sixty-four permanent human mandibular first molars (32 sound and 32 with occlusal caries, following the International Caries Detection and Assessment System) were selected. Each prepared substrate (sound and CAD) was co

... Show More
View Publication
Scopus (13)
Crossref (13)
Scopus Clarivate Crossref
Publication Date
Mon Jan 11 2021
Journal Name
Der Pharmacia Lettre
Implementations of Transition Metal complexes of shiff Base Derived Ampyrone
...Show More Authors

Implementations of Transition Metal complexes of shiff Base Derived Ampyrone

Publication Date
Wed Mar 10 2021
Journal Name
Baghdad Science Journal
synthesis and study of some mixed ligand complexes of caffeine
...Show More Authors

I've been in this research preparation and diagnostic complexes mixed Kandat of Alcavaúan Alpiculan ion Althaaossianat with some metal ions has been reactive in ethanol solvent and distilled water by (1:1) and water complexes and lotions to the accounts of the metal in the complex

View Publication Preview PDF
Publication Date
Wed Feb 20 2019
Journal Name
Iraqi Journal Of Physics
Preparation of polyaniline polymer and using it as a Vapor sensor of acids
...Show More Authors

 Polyaniline organic Semiconductor polymer was prepared by oxidation polymerization by adding hydrochloric acid concentration of 0.1M and potassium per sulfate concentration of 0.2M to 0.1M of aniline at room temperature, the polymer was deposited at glass substrate, the structural and optical properties were studies through UV-VIS, IR, XRD measurements, films have been operated as a sensor of vapor  H2SO4 and HCl  acids.

View Publication Preview PDF
Crossref
Publication Date
Sun Jun 05 2016
Journal Name
Baghdad Science Journal
Preparation and Characterization of Bimetallic Catalyst (NiO – CoO) for Desulfurization of Gas Oil
...Show More Authors

In this study NiO - CoO bimetallic catalysts are prepared with two Ni/Co ratios (70:30 and 80: 20) using the precipitation method of nitrate salts. The effects of Ni /Co ratio and preparation methods on the catalyst are analyzed by using different characterization techniques, i.e. atomic absorption (AA) , XRD, surface area and pore volume measurements according to the BET method . The results indicate that the best catalyst is the one containing the percentage of Ni :Co ( 70 : 30 ). Experiments indicate that the optimal conditions to prepare catalyst are stirring for three hours at a temperature of 60oC of the preparation , pH= (8-9) , calcination temperature at 400oC for two hours

... Show More
View Publication Preview PDF
Crossref