Water scarcity is one of the most important problems facing humanity in various fields such as economics, industry, agriculture, and tourism. This may push people to use low-quality water like industrial-wastewater. The application of some chemical compounds to get rid of heavy metals such as cadmium is an environmentally harmful approach. It is well-known that heavy metals as cadmium may induce harmful problems when present in water and invade to soil, plants and food chain of a human being. In this case, man will be forced to use the low quality water in irrigation. Application of natural materials instead of chemicals to remove cadmium from polluted water is an environmental friendly approach. Attention was drawn in this research work to use some natural minerals as zeolite, bentonite and montmorillonite to adsorb cadmium element from polluted water. Various concentrations of cadmium in solutions 10, 30 and 50 ppm were treated with three different ratios of each mineral; 1, 3 and 5% (W/V). The obtained results proved that increasing the ratio of amendments to 5% increased Cd adsorption from solution particularly at 50ppm Cd. Zeolite obtained the highest ratio of adsorption (47.90 ppm), followed by montmorillonite (44.99 ppm) and the lowest was bentonite (38.97 ppm). Therefore, it can be recommended that addition of zeolite is the most favorable material to remove Cd element from polluted water.
Soil is a crucial component of environment. Total soil analysis may give information about possible enrichment of the soil with heavy metals. Heavy metals, potentially contaminate soils, may have been dumped on the ground. chromium, nickel and cadmium,
Aniline and its derivatives are common contaminants in various wastewaters and represent a serious worry for societies health and a challenge to ecologists due to their dangers effects on to the human health.
ZSM-5 zeolite was prepared from locally available materials (kaolin and rice husk) for adsorption of aniline from synthetic wastewater. Characterization of the prepared zsm-5, kinetics and thermodynamic of the adsorption process were investigated.
The characterization results of the prepared zsm-5 zeolite showed that the surface area was 270.1 m2/g and pore volume 0.21828 cm3/g. The silica to alumina ratio (Si/Al) was 166. 47 and the sodium content was 11 wt. %. The atomic force microscope (AFM)
... Show MoreIn this work, the synergistic effect of chlorinated rubber (additive I),with zeolite 3A (additive II), zeolite 4A (additive III), and zeolite 5A (additive IV) in (1:1) weight percentage, on the flammability for unsaturated polyester resin was studied in the weight ratios for (3,7,10,13&15%) by preparing films of (130×130×3) mm in diameters. Three standard test methods used to measure were the flame retardation which are; ASTM: D-2863, ASTM: D- 635& ASTM: D-3014. Results obtained from these tests indicated that all of the additives were effective additive IV has the highest efficiency as a flame retardant.
In the present work, zeolite Y has been synthesized successfully by sol-gel method.Zeolite was synthesized by crystallization of the final gel which consist from seeding and feed stock gels at 85 oC. HY zeolite was prepared by an ion exchange process with ammonium chloride solution and then loaded with different percentages of platinum and titanium by the wet - impregnation method.
X-ray Diffraction (XRD), X-ray Florescence (XRF), Scanning Electron Microscopy (SEM), BET surface area and, Crushing strength were used to characterize the synthesized and prepared catalysts . Results showed high crystallinity 90% with silica to alumina ratio 5 for HY, high surface area of 600 m2/g and pore
... Show MoreLight naphtha one of the products from distillation column in oil refineries used as feedstock for gasoline production. The major constituents of light naphtha are (Normal Paraffin, Isoparaffin, Naphthene, and Aromatic). In this paper, we used zeolite (5A) with uniform pores size (5Aº) to separate normal paraffin from light naphtha, due to suitable pore size for this process and compare the behavior of adsorption with activated carbon which has a wide range of pores size (micropores and mesopores) and high surface area. The process is done in a continuous system - Fixed bed reactor- at the vapor phase with the constant conditions of flow rate 5 ml/min, temperature 180oC, pressure 1.6 bar and 100-gram weight o
... Show MoreBentonite is widely used in industrial applications. The present study reports the effect of adding different weights of ZnO to the Iraqi bentonite, on surface area, pore volume and real density. These surface properties were evaluated for pure and modified bentonite. The modification was made by adding different ZnO weights such as; ( 0.5%, 1%, 5%, 10% ). The effect of heat exposing for all modified clay samples at 500 ?C have been also evaluated. The results show that the addition of 0.5% ZnO leads to increase the surface area percentage about 36%, increase pore volume percentage about 5.48% and increase the real density percentage about 27.116%. When the samples exposed to 500 ?C, their surface area and pore volumes have been decreased a
... Show MoreDrilling solutions can be considered as an intricate mixture comprising of number of chemical additives which aid specific needs such as controlling the rheological properties and reducing corrosion. Inhibitors are substances that are added in small concentrations to corrosive environment to decrease the corrosion. Their applications can be found in drilling equipments. The effect of adding Zinc Sulphate and Carboxymethyl Cellulose to study their influence on the corrosion of carbon steel in Bentonite mud has been evaluated using Weight Loss Technique. This study focuses on determining rheological properties and corrosion characteristics. Results show CMC and ZnSO4 work as inhibitors when added to the Bentonite with inhibition
... Show MoreIn this study, the effect of grafting with magnesium (Mg) ratios (0.1, 0.3, 0.5) on the structural and optical properties of cadmium oxide films (CdO) was studied, as these films were prepared on glass bases using the method of pulse laser deposition (PLD). The crystallization nature of the prepared membranes was examined by X-ray diffraction technique (XRD), which showed that the synthesis of the prepared membranes is polycrystalline, and (AFM) images also showed that the increased deformation with magnesium led to an increase in the grain size ratio and a decrease in surface roughness, as well as the absorption coefficient was calculated. And the optical energy gap for the prepared membranes, where it was found that the absorption coef
... Show MoreIn this work, chemical spray pyrolysis deposition (CSP) technique was used to prepare a mixed In2O3-CdO thin films with different CdO content (10, 30 and 50)%volume ratio on glass substrates at 150 ᵒC substrate temperature. The surface morphology and structural properties were measured to find the optimum conditions to improve thin films properties for using as photo detector. Current –Time, the sensitivity and response speed vary for each mixture. Samples with 10% vol. CdO content has square pulse response with average rise time nearly 1s and fall time 1s.
In this paper, CdS/Si hetrojunction solar cell has been made by
Chemical Bath Deposition (CBD) of CdS thin film on to
monocrystalline silicon substrate. XRD measurements approved that
CdS film is changing the structure of CdS films from mixed
hexagonal and cubic phase to the hexagonal phase with [101]
predominant orientation. I-V characterization of the hetrojunction
shows good rectification, with high spectral responsivity of 0.41
A/W, quantum efficiency 90%,and specific detectivity 2.9*1014
cmHz1/2W -1 .