The aim of this research is to study the effect of welded joint design (Butt joint and lap joint) on thejoint strength during tension and fatigue loading with different current of welding (40,50,60,70,80) ^per, and different type of wire welding. The result of this research is showed that the effect of fatigue loading on the type of joint is more than the effect of tension loading on it. And the butt joint welding is better than the lap joint welding during the fatigue loaded.The experimental results of the effect of W'elding current showed that more increasing and more decreasing the value of the heat input, during the welding was found to produce mechanical brittleness on the buttjoint welding during the static and dynamic loading. Also it was found that welded lap joint properties are improved when the welding current is increase during the static and dynamic loading. Results indicate too that the more effect of the type of wires welding on the welded joint during the static and dynamic loading.?
The study involved 45 male and 45 females of diabetic patients type- ?? aged from 40-69years , and with the same numbers of males and females for control , all the patients and controls were without any periodontal diseases and without any systemic disease. Diabetic patients were divided in to three groups according to the degree of periodontitis , and the inflamed gingiva of all groups of diabetic patients were treated with the dried fruits powder (crude) of medicinal plants Quercus robur , Thuja occidenalis , Terminalia chebula, Anethum graveolens , respectively and mixture. Some immunological and antimicrobial factors (IgA, Lactoferrin , Lysozyme ) , were detected in serum and saliva of diabetic patients and the control
... Show MoreThe shoulder and hip joints though essentially both are ball and socket joints, show structural variability to serve functional needs.
This study aims at revealing some of the structural and functional properties of each of the two joints regarding the factors that contribute to the stability of any joint in the body, namely: bone, ligament, and muscle.
In this work polymeric composites were done from unsaturated polyester as a matrix reinforced with glass fiber type (E-glass) with two different volume fraction 20% & 40%. Fatigue tests showed that the number of fatigue cycles to failure limit for samples reinforced with uniform (woven Roving 0-90°) E-glass fiber and random (continuous fibers) with volume fraction 40% more than that for the same samples with volume fraction 20%. Also the fatigue results showed that the uniform samples failed with fatigue cycles more than that of random.
Jet grouting is one of the most widely applied soil improvement techniques. It is suitable for most geotechnical problems, including improving bearing capacity, decreasing settlement, forming seals, and stabilizing slopes. One of the difficulties faced by designers is determining the strength and geometry of elements created using this method. Jet grouted soil-cement columns in soil are a complicated issue because they are dependent on a number of parameters such as soil type, grout and water flow rate, rotation and lifting speed of monitor, nozzle jetting force, and water to cement ratio of slurry. This paper discusses the effect of the water-cement ratio on the physical and mechanical characteristics of soilcrete. In t
... Show MoreLong-term use of sulfonylureas including chlorpropamide, is known to potentiate the antidiuretic action of arginine vasopressin (AVP), predisposing to hyponatremia.The present study was designed to evaluate the effect of long term use of glibenclamide on serum and urinary levels of sodium and potassium in Type 2 DM patients in Iraqi DM centers. Ninety eight patients with Type 2 DM who were maintained on different doses of glibenclamide for at least 1 year, attending the centre for Diabetes and Endocrinology in Al-Rusafa, Baghdad, were enrolled in the study, in addition to 15 normal healthy subjects. Patients were allocated into three groups according to the dose of glibenc
... Show MoreBackground: This study aimed to compare the mechanical properties between four groups of newly fabricated combination wires according to their method of union, according to the gauges of wires and a comparison were made between them and their originals. Materials and method: A total of 60 stainless steel combination wires were fabricated , divided into four groups according to gauge of wires and their method of union, each of them with 15 samples, the groups were welded (0.016x0.022-0.016 and 0.016x0.022-0.018) and soldered (0.016x0.022-0.016 and 0.016x0.022-0.018), samples were made according to certain parameters which were : for the welded samples: length,weight, duration of pulsation and size of copper electrode tips used; for the sold
... Show MoreThis research studies the development and synthesis of blended nanocomposites filled with Titanium dioxide (TiO2). Blended nanocomposites based on unsaturated polyester resin (UPR) and epoxy resins were synthesized by reactive blending. The optimum quantity from nano partical of titanium dioxide was selected and different weight proportions 1%, 3%, 5%, and 7% ratios of new epoxy are blended with UPR resin. The dielectric breakdown strength and thermal conductivity properties of the blended nanocomposites were compared with those of the basis material (UPR and 3% TiO2).The results show good compatibility epoxy resins with the UPR resin on blending, dielectric breakdown strength values are higher while thermal conductivity values of
... Show MoreDate palm fiber is one of the common wastes available in the M. E. countries essentially Iraq. The aim of search to investigate the performance and effects of fiber date palm on the mechanical properties of high strength concrete, this fiber was used in three ratio 2, 4 and 6 % by vol. of concrete at ages of (7, 28, 90) days. Results demonstrated improvement in the compressive strength increased 19.2 %, 23.6%, 24.9 % for 2%, 4%, 6% of fiber respectively at age 28 days. Flexural strength increases 47.6%, 66.2%, 93.8% form (2,4,6) % of fiber respectively at age 28 days. Density increase about 0.41%, 0, 61 % 0.69 % for (2,4,6) % of fiber respectively at age 28. Absorption water decrease