The present work focuses on the changing of the structural characteristics of the grown materials through different material characterization methods. Semiconductor CdSxSe 1-x nano crystallines have been synthesized by chemical vapor depostion. (X- ray Diffraction; XRD), (Field Emission Scanning Electron Microscopy; FESEM), measured the characterization of Semiconductor CdSxSe1-x nano crystallines. The optical properties of semiconductor CdSxSe1-x nanocrystallines have been studied by the photoluminescence (PL) (He-Cd pulsed ultraviolet laser at 325nm excitation wavelength) at room temperature. The results showed the change rule of photoluminsence peak at different S/Se ratios according to the photoluminsence spectral analysis technology. The photuminscence peak can be continuously modulated between (500- 650) nm, so the tunable emission of the materials in the present work have novle applications in the area of bioscience and spectroscopy, etc.
The City of Ember is a very interesting novel that is although intended for young readers, have so many layers and messages that are misunderstood. In this research, both the novel and the film adaptation are studied with the intent to decode the warning messages that the novelist and the director tried to introduce to the audience. The research studies four vital messages; the first message is that history repeats itself for the novel has many allusions to the history of Jews and their painful holocaust and even goes back in history the days of Moses and the Exodus, the second message tackles the conspiracy theory that states nothing happens by accident and that everything is planned and connected hence comes the third message
... Show MoreThe optical energy gap(Eopt) and the width of the tails of localized states in the band gap (?E) for Se:2%Sb thin films prepared by thermal co-evaporation method as a function of annealing temperature are studied in the photon energy range ( 1 to 5.4)eV.Se2%Sb film was found to be indirect transition with energy gap of (1.973,2.077, 2.096, 2.17) eV at annealing temperature (295,370,445,520)K respectively. The Eopt and ?E of Se:2%Sb films as a function of annealing temperature showed an increase in Eopt and a decrease in ?E with increasing the annealing temperature. This behavior may be related to structural defects and dangling bonds.
Alloys of Bi2[Te1-x Sex]3 were prepared by melting technique with different values of Se percentage (x=0,0.1,0.3,0.5,0.7,0.9 and 1). Thin films of these alloys were prepared by using thermal evaporation technique under vacuum of 10-5 Torr on glass substrates, deposited at room temperature with a deposition rate (12nm/min) and a constant thickness (450±30 nm). The concentrations of the initial elements Bi, Te and Se in the Bi2 [Te1-x Sex]3 alloys with different values of Se percentage (x), were determined by XRF,The morphological and structural properties were determined by AFM and XRD techniques. AFM images of Bi2[Te1-x Sex]3 thin films show that the average diameter and the average surface roughness inc
... Show MoreCopper oxide thin films were deposited on glass substrate using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature. The thickness of the thin films was around 0.43?m.Copper oxide thin films were annealed in air at (200, 300 and 400°C for 45min.The film structure properties were characterized by x-ray diffraction (XRD). XRD patterns indicated the presence of polycrystalline CuO. The average grain size is calculated from the X-rays pattern, it is found that the grain size increased with increasing annealing temperature. Optical transmitter microscope (OTM) and atomic force microscope (AFM) was also used. Direct band gap values of 2.2 eV for an annealed sample and (2, 1.5, 1.4) eV at 200, 300,400oC respect
... Show MoreA thin CdS Films have been evaporated by thermal evaporation technique with different thicknesses (500, 1000, 1500 and 2000Å) and different duration times of annealing (60, 120 180 minutes) under 573 K annealing temperature, the vacuum was about 8 × 10-5 mbar and substrate temperature was 423 K. The structural properties of the films have been studied by X- ray diffraction technique (XRD). The crystal growth became stronger and more oriented as the film thickness (T) and duration time of annealing ( Ta) increases.
Thin films were prepared from melting coumrin C 2 dye in solvent DMF with PMMA with the same solvent and concentrations(1*10-2 5*10-3, 1*10-3 )M ,Films were either left on Flat surface for24hours or dried in avacuum oven for five hours at a temperature of 80c.The relative intensity of both the absorption and fluorescece spectrum are found to be increased with the increase of thickness of these films and concentration .Also the thickness of these films was measured by Mickelsons interfearing method.Also quantum efficiency of these films were measured too
This work involves synthesis of novel Schiff bases derivatives contining isoxazoline or pyrazoline units starting with chalcons . 4-Aminoacetophenone was reacted with 3-nitrobenzaldehyde in basic medium giving chalcone [I] by claisen-schemidt reaction. The chalcone [I] was reacted with hydroxylamine hydrochloride giving isoxazoline [II] in basic medium. The chalcone [I] could also react with hydrazitne hydrate to give pyrazoline [III] . The novel Schiff bases with structural formula [IV] and [V] were prepared by the reaction of amino compounds ; isoxazoline [II] and pyrazolines [III] with p-substituted aldehydes or p-subsituted ketones, respectively in dry benzene using drops of glacial acetic acid as a cat
... Show MoreMany researchers consider Homogeneous Charge Compression Ignition (HCCI) engine mode as a promising alternative to combustion in Spark Ignition and Compression Ignition Engines. The HCCI engine runs on lean mixtures of fuel and air, and the combustion is produced from the fuel autoignition instead of ignited by a spark. This combustion mode was investigated in this paper. A variable compression ratio, spark ignition engine type TD110 was used in the experiments. The tested fuel was Iraqi conventional gasoline (ON=82).
The results showed that HCCI engine can run in very lean equivalence ratios. The brake specific fuel consumption was reduced about 28% compared with a spark ignition engine. The experimental tests showed that the em
... Show More