Different coating layers of fluorescent agent (FCA) on the solar cells were used. An increase of 35% in the energy conversion efficiency of the solar cell have been obtained. This increase is attributed to the reduction ofthe reflected light, eflection spectra show low values at higher thickness which explained the increase ofthe conversion efficiency with increases of layer thickness.
The performance of single and two stage solar concentrator were studied ' " The ratio of the primary to the secondary mirrors diameter is taking to be 0.5, depending on the theoretical calculation for the accumulated energy by the concentrator with ratio between 0.0 to 0.9. The design of the systems were designed and examined by using a ray-tracing program. The efficiency of the single and the two stage concentrators are calculated and compared with and without cooling systems.
The present work is devoted to investigate the performance of a homemade Y-shape catalytic microreactor for degradation of dibenzothiophene (DBT), as a model of sulphur compounds including in gas oil, utilizing solar incident energy. The microchannel was coated with TiO2 nanoparticles which were used as a photocatalyst. Performance of the microreactor was investigated using different conditions (e.g., DBT concentration, LHSV, operating temperature, and (H2O2/DBT) ratio). Our experiments show that, in the absence of UV light, no reaction takes place. The results revealed that outlet concentration of DBT decreases as the mean residence time in the microreactor increases. Also, it was noted that operating temperature s
... Show MoreSilicon nanowire arrays (SiNWs) are created utilizing the metal-assisted chemical etching method with an Ag metal as a catalyst and different etching time of 15, 30, and 60 minutes using n-Si (100). Physical properties such as structural, surface morphology, and optical properties of the prepared SiNWs are studied. The diameter of prepared SiNWs ranged from 20 to 280 nm, and the reflectance in the visible part of the wavelength spectrum was less than 1% for all prepared samples. The obtained energy gap of prepared SiNWs was around 2 eV, which is higher than the energy gap of bulk silicon. X-ray diffraction (XRD) has diffraction peaks at 68.70o for all prepared samples. The heterojunction solar cell was fabricated based on the
... Show MoreSilver Indium Aluminum Selenium AgIn1xAlxSe2 AIAS for x=01 thin films was deposited by thermal evaporation at RT and different︣︢︡ ︠︣1thickness 100 150 and 200 nm on the glass Substrate and p2Si wafer to produce AIAS/p3Si heterojunctionsolarcell4 Structural optical electrical and photovoltaicproperties6 are investigated for the samples XRD analysis reveals that all the deposited AIAS films show polycrystalline structure without any change due to increase of thickness Average diameter and roughness calculated from AFM images shows an increase in its value with increasing thickness The optical absorbance and transmittance for samples are measured using a spectrometer type UV Visible 1800 spectra1photometer to study the energy6gap The
... Show MoreThe n-type Au thin films of 500nm thickness was evaporated by thermal evaporation method on p-type silicon wafer of [111] direction to formed Au/Si heterojunction solar cell. The AC conductivity, C-V and I-V characteristics of fabricated c-Au/Si diffusion heterojunction-(HJ) solar cell, has been studied. The first methods demonstrated that the AC conductivity due to with diffusiontunneling mechanism, while the second show that, the heterojunction profile is abrupt, the heterojunction parameters have been played out, such as the depletion width, built-in voltage, and concentration. And finally the third one show that the c-Au/Si HJ has rectification properties, and the solar cell yielded an open circuit voltage of (Vic) 0.4V, short circuit c
... Show MoreAgInSe2 (AIS) thin films solar cell involving of n-type AgInSe2 and Si of p-type substrate by using thermal evaporation method. The influence of annealing of the preparation AgInSe2 were considered to find the best properties of solar device. Thin film AIS have been deposited under the vacuum of 1.5*10-6 Torr with (400) nm thickness at R.T and annealing temperatures (473,573) K. Polycrystalline tetragonal structure for AIS thin films from XRD and increasing of surface roughness from AFM, energy gap values decreasing with increasing annealing temperatures, all films were negative type, I-V characteristics show increasing of efficiency with increasing of annealing temperatures.
Genotoxic effects of crude bacteriocin extracted from Citrobacter freundii were detected on albino mice bone marrow cells in vivo, using micronucleus (MN) and comet assay. The mice were administered intraperitoneally with 37.5, 75, 150 and 300 mg/kg of the extract for 24 hours. C. freundii was isolated from patients suffering from urinary tract infections (UTI). The bacteriocin producing isolates were determined using cup assayand the most efficient bacteriocin producers were selected. Bacteriocin was extracted from the efficient isolates via the induction with Mitomycin-C (2 mg/ml). Bacteriocin activity (320 U/ml) was determined by well diffusion method, while the protein concentration (2900µg/ml) was estim
... Show More Background: Prelabour rupture of membranes is a problem that faces the obstetricians. It has many maternal and fetal sequale and its etiology and management still controversial.
Objective: To test the absolute nucleated red blood cells counts at birth in infants who are born after prelabour rupture of membranes.
Methods: A prospective study conducted in AL-Kadhymia Teaching Hospital. Hundred pregnant women were included in this study. Fifty pregnant women who had prelabour rupture of membranes considered as group (1), other fifty pregnant women with intact membranes considered as group (2) through a period of one year. Nucleated red blood cell counts of venous cord blood obtained within one hour of life from 50 infants who we
Braces in straight bridge systems improve the lateral-torsional buckling resistance of the girders by reducing the unbraced length, while in horizontally curved and skew bridges, the braces are primary structural elements for controlling deformations by engaging adjacent girders to act as a system to resist the potentially large forces and torques caused by the curved or skewed geometry of the bridge. The cross-frames are usually designed as torsional braces, which increase the overall strength and stiffness of the individual girders by creating a girder system that translates and rotates as a unit along the bracing lines. However, when they transmit the truck’s live load forces, they can produce fatigue cracks at their connection
... Show More