Nanoparticles of Pb1-xCdxS within the composition of 0≤x≤1 were prepared from the reaction of aqueous solution of cadmium acetate, lead acetate, thiourea, and NaOH by chemical co-precipitation. The prepared samples were characterized by UV-Vis spectroscopy(in the range 300-1100nm) to study the optical properties, AFM and SEM to check the surface morphology(Roughness average and shape) and the particle size. XRD technique was used to determine the crystalline structure, XRD technique was used to determine the purity of the phase and the crystalline structure, The crystalline size average of the nanoparticles have been found to be 20.7, 15.48, 11.9, 11.8, and 13.65 nm for PbS, Pb0.75Cd0.25S, Pb0.5Cd0.5S, Pb0.25Cd0.75S, and CdS respectively. The results indicate that crystalline structure of all prepared samples is cubic except CdS which shows hexagonal and cubic structure. The particle size was found within the range of (64.81 to 91.14) nm, with a high purity.
Heterocyclic compounds are employed in many applications, and numerous researchers have created liquid crystals by adding heterocyclic to the structures of these molecules. This work includes the synthesis and characterization of new compounds that contain 5H-thiazolo [4,3-b][1,3,4] thiadiazol united in multiple steps, starting with the synthesis of the aldehyde compound [I] by reaction chloro ethyl acetate with 4-hydroxybenzaldehyde in the presence of ethanol and potassium carbonate, followed by reactions with thiosemicarbazide, mercapto acetic acid in sulphuric acid to produce compound [II] then reflux compound [II] with hydrazine hydrate to product compound [III], after that reaction the later compound with nalkoxybenzaldehyde [IV]n and
... Show MoreThin films were prepared from poly Berrol way Ketrrukemaaih pole of platinum concentrations both Albaarol and salt in the electrolytic Alastontrel using positive effort of 7 volts on the pole and the electrical wiring of the membrane record
This study involves the synthesis of a new class of silicon polymers, designated as P1-P7, derived from dichlorodimethylsilane (DCDMS) in combination with various organic compounds (Schiff bases prepared from different amines and appropriate aldehydes or ketones) [I-V] through condensation polymerization. The structures of all monomers and polymers were characterization by FTIR and 1HNMR spectroscopy (for some polymers). The results of thermogravimetric analysis (TGA) and differential scanning calorimetry DSC test show stable thermal behaviour. Polymers with a higher concentration of aromatic rings in their repeating structural units exhibited a higher temperature for weight loss, indicating increased thermal stability. Thermal meas
... Show MoreThe increasing use of plastics in various aspects of modern life resulted in the availability of enormous amount of wastes, including a negative effect on the environment and humans. So it is necessary to find solutions to deal with these wastes and ensure to use them as solutions to use in concrete mix . In this research the production of concrete containing high and low density polyethylene has been used by (5, 10, 15)% as a replacement of part of the volume of sand, so as to obtain concrete good compressive strength as well as other benefits such as improved possibility of pumping concrete and reduce the loss of concrete for workability polymer is a material that is non-absorbable of water . It is also intended to dispose of these was
... Show MoreNanocomposite was prepared using unsaturated polyester (UP) resin as a matrix and graphene nanoparticles as a reinforcement material in six percentage weights (0, 0.1, 0.2, 0.3, 1 and 1.5%). Mechanical, calorimetric and thermal studies were performed on the (UP) resin/graphene nanocomposite. All tests showed a clear improvement of all mechanical properties examined (hardness, flexural strength (F.S), impact strength (I.S) and tensile strength (T.S)) with increasing graphene percentage. In addition, the temperature of glass transition and thermal conductivity of this composite increased with increasing graphene content.
This study involves the synthesis of a new class of silicon polymers, designated as P1-P7, derived from dichlorodimethylsilane (DCDMS) in combination with various organic compounds (Schiff bases prepared from different amines and appropriate aldehydes or ketones) [I-V] through condensation polymerization. The structures of all monomers and polymers were characterization by FTIR and 1HNMR spectroscopy (for some polymers). The results of thermogravimetric analysis (TGA) and differential scanning calorimetry DSC test show stable thermal behaviour. Polymers with a higher concentration of aromatic rings in their repeating structural units exhibited a higher temperature for weight loss, indicating increased thermal stability. Thermal meas
... Show MoreThe performance of asphalt pavements is crucial due to heavy traffic loads from civil and industrial developments. Various additives and modifiers are used in flexible roads to improve their resistance to deterioration caused by climatic changes. From this context, modifying the asphalt binder with polymers is popular in asphalt pavement construction. The present research investigates the effect of Polyethylene (PE) polymers in powder form on the characteristics of asphalt mixtures since these polymers are composed of hydrocarbons. It is similar to asphalt binders, making them very effective in enhancing the performance of neat asphalt produced from the oil refinery. To confirm this, two types of PE, High-Density PE (HDPE) and Low-Density P
... Show MoreThe refractive indices, nD densities 𝜌, and viscosities of binary mixtures of sulfolane + n -butanol + sec- butanol + iso- butanol + tert – butanol + n-propanol and iso- propanol were measured at 298.15K. Form experimental data, excess molar volum VE , excess molar refractivity ∆nD, excess molar viscosity E and excess molar Gibbs free energy of activation of viscous flow G *E were calculated. From n-propanol – sulfolane and iso- propanol sulfolane mixtures showed negative ∆nD, n-butanol – sulfolane, sec-butanal – sulfolane, iso-butanol – sulfolane and tert- butanol sulfolane , nD was positive over the whole mole fraction rang , while VE , E and G *E show a negative deviation. The
... Show More